Industrially applicable mitigation of BO-LID in Cz-Si PERC-type solar cells within a coupled fast firing and halogen lamp based belt-line regenerator – A parameter study

Christian Derricks, Axel Herguth, Giso Hahn, Olaf Romer, Thomas Pernau

Publisher page

Abstract

Abstract The benefit of sophisticated rear surface passivation quality in highly efficient solar cell structures made of boron-doped oxygen-rich Cz-Si wafers (e.g. PERC) can be reduced if bulk lifetime becomes a limiting factor due to boron-oxygen related light-induced degradation (BO-LID). A permanent lifetime recovery can be achieved through a regeneration treatment under illumination at elevated temperature. To evaluate the applicability of BO mitigation by means of regeneration at industrial relevant conditions, industrially-made PERC solar cell precursors were processed in a coupled fast firing and regeneration tool where the latter comprises an illuminated zone through which the solar cells transit on a belt. The treatment was evaluated by a subsequent intentional degradation. The results show that untreated solar cells suffer from BO-LID while properly treated samples are almost free of BO-LID demonstrating the applicability of a fast (around 15–30 s) and coupled regeneration process in mass production. Furthermore, it is found that fluctuations in precursor quality and/or variations in firing conditions are of minor significance for the BO-LID mitigation process. The firing conditions process window (peak firing temperature and belt velocity) overlaps with the treatment conditions window having the benefit of independent optimization.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Investigation of photon and thermal induced changes in silicon solar cells
2. Degradation of crystalline silicon due to boron-oxygen defects10.1109/JPHOTOV.2016.2614119 ↗
3. Eliminating light-induced degradation in commercial p-Type Czochralski silicon solar cells10.3390/app8010010 ↗
4. A generalized model for boron-oxygen related light induced degradation in crystalline silicon
5. 22.8% efficient silicon solar cell10.1063/1.101596 ↗
6. The passivated emitter and rear cell (PERC): from conception to mass production10.1016/j.solmat.2015.06.055 ↗
7. Solar cells with efficiencies above 21% processed from Czochralski grown silicon
8. Investigation of carrier lifetime instabilities in CZ-grown silicon
9. Degradation of carrier lifetime in Cz silicon solar cells10.1016/S0927-0248(00)00098-2 ↗
10. Electrical and thermal properties of the metastable defect in boron-doped Czochralski silicon (Cz-Si)
11. Electronically activated boron-oxygen-related recombination centers in crystalline silicon10.1063/1.2140584 ↗
12. Avoiding boron-oxygen related degradation in highly boron-doped Cz silicon
13. Deactivation of the boron–oxygen recombination center in silicon by illumination at elevated temperature10.1002/pssr.200802009 ↗
14. Impact of dopant compensation on the deactivation of boron-oxygen recombination centers in crystalline silicon10.1063/1.3272918 ↗
15. Kinetics of the boron-oxygen related defect in theory and experiment10.1063/1.3517155 ↗
16. Impact of oxygen on the permanent deactivation of boron–oxygen-related recombination centers in crystalline silicon10.1063/1.3431359 ↗
17. Influence of hydrogen effusion from hydrogenated silicon nitride layers on the regeneration of boron-oxygen related defects in crystalline silicon10.1063/1.4833243 ↗
18. Influence of hydrogen on the regeneration of boron-oxygen related defects in crystalline silicon10.1063/1.4804310 ↗
19. Lifetimes exceeding 1 ms in 1 Ωcm boron-doped Cz-silicon10.1016/j.solmat.2014.06.011 ↗
20. Accelerated formation of the boron-oxygen complex in p-type Czochralski silicon10.1002/pssr.201510064 ↗
21. Influence of the formation- and passivation rate of boron-oxygen defects for mitigating carrier-induced degradation in silicon within a hydrogen-based model10.1063/1.4941387 ↗
22. Review of light-induced degradation in crystalline silicon solar cells10.1016/j.solmat.2015.11.047 ↗
23. Permanent deactivation of boron-oxygen recombination centres in silicon10.1002/pssb.201600082 ↗
24. The nature of boron-oxygen lifetime-degrading centres in silicon10.1002/pssc.201600016 ↗
25. Multiple pathways for permanent deactivation of boron-oxygen defects in p-type silicon10.1016/j.solmat.2017.06.041 ↗
26. Kinetics of the permanent deactivation of the boron-oxygen complex in crystalline silicon as a function of illumination intensity10.1063/1.4978266 ↗
27. Recent insights into boron-oxygen related degradation: evidence of a single defect10.1016/j.solmat.2017.06.038 ↗
28. Investigations on the long time behavior of the metastable boron-oxygen complex in crystalline silicon10.1002/pip.779 ↗
29. Hydrogen passivation of B-O defects in Czochralski silicon10.1016/j.egypro.2013.07.317 ↗
30. Advanced bulk defect passivation for silicon solar cells10.1109/JPHOTOV.2013.2281732 ↗
31. Hydrogenated silicon nitride for regeneration of light induced degradation
32. Molecular hydrogen formation in hydrogenated silicon nitride10.1063/1.2396900 ↗
33. Regeneration of boron-oxygen related degradation in Cz-Si PERC-type solar cells at high temperatures
34. Production-compatible regeneration of boron-doped Czochralski-silicon in a combined fast-firing and regeneration belt-line furnace
35. Rather high speed regeneration of BO-defects: regeneration experiments with large cell batches
36. Keep a LID on it
37. Ultrafast in-line capable regeneration process for preventing light induced degradation of boron-doped p-type Cz-silicon PERC solar cells
38. Rapid mitigation of carrier-induced degradation in commercial silicon solar cells10.7567/JJAP.56.08MB13 ↗
39. The development of in-line regeneration tool for the effective suppression of light-induced-degradation on p-type silicon solar cells
40. LEDs for the implementation of advanced hydrogenation using hydrogen charge-state control10.1155/2018/2439425 ↗
41. Elimination of BO-LID in mass production using illuminated annealing in a coupled firing and regeneration tool
42. On the meaning(fullness) of the intensity unit ‘suns’ in light induced degradation experiments10.1016/j.egypro.2017.09.339 ↗
43. How to properly assess boron-oxygen related degradation in crystalline silicon
44. A fast, preparation‐free method - to detect iron in silicon10.1063/1.345063 ↗
45. Iron and its complexes in silicon10.1007/s003390050968 ↗
46. Dynamics of light-induced FeB pair dissociation in crystalline silicon10.1063/1.1823587 ↗
47. Iron detection in crystalline silicon by carrier lifetime measurements for arbitrary injection and doping10.1063/1.1637136 ↗
48. Imaging of metastable defects in silicon10.1109/JPHOTOV.2011.2169942 ↗
49. Investigating the influence of interstitial iron on the study of boron-oxygen defects
50. Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon10.1016/j.solmat.2017.08.003 ↗
51. Mass production of p-type Cz silicon solar cells approaching average stable conversion efficiencies of 22%10.1016/j.egypro.2017.09.308 ↗
52. Temperature and light-induced changes in bulk and passivation quality of boron-doped float-zone silicon coated with SiNx:H10.1109/JPHOTOV.2017.2649601 ↗
53. Stability of effective lifetime of float-zone silicon wafers with AlOx surface passivation schemes under illumination at elevated temperature10.1016/j.egypro.2017.09.320 ↗