journal article·2014-09

Effect of plasma treated Ag/indium tin oxide anode modification on stability of polymer solar cells

Bobins Augustine, Rafal Sliz, Kimmo Lahtonen, Mika Valden, Risto Myllylä, Tapio Fabritius

Publisher page

Abstract

Abstract The most commonly used hole transporting layer (HTL) in conventional polymer solar cells is poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate) PEDOT:PSS. The acidic nature of this HTL is responsible for etching of the indium tin oxide (ITO) layer which is the anode in polymer solar cells and leads to degradation of efficiency in polymer solar cells in the long run. In this article we explored the effect of plasma treated Ag as an intermediate layer between ITO and PEDOT:PSS for over one month period. It was found that the devices with plasma treated Ag as an intermediate layer with thickness of 5 nm resulted in only 30% degradation over one month and did not decrease the initial power conversion efficiency (PCE) compared to the cell without the anode modification, whereas the devices without the intermediate layer, degraded up to 66% of the initial PCE. The mechanism was analyzed using XPS measurements and found out that indium from ITO etches out and diffuses to the subsequent polymer layer. Further, the experiment revealed that the presence of plasma treated Ag layer restricted the rapid indium diffusion, which accounted to enhanced device stability.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Organic Electronics and Photovoltaics · Conducting polymers and applications · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Elschner · 2011 · 123
2. Effects of layer thickness and annealing of PEDOT: PSS layers in organic photodetectors10.1021/ma901182u ↗
3. Stability of the interface between indium-tin-oxide and poly(3,4-ethylenedioxythiophene)/poly(styrenesulfonate) in polymer light-emitting diodes10.1063/1.1315344 ↗
4. Lide · 2002
5. Stability/degradation of polymer solar cells10.1016/j.solmat.2008.01.005 ↗
6. Stability and photodegradation mechanisms of conjugated polymer/fullerene plastic solar cells10.1016/S0927-0248(99)00094-X ↗
7. The thermal ageing of poly(3,4-ethylenedioxythiophene). An investigation by X-ray absorption and X-ray photoelectron spectroscopy10.1016/0301-0104(95)00026-K ↗
8. Electrochemical and spectroscopic characterization of polyalkylenedioxythiophenes10.1016/0022-0728(94)87085-3 ↗
9. Influence of the blend concentration of P3HT: PCBM in the performances of BHJ solar cells
10. Thermally stable, efficient polymer solar cells with nanoscale control of the interpenetrating network morphology10.1002/adfm.200500211 ↗
11. Effect of LiF/metal electrodes on the performance of plastic solar cells10.1063/1.1446988 ↗
12. 4.8% Efficient poly(3-hexylthiophene)-fullerene derivative (1:0.8) bulk heterojunction photovoltaic devices with plasma treated Ag Ox/indium tin oxide anode modification10.1063/1.2830619 ↗
13. Evaluating carrier accumulation in degraded bulk heterojunction organic solar cells by a thermally stimulated current technique10.1002/adfm.200901573 ↗
14. Instrumentation and analytical methods of an x-ray photoelectron spectroscopy–scanning tunneling microscopy surface analysis system for studying nanostructured materials10.1063/1.2221539 ↗
15. Long-term operational lifetime and degradation analysis of P3HT: PCBM photovoltaic cells10.1016/j.solmat.2010.09.007 ↗