Field effect surface passivation of SiO2/Si interfaces by heat treatment with high-pressure H2O vapor
Source abstract
Abstract
We investigated a simple field effect passivation of the silicon surfaces using the high-pressure H 2 O vapor heating. Heat treatment with 2.1 x 10 6 Pa H 2 O vapor at 260°C for 3 h reduced the surface recombination velocity from 405cm/s (before the heat treatment) to 38cm/s for the thermally evaporated SiO x film/Si. Additional deposition of 140 nm-SiO x films (x < 2) with a high density of fixed positive charges on the SiO 2 /Si samples further decreased the surface recombination velocity to 22 cm/s. We also demonstrated the field effect passivation for n-type silicon wafer coated with thermally grown SiO 2 . Additional deposition of 210 nm SiO x films on both the front and rear surfaces increased the effective lifetime from 1.4 to 4.6 ms. Combination of thermal evaporation of SiO x film and the heat treatment with high-pressure H 2 O vapor is effective for low-temperature passivation of the silicon surface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (5)
Show source-provided references
1. Pertron · Appl. Phys. A · 1987 · 43 · 15310.1007/BF00615975 ↗
2. Nagayoshi · J. Appl. Phys. · 1996 · 35 · L104710.1143/JJAP.35.L1047 ↗
3. Sameshima · Jpn. J. Appl. Phys. · 1997 · 36 · L68710.1143/JJAP.36.L687 ↗
4. Sameshima · Thin Solid Films · 1998 · 335 · 13810.1016/S0040-6090(98)00887-6 ↗
5. Sameshima · Jpn. J. Appl. Phys. · 1998 · 37 · L145210.1143/JJAP.37.L1452 ↗