Enhancing dielectric-silicon interfaces through surface electric fields during firing
Source abstract
Abstract
Minimising charge losses at silicon interfaces is a major development area for highly efficient solar cells. Here we report on the interface improvements achieved by establishing a surface electric field during low-temperature firing of dielectric thin films. By inducing a corona electric field on the surface of a thin film stack, we observe significant modifications to the silicon-dielectric interface upon annealing, which correlate with the characteristics of interface defects. The passivation properties of the interfaces strongly depend on the polarity and strength of the electric field during firing, as well as the dielectric materials in the layer stack. We show that the surface electric fields not only influence surface carrier population but also affect the resulting chemical interface properties post-annealing. It is postulated that hydrogen migration plays a role in these observed effects. Leveraging the corona-induced electric field enables fine-tuning of both the chemical and field-effect passivation in thin film surface dielectrics, resulting in recombination current densities as low as 2.8 fA cm−2 in research-grade float zone silicon, and 14 fA cm−2 in industrial-grade textured silicon. The simplicity and versatility of the thin film electric polarisation enable a new strategy for controlling and exploiting the chemical enhancement of interfaces in solar cell devices, from current TOPCon and PERC devices to future multijunction silicon-based cells.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and devices · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Crystalline silicon photovoltaics: a cost analysis framework for determining technology pathways to reach baseload electricity costs10.1039/c2ee03489a ↗
2. Photovoltaics at multi-terawatt scale: Waiting is not an option
3. Commercial progress and challenges for photovoltaics10.1038/nenergy.2015.15 ↗
4. Surface passivation of crystalline silicon solar cells: present and future10.1016/j.solmat.2018.06.047 ↗
5. Surface passivation of crystalline silicon solar cells: a review10.1002/1099-159X(200009/10)8:5<473::AID-PIP337>3.0.CO;2-D ↗
6. Surface passivation of silicon solar cells using plasma-enhanced chemical-vapour-deposited SiN films and thin thermal SiO 2/plasma SiN stacks10.1088/0268-1242/16/3/308 ↗
7. Carrier population control and surface passivation in solar cells10.1016/j.solmat.2018.04.026 ↗
8. Advances in the surface passivation of silicon solar cells10.1016/j.egypro.2012.02.004 ↗
9. Field-effect passivation of the SiO2Si interface10.1063/1.370784 ↗
10. Potassium ions in SiO 2 : electrets for silicon surface passivation10.1088/1361-6463/aa9b1b ↗
11. Scalable techniques for producing field-effect passivation in high-efficiency silicon solar cells10.1109/JPHOTOV.2018.2872032 ↗
12. Bulk and surface passivation of silicon solar cells accomplished by silicon nitride deposited on industrial scale by microwave PECVD10.1002/pip.611 ↗
13. Passivation and depassivation of silicon dangling bonds at the Si/SiO 2 interface by atomic hydrogen10.1063/1.110758 ↗
14. An enhanced alneal process to produce SRV< 1 cm/s in 1 $Ω$ cm n-type Si10.1016/j.solmat.2017.06.022 ↗
15. Remote PECVD silicon nitride—a key technology for the crystalline silicon PV industry of the 21st century
16. Overview on SiN surface passivation of crystalline silicon solar cells10.1016/S0927-0248(00)00099-4 ↗
17. H loss mechanism during anneal of silicon nitride: chemical dissociation10.1063/1.1321730 ↗
18. Effect of precursors on propagation loss for plasma-enhanced chemical vapor deposition of SiN_x:H waveguides10.1364/OME.6.002892 ↗
19. Influence of the deposition temperature on the c-Si surface passivation by Al[sub 2]O[sub 3] films synthesized by ALD and PECVD10.1149/1.3276040 ↗
20. Reactions of hydrogen with Si-SiO/sub 2/interfaces10.1109/23.903763 ↗
21. Defect generation at charge-passivated Si–SiO2 interfaces by ultraviolet light10.1109/TED.2010.2051199 ↗
22. Universal alignment of hydrogen levels in semiconductors, insulators and solutions10.1038/nature01665 ↗
23. Dual role of fluorine at the Si–SiO2 interface10.1063/1.1825621 ↗
24. Defect generation by hydrogen at the Si-SiO2 interface10.1103/PhysRevLett.87.165506 ↗
25. Modelling of hydrogen transport in silicon solar cell structures under equilibrium conditions10.1063/1.5016854 ↗
