journal article·2022-10

An industrial scale solution to achieving light-induced degradation (LID) free silicon solar systems: >5% performance gain at system level with advanced hydrogenation technology

Z.P. Ling, Q.X. Lim, K.N. Lim, J.W. Ho, S. Wang

Publisher page

Abstract

Light-induced degradation (LID) and light- and elevated-temperature induced degradation (LeTID) effects in p-type monocrystalline silicon (Si) passivated emitter and rear contact (PERC) cell structure have been extensively studied in recent years. Various advanced hydrogenation techniques were previously reported, and aimed to eliminate or at least minimize the effect of LID/LeTID on solar cell performance stability. However, there are limited reports on the long-term performance of solar modules which comprise of these treated solar cells and deployed in typical outdoor conditions. This work aims to provide quantified outdoor performance data for comparing solar modules that are comprised of either hydrogenated or non-hydrogenated reference p-PERC silicon solar cells. A total of 1150 solar modules (>82,000 p-PERC silicon solar cells) were deployed on a commercial building rooftop with identical placement and real-time performance monitoring over an extended period of 12 months under standard outdoor conditions. The results showed that effective advanced hydrogenation is achievable with process time as short as 5 s, although a longer process time of 10–15 s delivered optimal results. The advanced hydrogenation technology in this work can effectively address the LID and LeTID issues on the cell, module, and system levels, with >5% higher power generation capability on hydrogenated solar arrays as compared to the non-hydrogenated reference. Solar cell and module manufacturers strive to produce products with long-term stability, and the successful demonstration of the advanced hydrogenation technology in this work could serve this demand. A future perspective for advanced hydrogenation technologies is also presented.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Photovoltaic System Optimization Techniques · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. 2019
2. 2021
3. Fischer
4. Summary for policymakers
5. Investigation of photon and thermal changes in silicon solar cells
6. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
7. Rapid stabilization of high-performance multicrystalline P-type silicon PERC cells10.1109/JPHOTOV.2016.2606704 ↗
8. Engineering solutions and root-cause analysis for light-induced degradation in p-type multicrystalline silicon PERC modules10.1109/JPHOTOV.2016.2556981 ↗
9. Lifetime degradation and regeneration in multicrystalline silicon under illumination at elevated temperature10.1063/1.4944839 ↗
10. Impact of the firing temperature profile on light induced degradation of multicrystalline silicon10.1002/pssr.201600272 ↗
11. Investigating possible causes of light induced degradation in boron-doped float-zone silicon
12. Firing temperature profile impact on light induced degradation in multicrystalline silicon10.1016/j.egypro.2017.09.082 ↗
13. Impact of rapid firing thermal processes on meta-stable defects: preformation of the LeTID and the suppression of B-O defects
14. Light-induced degradation of PECVD aluminium oxide passivated silicon solar cells10.1002/pssr.201409424 ↗
15. Light-induced degradation of silicon solar cells with aluminiumoxide passivated rear side10.1016/j.egypro.2015.07.086 ↗
16. Influence of Al2O3 and SiNx passivation layers on LeTID10.1016/j.egypro.2016.07.079 ↗
17. Degradation of crystalline silicon due to boron–oxygen defects10.1109/JPHOTOV.2016.2614119 ↗
18. Modelling kinetics of the boron-oxygen defect system10.1016/j.egypro.2016.07.008 ↗
19. Natural recovery from LID: regeneration under field conditions
20. Modelling the long-term behaviour of boron-oxygen defect passivation in the field using typical meteorological year data (TMY2)
21. Structure and transformation of the metastable boron- and oxygen-related defect center in crystalline silicon10.1103/PhysRevB.69.024107 ↗
22. Advanced bulk defect passivation for silicon solar cells10.1109/JPHOTOV.2013.2281732 ↗
23. A unified approach to modelling the charge state of monatomic hydrogen and other defects in crystalline silicon10.1063/1.4906465 ↗
24. Rapid mitigation of carrier-induced degradation in commercial silicon solar cells10.7567/JJAP.56.08MB13 ↗
25. Advanced hydrogenation of dislocation clusters and boron-oxygen defects in silicon solar cells10.1016/j.egypro.2015.07.113 ↗
26. Lifetime instabilities in gallium doped monocrystalline PERC silicon solar cells10.1016/j.solmat.2019.110299 ↗
27. High efficiency gallium doped and boron doped multicrystalline silicon solar cells
28. Solar
29. Light-induced activation and deactivation of bulk defects in boron-doped float-zone silicon10.1063/1.4983024 ↗
30. Light-induced degradation and regeneration in n-type silicon10.1016/j.egypro.2015.07.090 ↗
31. Investigation of light-induced degradation in N-Type silicon heterojunction solar cells during illuminated annealing at elevated temperatures10.1016/j.solmat.2020.110752 ↗
32. Hydrogen induced degradation: a possible mechanism for light- and elevated temperature- induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
33. Potential-induced degradation in photovoltaic modules: a critical review10.1039/C6EE02271E ↗
34. Research on hot spot risk for high-efficiency solar module10.1016/j.egypro.2017.09.399 ↗
35. Attaining a 30-year photovoltaic system lifetime: the BOS issues10.1002/pip.4670020205 ↗
36. Failure modes evaluation of PV module via materials degradation approach10.1016/j.egypro.2013.05.066 ↗
37. Jordan · 2015
38. Eliminating light-induced degradation in commercial p-type czochralski silicon solar cells10.3390/app8010010 ↗
39. Development of advanced hydrogenation processes for silicon solar cells via an improved understanding of the behaviour of hydrogen in silicon10.1002/pip.3240 ↗
40. LEDs for the implementation of advanced hydrogenation using hydrogen charge-state control10.1155/2018/2439425 ↗
41. Hydrogenation behaviors in passivated emitter and rear silicon solar cells with variously hydrogenated SiNx films10.1016/j.apsusc.2020.146386 ↗
42. The investigation on hydrogenation platform for silicon solar cells based on high intensity infrared LEDs10.1063/1.5012781 ↗
43. Status review and future perspectives on mitigating light-induced degradation on silicon-based solar cells10.1016/j.rser.2022.112223 ↗
44. Progress in the understanding of light- and elevated temperature-induced degradation in silicon solar cells: a review
45. Elimination of BO-LID in mass production using illuminated annealing in a coupled firing and regeneration tool10.1063/1.5049321 ↗
46. Systems
47. Influence of double current injection annealing on anti-LID effect in mono-like cast silicon PERC solar cells10.1007/s10854-020-02870-5 ↗
48. 5 - case studies: photoluminescence characterization
49. Rapid passivation of carrier-induced defects in p-type multi-crystalline silicon10.1016/j.solmat.2016.05.022 ↗