Recombination activity of oxide precipitates with iron decoration in silicon
Source abstract
Abstract
Oxide precipitates are common defects in Czochralski-grown silicon material, which introduce recombination centers and limit the subsequent device efficiency. Moreover, iron contamination in silicon is known to decorate the oxide precipitates and significantly increase their recombination activity. In this study, we aim to quantify this increased recombination activity by analyzing the injection-dependent lifetime spectroscopy (IDLS) of n-type Czochralski silicon wafers containing oxide precipitates with or without iron contamination. The previously reported energy levels and capture coefficient ratios of oxide precipitates in silicon [Murphy et al. (2012).] were found to provide a good fitting to our experimental data, for both samples with and without iron, which suggests that iron decoration is unlikely to change those defect parameters of oxide precipitates, confirming previous reports. The product of capture coefficient for holes and defect density was extracted for each defect, with a variety of process conditions being examined: oxide precipitate growth time, cooling rate after thermal anneal, and subsequent phosphorus diffusion gettering. Fe decoration of oxide precipitates was found to enhance the recombination rate, the extent of which is not related to the cooling rates used in this study. A longer oxide precipitate growth anneal was found to introduce more recombination centers, with the recombination rate being similarly enhanced after iron decoration. Lastly, a phosphorus diffusion gettering step can fully reverse the impact of iron decoration for the conditions applied in this study, which is likely due to the lack of large iron precipitates formed during the applied cooling processes. • Injection-dependent lifetime spectroscopy reveals the recombination activity of oxide precipitates. • Iron decoration significantly enhances the recombination rate of oxide precipitates. • Phosphorus gettering effectively reverses iron decoration, restoring carrier lifetimes. • Cooling rate variations in this work have a negligible impact on oxide precipitate recombination behavior. • Findings provide key insights for optimizing silicon solar cell fabrication.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Metallurgical Processes and Thermodynamics · Iron and Steelmaking Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Investigating wafer quality in industrial czochralski-grown gallium-doped p-type silicon ingots with melt recharging10.1002/solr.202300304 ↗
2. Industrial Czochralski n-type silicon wafers: gettering effectiveness and possible bulk limiting defects10.1002/solr.202300928 ↗
3. Auger-limited bulk lifetimes in industrial Czochralski-grown n-type silicon ingots with melt recharging10.1016/j.solmat.2024.113143 ↗
4. Direct comparison of boron, phosphorus, and aluminum gettering of iron in crystalline silicon10.1063/1.3569890 ↗
5. Effective impurity gettering by phosphorus- and boron-diffused polysilicon passivating contacts for silicon solar cells10.1016/j.solmat.2017.11.004 ↗
6. Gettering in silicon photovoltaics: a review
7. Comparing the gettering effect of heavily doped polysilicon films and its implications for tunnel oxide-passivated contact solar cells10.1002/solr.202370081 ↗
8. Effect of oxygen precipitation on the performance of Czochralski silicon solar cells10.1016/j.solmat.2011.06.044 ↗
9. Thermal History Index as a bulk quality indicator for Czochralski solar wafers10.1016/j.solmat.2016.05.051 ↗
10. Onset of ring defects in n-type Czochralski-grown silicon wafers10.1063/5.0005899 ↗
11. Experimental and theoretical study of oxygen precipitation and the resulting limitation of silicon solar cell wafers10.1109/JPHOTOV.2020.3044353 ↗
12. Detecting efficiency-limiting defects in Czochralski-grown silicon wafers in solar cell production using photoluminescence imaging10.1002/pssr.201105183 ↗
13. Ring defects in n-type Czochralski-grown silicon: a high spatial resolution study using Fourier-transform infrared spectroscopy, micro-photoluminescence, and micro-Raman10.1063/1.5057724 ↗
14. On the nature of striations in n-type silicon solar cells10.1063/1.4959558 ↗