26. Vacuum-free, room-temperature organic passivation of silicon: toward very low recombination of micro-/nanotextured surface structures10.1021/acsami.8b17379 ↗
27. Development of passivating edge shingle modules with right cut, new loss evaluation and liquid-based edge passivation strategy10.1016/j.solmat.2023.112513 ↗
28. Enhanced surface passivation of subnanometer silicon dioxide films by superacidic treatments10.1021/acsaem.1c02935 ↗
29. In-line and vertical texturing of mono-crystalline solar cells
30. Controlling surface carrier density via a PEDOT:PSS gate: an application to the study of silicon-dielectric interface recombination10.1002/solr.201800172 ↗
31. Effect of annealing on performance of PEDOT:PSS/n-GaN Schottky solar cells10.1088/1674-1056/23/7/077303 ↗
32. Effects of layer thickness and annealing of PEDOT:PSS layers in organic photodetectors10.1021/ma901182u ↗
33. Determination of Si-SiO2 interface recombination parameters using a gate-controlled point-junction diode under illumination10.1109/16.2441 ↗
34. Charge fluctuations at the Si–SiO2 interface and its effect on surface recombination in solar cells10.1016/j.solmat.2020.110649 ↗
35. On the c-Si/SiO2 interface recombination parameters from photo-conductance decay measurements10.1063/1.4979722 ↗
36. Statistics of the recombinations of holes and electrons10.1103/PhysRev.87.835 ↗
37. Carrier-diffusion corrected J0-analysis of charge carrier lifetime measurements for increased consistency10.1016/j.solmat.2015.06.043 ↗
38. On the determination of the emitter saturation current density from lifetime measurements of silicon devices10.1002/pip.2167 ↗
39. Measurement of the emitter saturation current by a contactless photoconductivity decay method
40. Reassessment of the intrinsic bulk recombination in crystalline silicon10.1016/j.solmat.2021.111467 ↗
41. Dispersion-related description of temperature dependencies of band gaps in semiconductors10.1103/PhysRevB.66.085201 ↗
42. Quantifying surface recombination - improvements in determination and simulation of the surface recombination parameter J0s10.1109/JPHOTOV.2023.3265859 ↗
43. The influence of surface electric fields on the chemical passivation of Si-SiO2 interfaces after firing10.1063/5.0089930 ↗
44. Long term stability of c-Si surface passivation using corona charged SiO210.1016/j.apsusc.2017.03.204 ↗
45. Corona charge in SiO2: kinetics and surface passivation for high efficiency silicon solar cells10.1016/j.egypro.2016.07.090 ↗
46. Passivation of textured silicon wafers:influence of pyramid size distribution, a-Si:H deposition temperature, and post-treatment10.1016/j.egypro.2013.07.360 ↗
47. Influence of pyramid size of chemically textured silicon wafers on the characteristics of industrial solar cells, 25th European Photovoltaic Solar Energy Conference and Exhibition
48. Recombination at textured silicon surfaces passivated with silicon dioxide10.1063/1.3153979 ↗
49. Trap creation in silicon dioxide produced by hot electrons10.1063/1.342824 ↗
50. Hot-electron-induced hydrogen redistribution and defect generation in metal-oxide-semiconductor capacitors10.1063/1.357420 ↗
51. Hydrogen related defects in float zone silicon investigated using a shielded hydrogen plasma
52. Hydrogen-induced degradation
53. Hydrogen induced degradation: a possible mechanism for light- and elevated temperature- induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
54. Energetics and diffusion of hydrogen in SiO210.1103/PhysRevB.61.4417 ↗
55. Diffusion and permeation of He, Ne, Ar, Kr, and D2 through silicon oxide thin films10.1063/1.1675072 ↗
56. Very low surface recombination velocity in n-type c-Si using extrinsic field effect passivation10.1063/1.4892099 ↗
57. Dielectric surface passivation for silicon solar cells: a review
58. The contribution of planes, vertices, and edges to recombination at pyramidally textured surfaces10.1109/JPHOTOV.2011.2165530 ↗
59. Exceptional silicon surface passivation by an ONO dielectric stack10.1016/j.solmat.2018.05.061 ↗
60. Bias-voltage photoconductance and photoluminescence for the determination of silicon-dielectric interface properties in SiO2/Al2O3 stacks10.1063/5.0153204 ↗
61. Low temperature surface passivation for silicon solar cells10.1016/0927-0248(95)00155-7 ↗
62. Interface states and fixed charges in MNOS structures with APCVD and plasma silicon nitride10.1149/1.2115936 ↗
