journal article·2022-08

High-temperature corrosion rate and diffusion modelling of Ni-coated incoloy 800H alloy in MgCl2–KCl heat transfer fluid

Yuxiang Peng, Pravin S. Shinde, Ramana G. Reddy

Publisher page

Abstract

The polarization and long-term dipping corrosion behaviors of pristine and Ni-coated Incoloy 800H (800H) alloys were investigated in the eutectic MgCl 2 –KCl molten salt at different temperatures and compared their performance with expensive Haynes 230 (H230) alloy. The corrosion rates of all the studied alloys increased with temperature. The corrosion rates obtained from the electrochemical study showed Ni-coating increases the corrosion resistance of 800H alloy. Further, the linear polarization measurements were also performed at different temperatures to investigate the effect of Ni-coating on the exchange-current density. A long-term corrosion study showed that 800H has a higher corrosion rate than H230. However, Ni-coating significantly decreased the corrosion rate of 800H (even lower than H230) in the molten MgCl 2 –KCl salt. A diffusion model for Ni-coated 800H was presented to describe the diffusion behavior of Cr, Fe, and Ni elements in the Ni-coated 800H alloy in a long-term corrosion study. The diffusion model was simulated based on the partial differential equations and known initial boundary conditions. The simulated result is compared with experimental data by altering the diffusion coefficient and reasonable values of diffusion coefficients of Cr, Fe, and Ni in 800H alloy and Ni-coating. The estimated diffusion coefficient (D) values in the Ni-coating from 800H alloy are in the range of 2–4 × 10 −11 cm 2 s ˗1, 4–6 × 10 −11 cm 2 s ˗1, and 5–8 × 10 −11 cm 2 s ˗1 for Cr, Fe, and Ni, respectively. The overall results indicated that Ni-coated 800H could be employed as a suitable alternative construction material for solar thermal energy storage containers.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Phase Change Materials Research · Adsorption and Cooling Systems · Chemical Looping and Thermochemical Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Biomass-coal co-combustion: opportunity for affordable renewable energy10.1016/j.fuel.2004.09.023 ↗
2. Sabharwall · 2010
3. Parabolic-trough solar collectors and their applications10.1016/j.rser.2010.03.012 ↗
4. Hot corrosion studies using electrochemical techniques of alloys in a chloride molten salt (NaCl-LiCl) at 650 oC
5. Molten nitrate salt development for thermal energy storage in parabolic trough solar power systems
6. Corrosion of alloys in a chloride molten salt (NaCl-LiCl) for solar thermal technologies10.1016/j.solmat.2016.05.052 ↗
7. Thermodynamic modeling of eutectic point in the LiNO3-NaNO3-KNO3 ternary system10.1007/s11669-012-0005-4 ↗
8. Thermodynamic properties of potassium nitrate–magnesium nitrate compound [2KNO3· Mg (NO3)2]10.1016/j.tca.2011.12.010 ↗
9. High thermal energy storage density LiNO3–NaNO3–KNO3–KNO2 quaternary molten salt for parabolic trough solar power generation
10. Thermal stability of the eutectic composition in LiNO3–NaNO3–KNO3 ternary system used for thermal energy storage10.1016/j.solmat.2012.01.009 ↗
11. Thermal conductivity of the ternary eutectic LiNO3–NaNO3–KNO3 salt mixture in the solid state using a simple inverse method10.1016/j.solmat.2012.02.030 ↗
12. Pacheco · 2002 · 45
13. Solar tower power plant in Germany and future perspectives of the development of the technology in Greece and Cyprus10.1016/j.renene.2009.11.003 ↗
14. Reilly · 2001
15. Passerini · 2010
16. Sridharan · 2012
17. Williams · 2006
18. Thermodynamic and kinetic consideration on the corrosion of Fe, Ni and Cr beneath a molten KCl–ZnCl2 mixture10.1016/j.corsci.2005.02.015 ↗
19. Susskind · 1960
20. Anderson · 2012
21. Hot corrosion in gas turbine components10.1016/S1350-6307(00)00035-2 ↗
22. Corrosion behavior of Incoloy 800H/HT in the fluoride molten salt FLiNaK+ MFx (MFx= CrF3, FeF2, FeF3 and NiF2)10.1039/C5NJ01839K ↗
23. Creep crack growth behavior of several structural alloys10.1007/BF02664831 ↗
24. Nickel-plating for active metal dissolution resistance in molten fluoride salts10.1016/j.jnucmat.2011.01.032 ↗
25. The preparation of corrosion-resistant layers by the electrolytic deposition of tantalum on nickel and stainless steel10.1016/0010-938X(81)90061-5 ↗
26. Corrosion resistance of alumina forming alloys against molten chlorides for energy production. II: electrochemical impedance spectroscopy under thermal cycling conditions10.1016/j.solmat.2017.03.025 ↗
27. Molten salt corrosion of stainless steels and low-Cr steel in CSP plants10.1007/s11085-012-9310-x ↗
28. Electrochemical monitoring of high-temperature molten-salt corrosion10.1007/BF00665670 ↗
29. Corrosion of nickel-based alloys in ultra-high temperature heat transfer fluid10.1515/htmp-2016-0017 ↗
30. Investigating corrosion behavior of Ni and Ni-20Cr in molten ZnCl210.1016/j.corsci.2020.109105 ↗
31. Ahmad · 2006
32. The electrochemistry of chromium in molten LiCl+ KCl10.1016/S0022-0728(75)80229-4 ↗
33. Impact of corrosion test container material in molten fluorides10.1115/1.4031682 ↗
34. Olson · 2016
35. Hot corrosion behavior of commercial alloys in thermal energy storage material of molten MgCl2/KCl/NaCl under inert atmosphere10.1016/j.solmat.2018.04.025 ↗
36. Ambrosek · 2011
37. Farlow · 1993
38. Materials corrosion in molten LiF–NaF–KF salt10.1016/j.jfluchem.2008.05.008 ↗
39. Effect of Mn additions on diffusion behavior of Fe in molten magnesium alloys by solid-liquid diffusion couples10.1016/j.jallcom.2017.03.245 ↗