Higher stability of p-type Ga-doped Czochralski silicon for light and elevated-temperature induced degradation: Insights into Ga-related precursors
Source abstract
Abstract
Light and elevated temperature-induced degradation (LeTID) is still a challenge for crystalline silicon solar cells. In this study, p-type Ga-doped Czochralski silicon (Cz-Si) passivated emitter rear contact (PERC) solar cells have been demonstrated to obtain higher stability for LeTID as compared to B-doped counterparts. Meanwhile, the degradation behavior in p-type Ga-doped Cz-Si with PERC structure is investigated. It is found that p-type Ga-doped Cz-Si behave quite differently than B-doped counterparts: during dark annealing at 170–260 °C, Ga-doped Cz-Si wafers have shown an extremely slower degradation in minority carrier lifetime, i. e., with a temperature-dependent precursor time where the lifetime stays almost stable at the beginning of degradation. In addition, an equivalent activation energy of E A = 1.05 ± 0.05 eV was obtained from the temperature-dependent precursor time. At last, by density functional theory (DFT) calculations, the molecular structures of the possible LeTID defect precursors, Ga-H and B-H complexes, are optimized, and the formation energies of Ga-H and B-H complexes are derived to be - 1.09 and - 0.96 eV, respectively. Further calculation also confirms a higher equilibrium temperature of reaction of acceptor-hydrogen formation and dissociation for Ga-doped Cz-Si wafers. Therefore, the lower formation energy of Ga-H complex can be one of the root causes for better LeTID stability in Ga-doped Cz-Si, while the participation of dopant in precursor transition of LeTID defect can be confirmed.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Silicon Nanostructures and Photoluminescence · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Development of the PERC solar cell10.1109/JPHOTOV.2019.2899460 ↗
2. Generation kinetics of boron-oxygen complexes in p-type compensated c-Si10.1063/1.4868635 ↗
3. An industrial solution to light-induced degradation of crystalline silicon solar cells10.1007/s11708-016-0430-x ↗
4. Investigations on the long time Behavior of the metastable Boron-Oxygen complex in crystalline silicon10.1002/pip.779 ↗
5. Lifetime instabilities in gallium doped monocrystalline PERC silicon solar cells10.1016/j.solmat.2019.110299 ↗
6. Gallium-doped silicon for high-efficiency commercial passivated emitter and rear solar cells10.1002/solr.202000754 ↗
7. Influence of dopant elements on degradation phenomena in B- and Ga-doped czochralski-grown silicon10.1002/solr.202100147 ↗
8. Investigation on the light and elevated temperature induced degradation of gallium-doped Cz-Si10.1016/j.solener.2021.07.023 ↗
9. Ieee, A new mc-Si degradation effect called LeTID
10. On the defect physics behind light and elevated temperature-induced degradation (LeTID) of multicrystalline silicon solar cells10.1109/JPHOTOV.2019.2937223 ↗
11. Evaluating root cause: the distinct roles of hydrogen and firing in activating light- and elevated temperature-induced degradation10.1063/1.5041756 ↗
12. The effect and mechanism of current injection to suppress light and elevated temperature induced degradation in p-type cast-mono and multicrystalline silicon Passivated Emitter and Rear cells10.1016/j.solener.2022.02.032 ↗
13. Progress in the understanding of light- and elevated temperature-induced degradation in silicon solar cells: a review10.1002/pip.3362 ↗
14. Improved surface passivation of rear SiNx/AlOx stacks in p-type boron-doped Czochralski silicon wafers during dark annealing at elevated temperatures
15. New insights on LeTID/BO-LID in p-type mono-crystalline silicon10.1016/j.solmat.2021.111085 ↗
16. Light-induced lifetime degradation in high-performance multicrystalline silicon: detailed kinetics of the defect activation10.1016/j.solmat.2017.08.007 ↗
17. Generalized gradient approximation for the exchange-correlation hole of a many-electron system10.1103/PhysRevB.54.16533 ↗
18. A four-state kinetic model for the carrier-induced degradation in multicrystalline silicon: introducing the reservoir state10.1016/j.solmat.2018.04.024 ↗
19. Performance degradation of commercial Ga-doped passivated emitter and rear cell solar modules in the field10.1002/pip.3512 ↗
20. On the impact of dark annealing and room temperature illumination on p-type multicrystalline silicon wafers10.1016/j.solmat.2018.09.018 ↗
21. Kinetics study on carrier injection-induced degradation and regeneration at elevated temperature in p-type cast-monosilicon passivated emitter rear contact solar cells10.1002/solr.202100035 ↗
22. Impact of hydrogen in Ga-doped silicon on maximum LeTID defect density10.1002/solr.202300501 ↗
23. Lifetime spectroscopy for defect characterization: systematic analysis of the possibilities and restrictions10.1063/1.1428095 ↗
24. Lifetime spectroscopy investigation of light-induced degradation in p-type multicrystalline silicon PERC10.1109/JPHOTOV.2016.2606699 ↗
25. Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon10.1016/j.solmat.2017.08.003 ↗
26. Formation, dissociation, and diffusion of various hydrogen dimers in silicon10.1002/pssb.201600779 ↗
27. Raman spectroscopy of hydrogen molecules in crystalline silicon10.1103/PhysRevLett.81.421 ↗
28. The interaction of hydrogen with deep level defects in silicon10.4028/www.scientific.net/SSP.71.173 ↗
29. Solubility of hydrogen in silicon at 1300 °C10.1063/1.108602 ↗
30. H2 molecules in crystalline silicon10.1016/S0921-5107(98)00264-5 ↗
31. Progress of hydrogenation engineering in crystalline silicon solar cells: a review10.1088/1361-6463/ac9066 ↗
32. On the kinetics of the exchange of hydrogen between hydrogen-boron pairs and hydrogen dimers in crystalline silicon10.1063/5.0086307 ↗
33. Correlation study between LeTID defect density, hydrogen and firing profile in Ga-doped crystalline silicon10.1016/j.solmat.2023.112456 ↗
34. Impact of fast-firing conditions on light-and elevated-temperature-induced degradation (LeTID) in Ga-doped Cz-Si10.1109/JPHOTOV.2023.3304118 ↗
35. Hydrogen localization near boron in silicon10.1063/1.95599 ↗
36. Dissociation-energies of shallow hydrogen pairs in silicon10.1103/PhysRevB.39.13549 ↗
37. Temporary recovery of the defect responsible for light- and elevated temperature-induced degradation: insights into the physical mechanisms behind LeTID10.1109/JPHOTOV.2020.3025240 ↗
38. Why is gallium-doped silicon (sometimes) stable? Kinetics of light and elevated temperature induced degradation10.1016/j.solmat.2024.112986 ↗
39. Kinetics of carrier-induced degradation at elevated temperature in multicrystalline silicon solar cells10.1016/j.solmat.2017.05.066 ↗