journal article·2024-12Open access

Long-term carrier lifetime instabilities in n-type FZ- and Cz-silicon under illumination at elevated temperature

Melanie Mehler, Nicolas Weinert, Nicole Aßmann, Axel Herguth, Giso Hahn, Fabian Geml

Abstract

Even though n-type Si wafers show a lower extent of light-induced degradation, similar degradation and regeneration behavior as in p-type Si materials has been observed for various n-type Si monocrystalline materials. In this work, the long-term behavior of minority charge carrier lifetime in non-diffused n-type FZ-Si and Cz-Si wafers during illumination at elevated temperatures is investigated. Thereby, various influencing factors such as peak firing temperature and treatment temperature are considered. Degradation and a very strong regeneration effect, which exceeds the initial effective lifetime value, can be observed in the samples. Since surface-related saturation current density remains almost constant during degradation and regeneration, the effect seems to be bulk related. The extent of degradation and regeneration could be shown to be firing temperature-dependent. It could also be shown for n-type FZ-Si wafers that higher firing temperatures result in an increased H 2 content within the silicon bulk . Investigations of the injection-dependent defect density revealed that the defect formed during degradation is not a deep level Shockley-Read-Hall defect. Observations at different treatment temperatures and constant illumination of 0.9(1) sun photon flux equivalent have shown that a higher treatment temperature leads to faster degradation and regeneration kinetics. Similarly, higher injection rates also speed up regeneration kinetics. Since degradation also occurs in darkness, the bulk related degradation effect in n-type FZ-Si is charge carrier-induced and not necessarily light-induced.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Advancements in Semiconductor Devices and Circuit Design

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Lifetime degradation and regeneration in multicrystalline silicon under illumination at elevated temperature10.1063/1.4944839 ↗
2. Impact of the firing temperature profile on light induced degradation of multicrystalline silicon10.1002/pssr.201600272 ↗
3. Firing and gettering dependence of effective defect density in material exhibiting LeTID10.1063/1.5049334 ↗
4. LeTID mitigation via an adapted firing process in p-type PERC cells from SMART cast-monocrystalline, Czochralski and high-performance multicrystalline silicon10.1002/pip.3467 ↗
5. A new light induced volume degradation effect of mc-Si solar cells and modules
6. Influence of silicon nitride and its hydrogen content on carrier-induced degradation in multicrystalline silicon
7. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
8. Impact of temperature and doping on LeTID and regeneration in mc-Si
9. Evaluating root cause: the distinct roles of hydrogen and firing in activating light-and elevated temperature-induced degradation10.1063/1.5041756 ↗
10. On the defect physics behind light and elevated temperature-induced degradation (LeTID) of multicrystalline silicon solar cells10.1109/JPHOTOV.2019.2937223 ↗
11. On the role of AlOx thickness in AlOx/SiNy: H layer stacks regarding light-and elevated temperature-induced degradation and hydrogen diffusion in c-Si10.1109/JPHOTOV.2021.3075850 ↗
12. Lifetime degradation on n-type wafers with boron-diffused and SiO2/SiN-passivated surface10.1016/j.egypro.2014.08.082 ↗
13. Light and elevated temperature induced degradation in p-type and n-type cast-grown multicrystalline and mono-like silicon10.1016/j.solmat.2018.03.002 ↗
14. Hydrogen-induced degradation: explaining the mechanism behind light-and elevated temperature-induced degradation in n-and p-type silicon10.1016/j.solmat.2019.110353 ↗
15. Enhanced stability of passivation quality on diffused silicon surfaces under light-induced degradation conditions10.1016/j.solmat.2018.08.019 ↗
16. Degradation and recovery of n-type multi-crystalline silicon under illuminated and dark annealing conditions at moderate temperatures10.1109/JPHOTOV.2018.2885711 ↗
17. Hydrogen induced degradation: a possible mechanism for light-and elevated temperature-induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
18. Investigation of LeTID where we can control it–Application of FZ silicon for defect studies10.1063/1.5123893 ↗
19. 24.58% efficient commercial n-type silicon solar cells with hydrogenation10.1002/pip.3464 ↗
20. The impact of different hydrogen configurations on light-and elevated-temperature-induced degradation10.1109/JPHOTOV.2023.3236185 ↗
21. On the meaning (fullness) of the intensity unit ‘suns’ in light induced degradation experiments10.1016/j.egypro.2017.09.339 ↗
22. On the lifetime-equivalent defect density: properties, application, and pitfalls10.1109/JPHOTOV.2019.2922470 ↗
23. On the impact of bulk lifetime on the quantification of re-combination at the surface of semiconductors10.1109/JPHOTOV.2023.3291453 ↗
24. Light and elevated temperature induced degradation in mono-like and float-zone silicon: correlations to material types, silicon nitride films, and dopant diffusion10.1109/JPHOTOV.2021.3082645 ↗
25. Determination of BO-LID and LeTID related activation energies in Cz-Si and FZ-Si using constant injection conditions10.1063/1.5123890 ↗
26. Light-induced activation and deactivation of bulk defects in boron-doped float-zone silicon10.1063/1.4983024 ↗
27. Hydrogen-related defects measured by infrared spectroscopy in multicrystalline silicon wafers throughout an illuminated annealing process10.1063/1.5142476 ↗
28. Hydrogen molecules in boron-doped crystalline silicon, Semicond
29. Interactions of hydrogen molecules with bond-centered interstitial oxygen and another defect center in silicon10.1103/PhysRevB.56.13118 ↗
30. Correlation study between LeTID defect density, hydrogen and firing profile in Ga-doped crystalline silicon10.1016/j.solmat.2023.112456 ↗
31. Statistics of the recombinations of holes and electrons10.1103/PhysRev.87.835 ↗
32. Electron-hole recombination in germanium10.1103/PhysRev.87.387 ↗
33. Rein · 2005
34. Lifetime spectroscopy for defect characterization: systematic analysis of the possibilities and restrictions10.1063/1.1428095 ↗
35. Defect and impurity diagnostics and process monitoring10.1016/S0927-0248(01)00187-8 ↗
36. Understanding lifetime degradation in Czochralski-grown n-type silicon after high-temperature processing"
37. Understanding the origin of Tabula Rasa-induced defects in n-type Cz c-Si: the case of nitrogen atmosphere10.1016/j.solmat.2022.112159 ↗
38. Lifetime spectroscopy investigation of light-induced degradation in p-type multicrystalline silicon PERC10.1109/JPHOTOV.2016.2606699 ↗
39. Recombination parameters of lifetime-limiting carrier-induced defects in multicrystalline silicon for solar cells10.1063/1.4977906 ↗
40. Why is gallium-doped silicon (sometimes) stable? Kinetics of light and elevated temperature induced degradation10.1016/j.solmat.2024.112986 ↗