C-276 nickel alloy corrosion in eutectic Na2CO3/NaCl molten salt under isothermal and thermal cycling conditions
Source abstract
Abstract
Thermal energy storage (TES) is a key component for the practical application of concentrating solar thermal power. Recently, a push for higher temperatures has increased interest in molten salts with melting points above 550 °C as phase change thermal energy storage media. Corrosion of a nickel superalloy (C-276) with a eutectic salt mixture (59.5 %wt Na 2 CO 3 /40.5 %wt NaCl) at 650 °C was analysed under both isothermal conditions and with thermal cycle between 600 and 650 °C. Corrosion rates of 400–500 μm/year under isothermal conditions and 200–300 μm/year under thermal cycling were determined by measuring thickness loss, and oxide growth was primarily responsible for the metal loss. Thermal cycling reduced corrosion thickness, however it remained intact with no cracking or buckling. Post-test analysis of the salt found that molybdenum, manganese and tungsten were most likely to be removed from the alloy. Isothermal conditions did not cause chromium to be removed from the alloy by the salt. However, chromium was present in the salt after thermal cycling, due to its removal from the oxide layer. Whilst the corrosion was above the maximum acceptable corrosion rate for a TES system, this study shows that oxide layers formed on alloy C-276 have protective capabilities in this salt, gaining maximum thickness after about 400 h and preventing the salt from attacking the metal directly. Longer testing with more samples is require to determine if the corrosion of this alloy is halted due to the oxide layer growth on the metal surface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Phase Change Materials Research · Adsorption and Cooling Systems · Solar Thermal and Photovoltaic Systems
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Experimental verification of theoretically estimated composition and enthalpy of fusion of eutectic salt mixtures10.1016/j.solmat.2017.09.033 ↗
2. Optimized salt selection for solar thermal latent heat energy storage10.1002/adsu.201800074 ↗
3. Eutectic Na2CO3–NaCl salt: a new phase change material for high temperature thermal storage10.1016/j.solmat.2016.04.002 ↗
4. An innovative empirical method for the accurate identification of the eutectic point of binary salts for solar thermal energy storage10.1016/j.mtcomm.2020.101864 ↗
5. Techno-economic analysis on the design of sensible and latent heat thermal energy storage systems for concentrated solar power plants10.1016/j.renene.2021.06.069 ↗
6. Review on concentrating solar power plants and new developments in high temperature thermal energy storage technologies10.1016/j.rser.2015.09.026 ↗
7. Corrosion mechanisms in chloride and carbonate salts
8. Corrosion of metallic stack components in molten carbonates: critical issues and recent findings10.1016/j.jpowsour.2007.11.100 ↗
9. Corrosion of stainless steel 316 in eutectic molten salts for thermal energy storage10.1016/j.solener.2018.03.053 ↗
10. Corrosion of steel alloys in eutectic NaCl+Na2CO3 at 700°C and Li2CO3 + K2CO3 + Na2CO3 at 450°C for thermal energy storage10.1016/j.solmat.2017.05.063 ↗
11. A eutectic salt high temperature phase change material: thermal stability and corrosion of SS316 with respect to thermal cycling10.1016/j.solmat.2017.05.047 ↗
12. Corrosion mechanism of SS316L exposed to NaCl/Na2CO3 molten salt in air and argon environments10.1016/j.corsci.2021.109966 ↗
13. Materials corrosion for thermal energy storage systems in concentrated solar power plants10.1016/j.rser.2018.01.010 ↗
14. Special Metals, Product handbook of high-performance nickel alloys, in: PCC-8064, Precision Castparts Corp, www.specialmetals.com.
15. High-temperature characteristics of stainless steels
16. Corrosion of Inconel 601 in molten salts for thermal energy storage10.1016/j.solmat.2017.07.036 ↗
17. Damage analysis of 601 nickel superalloy in eutectic Na2CO3/NaCl molten salt under isothermal and thermal cycling conditions10.1016/j.solener.2019.09.030 ↗
18. Hot corrosion behavior of commercial alloys in thermal energy storage material of molten MgCl2/KCl/NaCl under inert atmosphere10.1016/j.solmat.2018.04.025 ↗
19. Corrosion resistance of Hastelloys in molten metal-chloride heat-transfer fluids for concentrating solar power applications10.1016/j.solener.2014.02.002 ↗
20. High performance corrosion resistance of nickel-based alloys in molten salt Flibe10.13182/FST09-A8900 ↗
21. Aggressive corrosion of C-276 nickel superalloy in chloride/sulphate eutectic salt10.1016/j.solener.2021.09.023 ↗
22. An improved technique for molten salt corrosion sample preparation10.1016/j.solmat.2021.111057 ↗
23. Materials corrosion in molten LiF–NaF–KF salt10.1016/j.jfluchem.2008.05.008 ↗
24. Molten nitrate salts at 600 and 680 °C: thermophysical property changes and corrosion of high-temperature nickel alloys10.1016/j.solener.2014.01.028 ↗
25. Corrosion of stainless steels and carbon steel by molten mixtures of commercial nitrate salts10.1361/10599490417542 ↗
26. Electron microscopic analysis of heterogeneous precipitates in hastelloy C-27610.1007/BF02643394 ↗
27. Evans · 1961
28. 1998
29. Gibbs energy of formation of Na2WO4 and Na3WO4 in liquid sodium10.1016/S0022-3115(96)00715-5 ↗
30. Standard molar gibbs free energies of formation of Na2Mo2O7(s), Na2Mo3O10(l), and Na2Mo3O6(s) by solid-oxide-electrolyte galvanic cells10.1016/S0021-9614(05)80296-4 ↗