Residual impurities in a process chamber on the characteristics of a-Si:H solar cells
Source abstract
Abstract
Abstract Hydrogenated amorphous silicon (a-Si:H) p-i-n solar cells were grown in a single, non-load-locked chamber by using 13.56 MHz plasma. Residual air impurities were controlled with high vacuum pumping, or not controlled, and the concentrations were measured at the onset, before p-layer deposition. The low pressures (approximately 10 −7 –10 −8 Torr) of N 2 and O 2 near the lowest vacuum pressure of the chamber, incorporated base contamination levels of nitrogen and oxygen (approximately 10 18 –10 19 atoms/cm 3 ). High pressures of H 2 O (10 −5 –10 −6 Torr) resulted in extremely high oxygen contamination levels (approximately 10 21 atoms/cm 3 ), which was the dominant residual impurity. High concentration un-stabilized H 2 O showed a rapidly decreasing rate which induced non-uniform oxygen doping and resulted in a non-uniform distribution of the internal electric field in the i-layer. The net loss (ΔQE(0,V)) of quantum efficiency (QE) of the cells between zero and a forward bias showed the increase of QE loss in the long-wavelength region for increasing forward bias resulted in poor performance of the low fill factor and energy conversion efficiency, and a high series resistance of the cells. The removal of residual water vapor from the chamber is a key factor in improving the performance of a-Si:H solar cells.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Thin-Film Transistor Technologies · Silicon and Solar Cell Technologies · Silicon Nanostructures and Photoluminescence
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. Influence of N, O and C impurities in a-Si:H10.1016/S0022-3093(05)80138-3 ↗
2. Doping effect of oxygen or nitrogen impurity in hydrogenated amorphous silicon films10.1063/1.106102 ↗
3. Effects of the i-layer properties and impurity on the performance of a-Si solar cell10.1016/0927-0248(94)90054-X ↗
4. Influence of oxygen impurity in the intrinsic layer of amorphous silicon solar cells10.1063/1.112732 ↗
5. Influence of oxygen and nitrogen in the intrinsic layer of a-Si:H solar cells10.1143/JJAP.35.3819 ↗
6. Influence of base pressure and atmospheric contaminants on a-Si:H solar cell properties10.1063/1.3009384 ↗
7. Critical oxygen concentration in hydrogenated amorphous silicon solar cells dependent on the contamination source10.1063/1.3357424 ↗
8. Incorporation and critical concentration of oxygen in a-Si:H solar cells10.1016/j.solmat.2011.05.035 ↗
9. Impurities in thin-film silicon: influence on material properties and solar cell performance10.1016/j.jnoncrysol.2011.11.030 ↗
10. Kakiuchi · 2008 · 225
11. Nature of localized states in hydrogenated Si-base amorphous semiconductor films elucidated from LESR and CPM10.1143/JJAP.28.586 ↗