Connecting material degradation and power loss of PV modules using advanced statistical methodology
Source abstract
Abstract
The presented work focuses on the influence of different stress combinations (in climate-specific ageing tests) on polymer material degradation and electrical power loss of PV modules and how these data can be linked using advanced statistical methods. The statistical analysis is divided into three parts: in the first part, the direct effects of the climatic stresses on the electrical performance are assessed. The second part aims to correlate the electrical degradation behaviour with changes in the encapsulation material, and the third part does the same for the backsheet material of the modules. Time series of electrical data are extracted from IV curves and correlated with changes in material parameters obtained from fluorescence spectroscopy of the encapsulant as well as infrared spectroscopy and colour measurements of the backsheet. The data set analyzed consists of measurements that were taken throughout accelerated ageing experiments simulating stressors typically found for arid, tropical, moderate, and alpine climate zones. Significant correlations were found between the material changes - as indicated by the spectral measurements - and the electrical power loss of the test modules in the course of climate-specific ageing. The results of the analysis provide valuable input for possible measures of preventive maintenance based on condition monitoring of single modules. The methodology developed in this paper allows for an estimation of the power output for modules with identical design and bill of materials using simple, non-destructive measurement methods. The results from accelerated lab tests and the correlations determined from them can be used to predict the electrical power output of installed PV modules. As a result, deviations in module performance can be detected at an early stage and preventive maintenance measures in PV systems can be carried out.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Photovoltaic System Optimization Techniques · Advanced Battery Technologies Research · Photovoltaic Systems and Sustainability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (75)
Show source-provided references
1. Photovoltaics module reliability for the terawatt age10.1088/2516-1083/ac6111 ↗
2. Izumi · 2023 · 2023
3. Circular economy priorities for photovoltaics in the energy transition10.1371/journal.pone.0274351 ↗
4. Motivation, benefits, and challenges for new photovoltaic material & module developments10.1088/2516-1083/ac6f3f ↗
5. Oreski · 2021 · 2021
6. Potential Induced Degradation of solar cells and panels
7. Review of degradation and failure phenomena in photovoltaic modules10.1016/j.rser.2022.112160 ↗
8. Kettle · Prog. Photovoltaics Res. Appl. · 2022 · 30 · 136510.1002/pip.3577 ↗
9. Defects and performance of Si PV modules in the field – an analysis10.1039/D2EE00109H ↗
10. A new mc-Si degradation effect called LeTID
11. Evolution of LeTID defects in p-type multicrystalline silicon during degradation and regeneration10.1109/JPHOTOV.2017.2695496 ↗
12. Drivers for the cracking of multilayer polyamide-based backsheets in field photovoltaic modules: in-depth degradation mapping analysis10.1002/pip.3260 ↗
13. A comparison of key PV backsheet and module performance from fielded module exposures and accelerated tests10.1109/JPHOTOV.2014.2305472 ↗
14. Tracy · 2019
15. Error analysis of aged modules with cracked polyamide backsheets10.1016/j.solmat.2019.110194 ↗
16. Köntges · 2014
17. Simulation of water vapor ingress into PV-modules under different climatic conditions
18. Simulation of water ingress into PV-modules: IEC-testing versus outdoor exposure10.1016/j.solener.2015.03.007 ↗
19. Impact of permeation properties and backsheet-encapsulant interactions on the reliability of PV modules10.5402/2012/459731 ↗
20. Acetic acid permeation through photovoltaic backsheets: influence of the composition on the permeation rate10.1016/j.polymertesting.2017.04.025 ↗
21. Correlation of the loss in photovoltaic module performance with the ageing behaviour of the backsheets used10.1002/pip.2580 ↗
22. Acetic acid production and glass transition concerns with ethylene-vinyl acetate used in photovoltaic devices10.1016/j.solmat.2006.10.009 ↗
23. Temperature dependence of encapsulant volumetris resistivity and influence on potential induced degradation of c-Si modules
24. Potential induced degradation of solar cells and panels
25. Encapsulation of PV modules using ethylene vinyl acetate copolymer as a pottant: a critical review10.1016/0927-0248(95)00150-6 ↗
26. The causes and effects of degradation of encapsulant ethylene vinyl acetate copolymer (EVA) in crystalline silicon photovoltaic modules: a review10.1016/j.rser.2017.06.039 ↗
27. Moisture transport, adhesion, and corrosion protection of PV module packageing materials10.1016/j.solmat.2006.04.003 ↗