63. Electronic structure of hydrogen- and alkali-metal-vacancy complexes in silicon10.1103/PhysRevB.29.1819 ↗
64. Similarities in the electrical properties of transition metal–hydrogen complexes in silicon10.1016/S0921-5107(98)00282-7 ↗
65. Deep levels of chromium‐hydrogen complexes in silicon10.1063/1.356018 ↗
66. Extremely low surface recombination in 1 Ω cm n-type monocrystalline silicon
67. An improved methodology for extracting the interface defect density of passivated silicon solar cells10.1109/JPHOTOV.2016.2576685 ↗
68. Effect of surface texture on pinhole formation in SiO x-based passivated contacts for high-performance silicon solar cells10.1021/acsami.0c12795 ↗
69. Structural and passivating properties of SiNx:H deposited under different precursor gases
70. Impact of hydrogen‐rich silicon nitride material properties on light‐induced lifetime degradation in multicrystalline silicon10.1002/pssr.201900201 ↗
71. Study of the composition of hydrogenated silicon nitride SiNx:H for efficient surface and bulk passivation of silicon10.1016/j.solmat.2009.01.023 ↗
72. Manipulation of K center charge states in silicon nitride films to achieve excellent surface passivation for silicon solar cells10.1063/1.4863829 ↗
73. Characterisation and optimisation of PECVD SiNx as an antireflection coating and passivation layer for silicon solar cells10.1063/1.4795108 ↗
74. Development of advanced hydrogenation processes for silicon solar cells via an improved understanding of the behaviour of hydrogen in silicon10.1002/pip.3240 ↗
75. Effects of hydrogen annealing on silicon surfaces
76. Application of wide-bandgap hydrogenated amorphous silicon oxide layers to heterojunction solar cells for high quality passivation
77. Invasive nature of corona charging on thermal Si/SiO2 structures with nanometer-thick oxides revealed by electron spin resonance10.1063/1.1540245 ↗
78. Passivation of P b 0 and P b 1 interface defects in thermal (100) Si/SiO2 with molecular hydrogen10.1063/1.116308 ↗
79. Dissociation kinetics of hydrogen-passivated (100) Si/SiO2 interface defects10.1063/1.359148 ↗
80. Hydrogen induced donor-type Si/SiO2 interface states10.1063/1.112696 ↗
81. Kinetics of H2 passivation of Pb centers at the (111) Si-SiO2 interface10.1103/PhysRevB.38.9657 ↗
82. Interface state energy distribution and Pb defects at Si(110)/SiO2 interfaces: comparison to (111) and (100) silicon orientations10.1063/1.3527909 ↗
83. Chemical kinetics of hydrogen and (111) Si-SiO2 interface defects10.1063/1.103971 ↗
84. Revision of H2 passivation of Pb interface defects in standard (111)Si/SiO210.1063/1.115577 ↗
85. Electrical characterization of Pb centers in (100)Si–SiO2 structures: the influence of surface potential on passivation during post metallization anneal10.1063/1.373759 ↗
86. Comparative analysis of the H2 passivation of interface defects at the interface using electron spin resonance10.1016/0038-1098(95)00535-8 ↗
87. Dissociation kinetics of hydrogen-passivated (111) Si-SiO2 interface defects10.1103/PhysRevB.42.3444 ↗
88. Chemistry of Si-SiO2 interface trap annealing10.1063/1.340317 ↗
89. Thermally induced interface degradation in (100) and (111) Si/SiO2 analyzed by electron spin resonance10.1116/1.590449 ↗
90. The effects of water on oxide and interface trapped charge generation in thermal SiO2 films10.1063/1.329502 ↗
91. Elimination and generation of Si ‐ SiO2 interface traps by low temperature hydrogen annealing10.1149/1.2096133 ↗
92. Defect generation at the Si–SiO2 interface following corona charging10.1063/1.2749867 ↗
93. Decreasing interface defect densities via silicon oxide passivation at temperatures below 450 °C10.1021/acsami.0c12636 ↗
94. Hole injection and transport in SiO2 films on Si10.1063/1.88522 ↗
95. Hole traps in silicon dioxide10.1063/1.322730 ↗
96. High-field transport in SiO2 on silicon induced by corona charging of the unmetallized surface10.1063/1.322307 ↗
97. Post-irradiation cracking of H2 and formation of interface states in irradiated metal-oxide-semiconductor field-effect transistors10.1063/1.353348 ↗
98. Simultaneous elimination of electrically active defects in Si/SiO2 structures by implanted fluorine10.1016/0167-9317(93)90138-U ↗
99. Spatial distribution of trapped holes in SiO210.1063/1.357242 ↗
100. An investigation on anomalous hot-carrier-induced on-resistance reduction in n-type LDMOS transistors10.1109/TDMR.2009.2025770 ↗