journal article·2025-12Open access

The differential impact of light soaking and dark annealing on hydrogen species during a LeTID cycle in boron-doped FZ silicon: A quantitative FT-IR study

Nicole Aßmann, Benjamin Hammann, Mariann Carlsen Frøland, Wolfram Kwapil, Eduard Monakhov

Abstract

Hydrogen is recognized as the key species responsible for light- and elevated- temperature-induced degradation (LeTID) in silicon. The simplest hydrogen species detectable is acceptor-hydrogen, HB in boron-doped material. Many studies track HB trough resistivity measurements and infer the evolution of the hydrogen molecule, H 2 , often excluding other potentially relevant hydrogen-related species from consideration. This study presents a Fourier transform-infrared analysis of the evolution of the hydrogen species, HB, H 2 , the hydrogen dimer , and the vacancy-hydrogen complexes VH 4 and V 2 H 6 , during dark annealing and light soaking. The findings are compared to changes in lifetime-equivalent defect density observed over a LeTID cycle. Before solar cell processing the hydrogen species found are HB, H 2 , V 2 H 6 , and VH 4 . After processing, is formed, HB and H 2 increase in concentration, while VH 4 and V 2 H 6 disappear. Light soaking at 75 °C and 1 sun-equivalent and dark annealing at 175 °C both reduce H 2 and concentrations, while HB concentration increases with dark annealing but decreases during light soaking. Extended dark annealing results in a re-appearance of VH 4 . A considerable role of and VH 4 in the hydrogen balance in a LeTID cycle is demonstrated. Finally, several unidentified peaks are observed in the wavenumber range of 3000 cm − 1 to 3300 cm − 1 , showing sensitivity to different treatment conditions. Specifically, peaks at 3029 . 1 cm − 1 , 3102 . 1 cm − 1 , and 3238 . 9 cm − 1 grow only when light soaking took place as final step. Conversely, a peak at 3025 . 8 cm − 1 increases under dark annealing conditions and decreases with prolonged light soaking.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (70)