15. Ring-like defect formation in N-type czochralski-grown silicon wafers during thermal donor formation
16. The effect of oxide precipitates on minority carrier lifetime in p-type silicon10.1063/1.3632067 ↗
17. The effect of oxide precipitates on minority carrier lifetime in n -type silicon10.1063/1.4936852 ↗
18. Electron spin resonance centers associated with oxygen precipitates in Czochralski silicon crystals10.1063/1.1305325 ↗
19. Spin-dependent recombination in Czochralski silicon containing oxide precipitates10.1063/1.3675449 ↗
20. On the mechanism of recombination at oxide precipitates in silicon10.1063/1.4789858 ↗
21. Passivation and depassivation of silicon dangling bonds at the Si/SiO 2 interface by atomic hydrogen10.1063/1.110758 ↗
22. Hydrogen passivation of defect-rich n-type Czochralski silicon and oxygen precipitates10.1016/j.solmat.2015.05.009 ↗
23. EBIC investigations of dislocations and their interactions with impurities in silicon10.1002/pssa.2211380241 ↗
24. Electrical characteristics of oxygen precipitation related defects in Czochralski silicon wafers10.1016/0921-5107(95)01289-3 ↗
25. Recombination activity of contaminated dislocations in silicon: a model describing electron-beam-induced current contrast behavior10.1103/PhysRevB.63.115208 ↗
26. Competitive gettering of iron in silicon photovoltaics: oxide precipitates versus phosphorus diffusion10.1063/1.4892015 ↗
27. Onset of implant-related recombination in self-ion implanted and annealed crystalline silicon10.1063/1.1789630 ↗
28. Superacid passivation of crystalline silicon surfaces10.1021/acsami.6b07822 ↗
29. Room temperature enhancement of electronic materials by superacid analogues10.1021/acsnano.1c09085 ↗
30. Gettering of interstitial iron in silicon by plasma-enhanced chemical vapour deposited silicon nitride films10.1063/1.4967914 ↗
31. Impurity gettering effect of atomic layer deposited aluminium oxide films on silicon wafers10.1063/1.4983380 ↗
32. Contactless determination of current-voltage characteristics and minority-carrier lifetimes in semiconductors from quasi-steady-state photoconductance data10.1063/1.117723 ↗
33. A fast, preparation-free method to detect iron in silicon10.1063/1.345063 ↗
34. Iron detection in crystalline silicon by carrier lifetime measurements for arbitrary injection and doping10.1063/1.1637136 ↗
35. Doping dependence of the carrier lifetime crossover point upon dissociation of iron-boron pairs in crystalline silicon10.1063/1.2358126 ↗
36. Parameterisation of injection-dependent lifetime measurements in semiconductors in terms of Shockley-Read-Hall statistics: an application to oxide precipitates in silicon10.1063/1.4725475 ↗
37. Identification of lifetime limiting defects by temperature- and injection-dependent photoluminescence imaging10.1063/1.4961465 ↗
38. Comprehensive model for charge carrier recombination in czochralski-grown silicon due to oxygen precipitation in industrial solar cell manufacturing10.1002/solr.202200980 ↗
39. Iron and its complexes in silicon10.1007/s003390050968 ↗
40. Gettering of iron by oxygen precipitates10.1063/1.120592 ↗
41. Effective impurity gettering by phosphorus- and boron-diffused polysilicon passivating contacts for silicon solar cells10.1016/j.solmat.2017.11.004 ↗
42. Precipitation of iron in multicrystalline silicon during annealing10.1063/1.4868587 ↗
43. Iron precipitation at oxygen related bulk defects in Czochralski silicon10.1063/1.361755 ↗
44. Iron-oxygen interaction in silicon: a combined XBIC/XRF-EBIC-DLTS study of precipitation and complex building10.1016/j.physb.2009.08.132 ↗
45. Iron distribution in silicon after solar cell processing: synchrotron analysis and predictive modeling10.1063/1.3575583 ↗
46. Fundamental properties of intrinsic gettering of iron in a silicon wafer10.1063/1.351764 ↗
47. Experimental and theoretical study of heterogeneous iron precipitation in silicon10.1063/1.2472271 ↗
48. Chemical natures and distributions of metal impurities in multicrystalline silicon materials10.1002/pip.690 ↗
49. Recombination activity of interstitial iron and other transition metal point defects in p- and n-type crystalline silicon10.1063/1.1812833 ↗
50. Effect of metal impurities concentration on electrical properties in N-type Recharged-Czochralski silicon