journal article·2018-08

Reducing potential induced degradation of silicon solar cells by using a liquid oxidation technique

Y. Yang, Y.F. Zhao, C.S. Tang, S. Zou, Y.Q. Yu, X.P. Ma, Y. Zhou, X.D. Su, Y. Xin

Publisher page

Abstract

Abstract An ultrathin layer of SiOx formed on the surface of a silicon solar cell can significantly reduce the potential induced degradation effect in solar cell modules. In this work, a liquid oxidation (LO) technique was developed to oxidize silicon surfaces by using a Ti/IrO2–CoO2 anode that can produce a large amount of hydroxyl radicals (•OH) and other species. Our results indicate that the LO SiOx (2.5 nm) layer is very dense, thus the modules made from LO treated cells are better able to mitigate potential induced degradation than modules made from ozone oxidized cells.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and devices · TiO2 Photocatalysis and Solar Cells

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Microstructural analysis of crystal defects leading to potential-induced degradation (PID) of Si solar cells ☆10.1016/j.egypro.2013.05.042 ↗
2. S. Pingel, O. Frank, M. Winkler, S. Daryan, Potential induced degradation of solar cells and panels, in: Proceedings of the Photovoltaic Specialists Conference, 2010, pp. 002817–002822.10.1109/PVSC.2010.5616823 ↗
3. Explanation of potential-induced degradation of the shunting type by Na decoration of stacking faults in Si solar cells10.1016/j.solmat.2013.06.015 ↗
4. Potential-induced degradation in solar cells: electronic structure and diffusion mechanism of sodium in stacking faults of silicon10.1063/1.4894007 ↗
5. Sodium decoration of PID-s crystal defects after corona induced degradation of bare silicon solar cells ☆10.1016/j.egypro.2015.07.055 ↗
6. Injection‐level‐dependent recombination velocities at the Si‐SiO2 interface for various dopant concentrations10.1063/1.356399 ↗
7. Green · 1987 · 681
8. Overcoming over-plating problems for PECVD SiN x passivated laser doped p-type multi-crystalline silicon solar cells10.1016/j.solmat.2011.12.003 ↗
9. Silicon oxidation by ozone10.1088/0953-8984/21/18/183001 ↗
10. Effective surface passivation of p-type crystalline silicon with silicon oxides formed by light-induced anodisation10.1016/j.apsusc.2014.08.028 ↗
11. Low temperature oxidation of SiGe in ozone: ultrathin oxides10.1063/1.372134 ↗
12. Ultrathin silicon oxide film on Si(100) fabricated by highly concentrated ozone at atmospheric pressure10.1116/1.581808 ↗
13. Enhanced oxidation of silicon using a collimated hyperthermal ozone beam10.1063/1.1380242 ↗
14. Surface oxidation of multicrystalline silicon using atmospheric pressure plasma jet driven by radio frequency of 2.0 MHz10.1016/j.surfcoat.2016.07.070 ↗
15. Application of electrochemical degradation of wastewater composed of mixtures of phenol–formaldehyde10.1007/s11270-012-1245-y ↗
16. Advanced treatment of biologically pretreated coking wastewater by electrochemical oxidation using Ti/RuO2 –IrO2 electrodes10.1002/jctb.4006 ↗
17. A. Kapałka, G. Fóti, M. Panizza, L. Guo, X. Li, G. Chen, M.A. Rodrigo, P. Cañizares, J. Lobato, U. Griesbach, Electrochemistry for the Environment, Electrochemistry for the Environment, vol. 23, 2010, p. 263.
18. Electrodeposition of TiO2–RuO2–IrO2 coating on titanium substrate10.1016/j.spmi.2012.03.024 ↗
19. Pleskov · 2002 · 38 · 454
20. Selectivity between oxygen and chlorine evolution in the chlor-alkali and chlorate processes10.1021/acs.chemrev.5b00389 ↗
21. A review and comparison of different methods to determine the series resistance of solar cells10.1016/j.solmat.2007.05.026 ↗