Estimation of solar receiver corrosion conditions during operation to aid in the design of receiver-corrosion lab tests
Source abstract
Abstract
Solar power tower plants widely rely on molten nitrite salt as heat transfer fluid and storage media. However, its corrosiveness endangers several metallic components, with central receivers being one of the most compromised. Great efforts are being made to establish molten salt corrosion in different metals. Recently, the importance of the amount of salt used in these experiments has been highlighted. Yet, most tests disregard the hot-receiver-surface/salt ratio that would represent the receiver operation conditions. Commonly, larger metal surfaces are employed, accelerating molten salt thermal decomposition kinetics. Hence, this study seeks to develop basic design conditions for experimental corrosion tests to realistically mimic receiver-tube corrosion. Consequently, the high-temperature operation of two receiver designs, resembling those of Crescent Dunes and Gemasolar plants, with their tubes manufactured in HA230, is analysed. The yearly salt degradation in these plants is found to be nearly negligible due to the large salt volume stored and the relatively limited receiver surface above concerning temperatures, with the whole salt volume being exposed to it for around 20 min during a 25-year operation for large receivers. Moreover, the hot-metal-surface/solar-salt ratio ranges from 5 to 7 mm2/kg, depending on the receiver design, which should be preserved in a corrosion experiment. Metal loss is also estimated: less than 7 % of the receiver would lose at least 50 % of the initial tube thickness. Still, lower metal loss rates are expected since coefficients from static-isothermal tests were employed for the calculation, which also disregarded the metal surface/salt proportion, leading to an overestimation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Solar Thermal and Photovoltaic Systems · Solar-Powered Water Purification Methods · Nanofluid Flow and Heat Transfer
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. An evaluation of molten-salt power towers including results of the solar two project
2. Mehos · 2020
3. The power production operation of solar one, the 10 MWe solar thermal central receiver pilot plant10.1115/1.3268300 ↗
4. High temperature properties and decomposition of inorganic salts Part 3, nitrates and nitrites10.1063/1.3253104 ↗
5. The kinetics of the thermal decomposition of sodium nitrate and of the reaction between sodium nitrite and oxygen10.1021/j150545a005 ↗
6. The kinetics of the thermal decomposition of potassium nitrate and of the reaction between potassium nitrite and oxygen10.1021/ja01561a015 ↗
7. The thermal stability of binary alkali metal nitrates10.1016/0040-6031(84)87150-6 ↗
8. Tilley · 2014
9. High-temperature stability of nitrate/nitrite molten salt mixtures under different atmospheres10.1016/j.apenergy.2018.05.101 ↗
10. Nitrate/nitrite chemistry in NaNO3-KNO3 melts10.1021/ic00147a004 ↗
11. Solar Salt – pushing an old material for energy storage to a new limit10.1016/j.apenergy.2020.114535 ↗
12. Investigation of regeneration mechanisms of aged solar salt10.3390/ma14195664 ↗
13. A review of the chemical and physical properties of molten alkali nitrate salts and their effect on materials used for solar central receivers
14. Kruizenga · 2013
15. Kruizenga · 2013
16. Molten nitrate salts at 600 and 680°C: thermophysical property changes and corrosion of high-temperature nickel alloys10.1016/j.solener.2014.01.028 ↗
17. Effect of thermal cycling on the corrosion behaviour of stainless steels and Ni-based alloys in molten salts under air and argon10.1016/j.solener.2022.04.041 ↗
18. Comparative review of different influence factors on molten salt corrosion characteristics for thermal energy storage10.1016/j.solmat.2021.111485 ↗
