journal article·2019-09Open access

Lifetime spectroscopy with high spatial resolution based on temperature- and injection dependent photoluminescence imaging

Halvard Haug, Rune Søndenå, Amalie Berg, Marie Syre Wiig

Abstract

Abstract In this paper we present a method for performing temperature- and injection dependent lifetime spectroscopy (TIDLS) with high spatial resolution based on steady state photoluminescence (PL) images taken at a range of excitation intensities and temperatures. The PL lifetime images are calibrated based on temperature dependent photoconductance measurements, thus requiring a minimum of assumptions regarding the temperature dependency of the luminescence signal and detection system. PL image acquisition at varying conditions and subsequent data analysis is automated, allowing for investigations of different samples without the need for excessive operator time. We demonstrate the method by presenting lifetime data and TIDLS analysis from commercial HPMC-Si samples, highlighting the local differences in the recombination properties for high lifetime in-grain areas and lower lifetime areas dominated by dislocation clusters. These regions have been investigated for two etched and passivated neighboring wafers, one in the as-cut state and one where the bulk lifetime had been improved through key solar cell process steps. For the as-cut wafer we find two dominant defects in the low lifetime area, one of which is identified as FeB pairs, with E t = 0.90 ± 0.01 (above the valence band) and k = 0.4 ± 0.1. In the in-grain region of this wafer we also observe two dominating defects, one with an energy level of either 0.28 ± 0.01 eV or 0.74 ± 0.01 eV above the valence band and a k value of 25 ± 1. The other defect is shallow, within ~0.27 eV of the band edge, and could not be further identified with the chosen temperature range. For the wafer that had passed through solar cell processing, we find a clear, overall improvement in the lifetime and a change in the type of dominating defects: We observe that a single, deep defect with 0.35 eV E t eV and a capture cross section ratio k = 10 ± 1 can fully describe the observed lifetime data in the in-grain area after solar cell processing, whereas two defects are needed to describe the behavior of the lower lifetime regions. One of these defects is also a deep defect with 0.34 eV E t eV but with a higher k of 25 ± 2, and is thus similar to one of the defects observed in the in-grain region of the as-cut wafer. The other is a shallow defect with E t within 0.21 eV of the band edge. Finally, we show how the method can be used to show interesting new properties of the lifetime maps, including maps of the temperature coefficient of the lifetime, maps of the injection dependence of the lifetime and maps at a constant injection level.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Integrated Circuits and Semiconductor Failure Analysis · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. The effect of oxide precipitates on minority carrier lifetime in p-type silicon10.1063/1.3632067 ↗
2. Characterization of oxidation-induced stacking fault rings in Cz silicon: photoluminescence imaging and visual inspection after wright etch10.1016/j.egypro.2012.07.045 ↗
3. Nano-XRF analysis of metal impurities distribution at PL active grain boundaries during mc-silicon solar cell processing10.1109/JPHOTOV.2016.2621340 ↗
4. Recombination sources in p-type high performance multicrystalline silicon10.7567/JJAP.56.08MB16 ↗
5. Recent insights into boron-oxygen related degradation: evidence of a single defect10.1016/j.solmat.2017.06.038 ↗
6. Evolution of the light sensitive defects in high performance multicrystalline silicon wafers10.1063/1.5079496 ↗
7. Understanding the light-induced degradation at elevated temperatures: similarities between multicrystalline and floatzone p-type silicon10.1002/pip.2954 ↗
8. Solar cell efficiency tables (Version 53)10.1002/pip.3102 ↗
9. Evaluation of possible mechanisms behind P gettering of iron10.1063/1.3607239 ↗
10. The effect of phosphorus diffusion gettering on recombination at grain boundaries in HPMC-silicon wafers10.1016/j.egypro.2016.07.098 ↗
11. Recombination in ingot cast silicon solar cells10.1002/pssa.201084022 ↗
12. Impact of phosphorous gettering and hydrogenation on the surface recombination velocity of grain boundaries in p-type multicrystalline silicon10.1109/JPHOTOV.2015.2455341 ↗
13. Rein · 2005
14. Lifetime spectroscopy investigation of light-induced degradation in p-type multicrystalline silicon PERC10.1109/JPHOTOV.2016.2606699 ↗
15. Recombination parameters of lifetime-limiting carrier-induced defects in multicrystalline silicon for solar cells10.1063/1.4977906 ↗
16. Harmonically modulated luminescence: bridging gaps in carrier lifetime metrology across the PV processing chain10.1109/JPHOTOV.2014.2362304 ↗
17. Mundt L. E. et al., “Spatially resolved impurity identification via temperature- and injection-dependent photoluminescence imaging,” photovoltaics, IEEE Journal of, vol. 5, no. 5. pp. 1503–1509, 2015.10.1109/JPHOTOV.2015.2447837 ↗
18. Identification of lifetime limiting defects by temperature- and injection-dependent photoluminescence imaging10.1063/1.4961465 ↗
19. Identifying recombination parameters by injection-dependent lifetime spectroscopy on mc-silicon based on photoluminescence imaging10.1063/1.5049336 ↗
20. Temperature dependent photoluminescence imaging calibrated by photoconductance measurements10.1016/j.egypro.2017.09.338 ↗
21. Cobalt related defect levels in silicon analyzed by temperature- and injection-dependent lifetime spectroscopy10.1063/1.2433743 ↗
22. Electronic properties of interstitial iron and iron-boron pairs determined by means of advanced lifetime spectroscopy10.1063/1.2106017 ↗
23. Recombination activity of light-activated copper defects in p-type silicon studied by injection- and temperature-dependent lifetime spectroscopy10.1063/1.4963121 ↗
24. Improved quantitative description of Auger recombination in crystalline silicon10.1103/PhysRevB.86.165202 ↗
25. Murphy · 2012 · vol. 111
26. Temperature dependent photoluminescence imaging calibrated by photoconductance measurements10.1016/j.egypro.2017.09.338 ↗
27. Temperature dependence of the radiative recombination coefficient of intrinsic crystalline silicon10.1063/1.1610231 ↗
28. Hameiri · 2015 · 1
29. Carrier mobilities in silicon semi-empirically related to temperature, doping and injection level10.1016/0038-1101(81)90097-6 ↗
30. Sinton-Instruments
31. An accurate method for calibrating photoluminescence-based lifetime images on multi-crystalline silicon wafers10.1016/j.solmat.2014.06.004 ↗
32. Photoconductance-calibrated photoluminescence lifetime imaging of crystalline silicon10.1002/pssr.200802192 ↗
33. On the use of a bias-light correction for trapping effects in photoconductance-based lifetime measurements of silicon10.1063/1.1346652 ↗
34. Study of evolution of dislocation clusters in high performance multicrystalline silicon10.1016/j.solmat.2014.02.034 ↗
35. Temperature coefficient imaging for silicon solar cells10.1109/JPHOTOV.2018.2828839 ↗
36. Carrier de-smearing of photoluminescence images on silicon wafers using the continuity equation10.1063/1.4829658 ↗
37. A high-accuracy calibration method for temperature dependent photoluminescence imaging (to be published)10.1063/1.5123812 ↗
38. Imaging interstitial iron concentrations in boron-doped crystalline silicon using photoluminescence10.1063/1.2903895 ↗