Abstract The precipitation of P in the emitter region of H 3 PO 4 spray doped silicon for solar cell applications has been investigated by electron microscopy, X-ray microanalysis and electrical measurements after annealing for two different times. P, Si and O concentration profiles show that the composition of the phosphorous silicate glass (PSG) is in agreement with a solid solution of P 2 O 5 in SiO 2 and that P concentration is peaked at the PSG/Si interface. TEM observations have shown for the shorter annealing the formation of a 20 nm thick defect layer at the silicon surface; this layer evolves into a network of large rod-like monoclinic (or orthorhombic) SiP precipitates, which extend in depth up to about 100 nm for the longer treatment. The SiP crystal structure and the habit planes are the same as previously reported in literature. No deeper defect that could interact with the junction located at about 300 nm has been detected. Although the SiP precipitation takes place entirely at the Si surface, it is not significantly affected by the orientation of the crystals and by the texturing process. The amounts of both electrically active and inactive P obtained by the H 3 PO 4 spray technique have been compared with the ones obtained by the conventional POCl 3 technique. The former process presents a larger amount of inactive dopant, a finding that is in keeping with the microstructural and microanalytical observations. Instead the amount of active P is similar in the two cases, a result attributed to the precipitation and clustering phenomena of the excess dopant.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Phosphorus diffusion in silicon using POCl3
2. Kinetics of phosphorus predeposition in silicon using POCl310.1149/1.2134437 ↗
3. Predeposition in silicon as affected by the formation of orthorhombic SiP and cubic SiO2·P2O5 at the PSG–Si interface10.1149/1.2132905 ↗
4. Development of a phosphorus spray diffusion system for low cost silicon solar cells10.1149/1.2202088 ↗
5. C. Voyer, D. Biro, K. Wagner, J. Benik and R. Preu, Fabrication of textured solar cells using sprayed phosphoric acid as the dopant source for the in-line emitter diffusion, in:Proceedings of the 21th European PV Solar Energy Conference, Dresden, 4 September 2006, pp. 1157–1160.
6. N+ silicon solar cells emitters realized using phosphoric acid as doping source in a spray process10.1016/j.tsf.2006.01.005 ↗
7. Rapid thermal annealing of spin-coated phosphoric acid films for shallow junction formation10.1063/1.119547 ↗
8. J. Horzel, B. Schum, A. Lachowicz, J. Rossa, K. Vass, M. Jahn, Y. Gassembauer, H. von Campe, H. Boubekeur, U. Weber, A. Seidl, A. Armigliato, F. Seidel, T. Hantsvhel, P. Eyben, S. Vinzelberg, S.S.A. Gerst, W. Schmidt, On anomalous emitter regions forming during phosphorus diffusion processing of crystalline silicon solar cells, in: Proceedings of the 25th European and 5th World PV Conference, Valencia, 6–10 September 2010, pp. 1882–1891.
9. The quantitative analysis of thin specimens10.1111/j.1365-2818.1975.tb03895.x ↗
10. The system SiO2–P2O510.1111/j.1151-2916.1962.tb11186.x ↗
11. Dopant and carrier concentration in silicon, in equilibrium with monoclinic SiP precipitates10.1103/PhysRevB.53.7836 ↗
12. Supersaturation of self-interstitials and undersaturation of vacancies during phosphorus diffusion in silicon10.1063/1.94915 ↗
13. Dependence of anomalous P diffusion in Si on depth position of defects created by ion implantation10.1007/BF00619395 ↗
14. Supersaturation of self-interstitials and undersaturation of vacancies during phosphorus diffusion in silicon10.1063/1.94915 ↗
15. Electron microscopy of silicon monophosphide precipitates in P-diffused silicon10.1007/BF00540355 ↗
16. HREM of SiP precipitates at the (111) silicon surface during phosphorus predepostion10.1016/0304-3991(84)90113-X ↗
17. SiP precipitation within the doped silicon lattice, concomitant with phosphorus predeposition10.1063/1.322549 ↗
18. Precipitation as the phenomenon responsible for the electrically inactive phosphorus in silicon10.1063/1.330646 ↗
19. High concentration diffusivity and clustering of arsenic and phosphorus in silicon10.1063/1.367008 ↗
20. High resolution electron microscopy observations of precipitates in P supersaturated silicon10.1016/0304-3991(84)90075-5 ↗
21. J. Horzel, M. Jahn1, P. Schmitt1, W. Hefner1, K. Vaas1, M. Fiedler1, E. Parr1, J. Moschner1, P. Roth1, A. Lachowicz1,Y. Gassenbauer1, E. Schmich1, M. Bothar1, T. Neese1, I. Ernst1, T. Droste1, L. Lippert1, B. Schum1, W. Schmid, Homogeneous versus selective emitter-perspectives for future industrial processing of crystalline silicon solar cells,in: Proceedings of the 25th European and 5th World PV Conference, Valencia, 6–10 September 2010, pp. 1492–1498.