19. Dynamic corrosion testing of metals in solar salt for concentrated solar power10.1016/j.solmat.2021.111331 ↗
20. Concentrating solar power at higher limits: studies on molten nitrate salts at 620°C in a laboratory pilot‐scale hot tank10.1002/cite.202255349 ↗
21. Bradshaw · 2001
22. The corrosion behaviour of stainless steels and Ni-based alloys in nitrate salts under thermal cycling conditions in concentrated solar power plants10.1016/j.solener.2021.12.072 ↗
23. Solar thermal irradiation cycles and their influence on the corrosion behaviour of stainless steels with molten salt used in concentrated solar power plants10.1016/j.solmat.2022.112141 ↗
24. Experimental research of high temperature dynamic corrosion characteristic of stainless steels in nitrate eutectic molten salt10.1016/j.solener.2020.09.034 ↗
25. Corrosion of stainless steels and carbon steel by molten mixtures of commercial nitrate salts10.1361/10599490417542 ↗
26. Dynamic corrosion behavior of 316L stainless steel in quaternary nitrate-nitrite salts under different flow rates10.1016/j.solmat.2020.110821 ↗
27. Thermal design guidelines of solar power towers10.1016/j.applthermaleng.2013.11.014 ↗
28. Gemasolar, the first tower thermosolar commercial plant with molten salt storage
29. Advances in central receivers for concentrating solar applications10.1016/j.solener.2017.03.048 ↗
30. Lovegrove · 2012
31. Flow patterns of external solar receivers10.1016/j.solener.2015.10.025 ↗
32. Zavoico · 2001
33. American Society of Mechanical Engineers · 2010
34. Material selection for solar central receiver tubes10.1016/j.solmat.2021.111317 ↗
35. Morch · 2022
36. Haynes International · 2020
37. Wagner · 2008
38. Vant-Hull · 2012
39. Falcone · 1986
40. Reno · 2012
41. The role of “allowable flux density” in the design and operation of molten-salt solar central receivers10.1115/1.1464124 ↗
42. A procedure to predict solar receiver damage during transient conditions10.1016/j.rser.2021.111905 ↗
43. Thermal convection loop study of the corrosion of Incoloy 800 in molten NaNO3-KNO310.5006/1.3583131 ↗
44. Kinetics and mechanism of high temperature internal oxidation of Ni-14wt%W alloy at 1000°C10.4028/www.scientific.net/DDF.323-325.321 ↗
45. Principles and prevention of corrosion
46. Corrosion resistance of high nickel alloys in solar salt at 600°C for up to 4000 h10.1016/j.solmat.2022.111837 ↗
47. Solar flux distribution on central receivers: a projection method from analytic function10.1016/j.renene.2014.08.016 ↗
48. FluxSPT: tool for heliostat field aiming and flux mapping in solar power tower plants10.1063/5.0085656 ↗
49. Aiming factor to flatten the flux distribution on cylindrical receivers10.1016/j.energy.2018.04.002 ↗
50. Elevated temperature shakedown concepts10.1115/1.4003456 ↗
51. Barua · 2020
52. Comparison of simplified heat transfer models and CFD simulations for molten salt external receiver10.1016/j.applthermaleng.2014.08.072 ↗
53. Revised receiver efficiency of molten-salt power towers10.1016/j.rser.2015.08.004 ↗
54. Economic and thermo-mechanical design of tubular sCO2 central-receivers10.1016/j.renene.2021.06.047 ↗
55. Review of the API RP 14E erosional velocity equation: origin, applications, misuses, limitations and alternatives10.1016/j.wear.2019.01.119 ↗
56. Deflection and stresses in solar central receivers10.1016/j.solener.2019.11.066 ↗
57. Turbulent heat transfer in a circular tube with circumferentially varying thermal boundary conditions10.1016/0017-9310(74)90182-3 ↗
58. Velocity profile representation for fully developed turbulent flows in pipes: a modified power law10.3390/fluids6100369 ↗
59. Turbulent heat transfer in a circular tube with variable circumferential heat flux10.1016/0017-9310(63)90119-4 ↗
60. On turbulent flow near a wall10.2514/8.3713 ↗
61. Levenspiel · 1999
62. Picotti · 2022
63. Design, fabrication and testing of an apparatus for material compatibility testing in nitrate salts at temperatures up to 700°C