28. Investigation of the degradation and stabilization of EVA-based encapsulant in field-aged solar energy modules10.1016/S0141-3910(96)00162-0 ↗
29. Study on the degradation of different types of backsheets used in PV module under accelerated conditions10.1016/j.solmat.2013.09.036 ↗
30. Polymer foil additives trigger the formation of snail trails in photovoltaic modules10.1016/j.solmat.2014.06.028 ↗
31. Relation between degradation of polymeric components in crystalline silicon PV module and climatic conditions: a literature review10.1016/j.solmat.2018.12.027 ↗
32. Insulation resistance in relation to distribution of backsheet types in strings and inverters10.1016/j.solmat.2022.111913 ↗
33. Wet leakage resistance development of modules with various backsheet types10.1002/pip.3481 ↗
34. Evolution of inverter ground impedances for PV modules with various backsheet types10.1002/pip.3481 ↗
35. Quantification of UV protecting additives in ethylene-vinyl acetate copolymer encapsulants for photovoltaic modules with pyrolysis-gas chromatography-mass spectrometry10.1016/j.polymertesting.2022.107913 ↗
36. Influence of typical stabilizers on the ageing behavior of EVA foils for photovoltaic applications during artificial UV-weathering10.1016/j.polymertesting.2015.03.022 ↗
37. Comparison of degradation behavior of newly developed encapsulation materials for photovoltaic applications under different artificial ageing tests10.3390/polym13020271 ↗
38. Determination of stabilisers in polymeric materials used as encapsulants in photovoltaic modules10.1016/j.polymertesting.2013.12.004 ↗
39. Degradation of the encapsulant polymer in outdoor weathered photovoltaic modules: spatially resolved inspection of EVA ageing by fluorescence and correlation to electroluminescence10.1016/j.solmat.2012.03.022 ↗
40. Non-destructive degradation analysis of encapsulants in PV modules by Raman Spectroscopy10.1016/j.solmat.2011.01.030 ↗
41. On-site identification of the material composition of PV modules with mobile spectroscopic devices10.3390/en13081903 ↗
42. Nondestructive characterization of polymeric components of silicon solar modules by near-infrared absorption spectroscopy (NIRA)10.1016/j.solmat.2020.110702 ↗
43. Identification of the backsheet type of silicon photovoltaic modules from encapsulant fluorescence images10.1021/acsaem.2c03532 ↗
44. Climate specific accelerated ageing tests and evaluation of ageing induced electrical, physical, and chemical changes10.1002/pip.3090 ↗
45. Energiefonds
46. Statistical evaluation of PV system performance and failure data among different climate zones10.1016/j.renene.2019.02.135 ↗
47. Eder · 2019
48. Energiefonds · 2022
49. Quantifying the influence of encapsulant and backsheet composition on PV‐power and electrical degradation10.1002/pip.3679 ↗
50. Properties and degradation behaviour of polyolefin encapsulants for photovoltaic modules10.1002/pip.3323 ↗
51. Performance of PV modules using co-extruded backsheets based on polypropylene10.1016/j.solmat.2021.110976 ↗
52. Modeling of rates of moisture ingress into photovoltaic modules10.1016/j.solmat.2006.04.002 ↗
53. Non-destructive failure detection and visualization of artificially and naturally aged PV modules10.3390/en11051053 ↗
54. Review: ultraviolet fluorescence as assessment tool for photovoltaic modules10.1109/JPHOTOV.2019.2961781 ↗
55. ISO/CIE 11664-4:2019, Colorimetry — Part 4: CIE 1976 L*a*b* colour space. https://www.iso.org/standard/74166.html (accessed 18 April 2023).
56. Advanced UV-fluorescence image analysis for early detection of PV-power degradation10.1051/epjpv/2023001 ↗
57. 2021
58. Hipp · 2020
59. 2022
60. 2021 · 2022
61. Degradation science and pathways in PV systems
62. The coefficient of determination R2 and intra-class correlation coefficient from generalized linear mixed-effects models revisited and expanded10.1098/rsif.2017.0213 ↗
63. Barton · 2023
64. Light soaking effects on photovoltaic modules: overview and literature review
65. Nonlinear photovoltaic degradation rates: modeling and comparison against conventional methods10.1109/JPHOTOV.2020.2992432 ↗
66. Crosslinking and post-crosslinking of ethylene vinyl acetate in photovoltaic modules10.1002/app.44912 ↗
67. Optical transmission as a fast and non-destructive tool for determination of ethylene-co-vinyl acetate curing state in photovoltaic modules10.1002/pip.1175 ↗
68. Fluorescence analysis as a diagnostic tool for polymer encapsulation processing and degradation
69. Longitudinal functional data analysis10.1002/sta4.89 ↗
70. Ramsay · 2005
71. Functional regression10.1146/annurev-statistics-010814-020413 ↗
72. Estimating functional linear mixed-effects regression models10.1016/j.csda.2016.09.009 ↗
73. FTIR spectroscopic analysis of poly(ethylene terephthalate) on crystallization10.1016/j.eurpolymj.2012.06.006 ↗
74. Predictive models of poly(ethyleneterephthalate) film degradation under multifactor accelerated weathering exposures10.1371/journal.pone.0177614 ↗
75. Tests in linear mixed effects models10.18637/jss.v082.i13 ↗