Show source-provided references
1. Degradation of crystalline silicon due to boron-oxygen defects10.1109/JPHOTOV.2016.2614119 ↗
2. Fundamental boron-oxygen-related carrier lifetime limit in mono- and multicrystalline silicon10.1002/pip.586 ↗
3. Influence of hydrogen on the regeneration of boron-oxygen related defects in crystalline silicon10.1063/1.4804310 ↗
4. Hydrogen passivation of oxygen donors in Si10.1557/PROC-59-475 ↗
5. Interaction of hydrogen and thermal donor defects in silicon10.1063/1.98144 ↗
6. Electrical properties of deep silver- and iron-related centres in silicon10.1088/0022-3719/17/36/023 ↗
7. Deuterium passivation of grain-boundary dangling bonds in silicon thin films10.1063/1.92934 ↗
8. Hydrogen in silicon: A discussion of diffusion and passivation mechanisms10.1016/0927-0248(95)00098-4 ↗
9. Effect of PECVD silicon oxynitride film composition on the surface passivation of silicon wafers10.1016/j.solmat.2011.09.052 ↗
10. Understanding the light-induced degradation at elevated temperatures: Similarities between multicrystalline and floatzone p-type silicon10.1002/pip.2954 ↗
11. Hydrogen diffusion from PECVD silicon nitride into multicrystalline silicon wafers: Elastic recoil detection analysis (ERDA) measurements and impact on light and elevated temperature induced degradation (LETID)
12. Progress in the understanding of light- and elevated temperature-induced degradation in silicon solar cells: A review10.1002/pip.3362 ↗
13. Light induced degradation of rear passivated mc-Si solar cellsitle
14. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
15. Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon10.1016/j.solmat.2017.08.003 ↗
16. Light-induced activation and deactivation of bulk defects in boron-doped float-zone silicon10.1063/1.4983024 ↗
17. Influence of dopant elements on degradation phenomena in B- and Ga-doped Czochralski-grown silicon10.1002/solr.202100147 ↗
18. Hydrogen induced degradation: A possible mechanism for light- and elevated temperature- induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
19. Hydrogen-induced degradation: Explaining the mechanism behind light- and elevated temperature-induced degradation in n- and p-type silicon
20. Defect formation under high temperature dark-annealing compared to elevated temperature light soaking10.1016/j.solmat.2018.06.043 ↗
21. The impact of different hydrogen configurations on light-and elevated-temperature-induced degradation10.1109/JPHOTOV.2023.3236185 ↗
22. Solubility of hydrogen in silicon at 1300°C10.1063/1.108602 ↗
23. Hydrogen solubility and defects in silicon10.4028/www.scientific.net/MSF.143-147.861 ↗
24. Hydrogen molecules in boron-doped crystalline silicon10.1088/0268-1242/14/1/011 ↗
25. Quantitative analysis of boron-hydrogen pair dynamics by infrared absorption measurements at room temperature10.1063/5.0090965 ↗
26. Interactions of hydrogen molecules with bond-centered interstitial oxygen and another defect center in silicon10.1103/PhysRevB.56.13118 ↗
27. H2* defect in crystalline silicon10.1103/PhysRevLett.71.875 ↗
28. Hydrogen atoms and complexes in monocrystalline semiconductors
29. H2-related defects in Si quenched in H2 gas studied by optical absorption measurements10.1143/JJAP.38.L484 ↗
30. Hydrogen and hydrogen dimers in c -C, Si, Ge, and α-Sn10.1103/PhysRevB.50.17018 ↗
31. Solubility of hydrogen in silicon at high temperatures10.4028/www.scientific.net/SSP.32-33.155 ↗
32. Radiation-induced formation of H2* in silicon10.1103/PhysRevLett.82.815 ↗
33. Budde · 1998
34. Vacancy-hydrogen defects in silicon studied by Raman spectroscopy10.1103/PhysRevB.64.035204 ↗
35. Si isotopic structure of the infrared absorption of the fully hydrogenated vacancy in silicon10.1063/1.4803547 ↗
36. Formation, dissociation, and diffusion of various hydrogen dimers in silicon
37. Easy-to-apply methodology to measure the hydrogen concentration in boron-doped crystalline silicon
38. Formation dynamics of BH and GaH-pairs in crystalline silicon during dark annealing
39. Study on boron–hydrogen pairs in bare and passivated float-zone silicon wafers
40. Modulation of carrier-induced defect kinetics in multi-crystalline silicon PERC cells through dark annealing10.1002/solr.201600028 ↗
41. Impact of dark annealing on the kinetics of light- and elevated-temperature-induced degradation10.1109/JPHOTOV.2018.2866325 ↗
42. A four-state kinetic model for the carrier-induced degradation in multicrystalline silicon: Introducing the reservoir state10.1016/j.solmat.2018.04.024 ↗
43. Disappearance of hydrogen-boron pairs in silicon during illumination and its relevance to lifetime degradation and regeneration effects in solar cells
44. Deciphering the role of hydrogen in the degradation of silicon solar cells under light and elevated temperature10.1002/solr.202400457 ↗
45. Wafer FTIR - measuring interstitial oxygen on as cut and processed silicon wafers10.1016/j.egypro.2016.07.076 ↗
46. Reducing time and costs of FT-IR studies of the effect of SiNx, dopants, and emitter on hydrogen species in Si wafers and solar cell structures10.52825/siliconpv.v1i.840 ↗
47. Direct and indirect determination of hydrogen-boron complexes in float-zone silicon wafers10.1063/5.0089274 ↗
48. Hydrogen-related defects measured by infrared spectroscopy in multicrystalline silicon wafers throughout an illuminated annealing process10.1063/1.5142476 ↗
49. Tutorial: Novel properties of defects in semiconductors revealed by their vibrational spectra10.1063/1.5011036 ↗
50. Concentration of atomic hydrogen diffused into silicon in the temperature range 900-1300 °C10.1063/1.104726 ↗
51. Contactless determination of current-voltage characteristics and minority-carrier lifetimes in semiconductors from quasi-steady-state photoconductance data10.1063/1.117723 ↗
52. Quantifying surface recombination - improvements in determination and simulation of the surface recombination parameter J0s10.1109/JPHOTOV.2023.3265859 ↗
53. Pearton · 1992
54. Understanding the impact of the cooling ramp of the fast-firing process on light- and elevated-temperature-induced degradation
55. Doping dependence of boron-hydrogen dynamics in crystalline silicon10.1063/5.0215089 ↗
56. H interacting with intrinsic defects in Si10.4028/www.scientific.net/MSF.196-201.933 ↗
57. Interaction of hydrogen with carbon in multicrystalline Si solar-cell materials10.1063/1.3561367 ↗
58. Structure, energetics, and dissociation of Si-H bonds at dangling bonds in silicon10.1103/PhysRevB.49.14766 ↗
59. Hydrogen in C-rich Si and the diffusion of vacancy-H complexes
60. Dynamics of hydrogen in silicon at finite temperatures from first principles
61. Hydrogen in crystalline semiconductors10.1007/BF00615975 ↗
62. Microscopic structure of a VH4 center trapped by C in Si10.1103/PhysRevB.84.195205 ↗
63. Temporary recovery of the defect responsible for light- and elevated temperature-induced degradation: Insights into the physical mechanisms behind LeTID10.1109/JPHOTOV.2020.3025240 ↗
64. Optical Absorption of Impurities and Defects in Semiconducting Crystals10.1007/978-3-642-18018-7 ↗
65. Local vibrational modes of the metastable dicarbon center (Cs–Ci) in silicon10.1103/PhysRevB.60.8081 ↗
66. Method to determine carbon in silicon by infrared absorption spectroscopy10.1149/1.1589023 ↗
67. Cs–H2* defect in crystalline silicon10.1016/S0921-4526(01)00432-X ↗
68. Weakly bound carbon-hydrogen complex in silicon10.1103/PhysRevB.61.16659 ↗
69. Hydrogen dependent surface morphology study of plasma deposited SiN x:H films for two gas systems SiH4/NH3 and SiH4/N210.1166/jnn.2011.4096 ↗
70. Low-temperature conformal atomic layer deposition of SiNx films using Si2Cl6 and NH3 plasma10.1021/acsami.5b01531 ↗