Reduction of trapping and recombination in upgraded metallurgical grade silicon: Impact of phosphorous diffusion gettering

N. Dasilva-Villanueva, S. Catalán-Gómez, D. Fuertes Marrón, J.J. Torres, M. García-Corpas, C. del Cañizo

Abstract

Upgraded metallurgical grade (UMG) silicon (Si) has raised interest as an alternative material for solar cells due to its low cost, low environmental impact and low CAPEX. Maximum cell efficiencies at the level of those obtained from high purity poly-Si have been reported. However, a higher defect density and the compensated doping character result in UMG-based cell efficiencies varying over wider ranges in frequency distribution charts. In this report we characterize mc-Si UMG samples with different defect densities, comparing them with mono-Si UMG and commercial high-performance mc-Si samples, analysing the impact of carrier trapping by means of photoconductance (PC) decay measurements, and its evolution after applying a phosphorous diffusion gettering (PDG) process. When analyzing the decay time constant of the PC measurements, slow (66.8+-14.3 ms) and fast (16.1+-3.5 ms) traps are found in mc-Si samples, while no evidence of trapping is found in mono-UMG samples. Slow traps are effectively removed after the PDG process, while fast traps do remain. The influence of dislocations clusters and the possible role of oxygen, as revealed by Fourier-transform infrared spectroscopy (FTIR) is discussed. Finally, the improvement in minority carrier lifetime due to the PDG treatment is reported for each sample type, reaching values up to 140 us in mc-Si samples with no slow traps neither interstitial oxygen FTIR-peaks
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. 2021
2. 2021
3. 2012
4. Requirements of the Paris Climate Agreement for the coming 10 years on investments, technical roadmap, and expansion of PV manufacturing
5. Baliozian · 2020 · 420
6. L. Méndez, E. Forniés, D. Garrain, A.P. Vázquez, A. Souto, Upgraded Metallurgical Grade Silicon for Solar Electricity Production: a Comparative Life Cycle Assessment, (n.d.) vol. 56.
7. Performance of modules and solar cells made of 100% solar silicon purified by direct route
8. Towards 20% solar cell efficiency using silicon from metallurgical process route10.1016/j.egypro.2014.08.030 ↗
9. Mass production test of solar cells and modules made of 100% UMG silicon. 20.76% record efficiency10.3390/en12081495 ↗
10. Microstructure and conversion efficiency of multicrystalline silicon ingot prepared by upgraded metallurgical grade silicon10.1016/j.solmat.2018.06.010 ↗
11. Oxygen-related minority-carrier trapping centers in p-type Czochralski silicon10.1063/1.1483908 ↗
12. Application of phosphorus diffusion gettering process on upgraded metallurgical grade Si wafers and solar cells10.1016/j.apenergy.2010.03.026 ↗
13. Study of defects and impurities in multicrystalline silicon grown from metallurgical silicon feedstock10.1016/j.mseb.2008.05.013 ↗
14. Phosphorus diffusion gettering efficacy in upgraded metallurgical-grade solar silicon10.1007/s11664-018-6331-5 ↗
15. Overview of phosphorus diffusion and gettering in multicrystalline silicon10.1016/j.mseb.2008.10.060 ↗
16. Rein · 2005
17. Contactless determination of current–voltage characteristics and minority‐carrier lifetimes in semiconductors from quasi‐steady‐state photoconductance data10.1063/1.117723 ↗
18. How lifetime fluctuations, grain-boundary recombination, and junctions affect lifetime measurements and their correlation to silicon solar cell performance10.1016/j.solmat.2008.04.001 ↗
19. Anomalously high lifetimes measured by quasi-steady-state photoconductance in advanced solar cell structures10.1063/1.4840337 ↗
20. Trapping of minority carriers in silicon. I. P-type silicon10.1103/PhysRev.97.311 ↗
21. Trapping of minority carriers in multicrystalline silicon10.1063/1.123663 ↗
22. Understanding carrier trapping in multicrystalline silicon10.1016/S0927-0248(00)00134-3 ↗
23. Trapping-related recombination of charge carriers in silicon10.1063/1.3490240 ↗
24. Generalized procedure to determine the dependence os steady-state-photodocductance lifetime on the occupation of multipe defects10.1063/1.2999640 ↗
25. Reassessments of minority carrier traps in silicon with photoconductance decay measurements10.1109/JPHOTOV.2019.2903584 ↗
26. Trapping-related recombination of charge carriers in silicon
27. Jafari · 2019 · vol. 7 · 322
28. Phosphorous diffusion gettering of trapping centers in upgraded metallurgical‐grade solar silicon10.1002/pssr.202100054 ↗
29. Investigating minority carrier trapping in n-type Cz silicon by transient photoconductance measurements10.1063/1.3689786 ↗
30. UMG silicon for solar PV: from defects engineering to PV module degradation10.1016/j.solener.2021.03.076 ↗
31. Temporary surface passivation for characterisation of bulk defects in silicon: A review
32. A new defect Etch for Polycrystalline silicon10.1149/1.2115670 ↗
33. Dislocation engineering in multicrystalline silicon10.4028/www.scientific.net/SSP.156-158.11 ↗
34. An insight into dislocation density reduction in multicrystalline silicon10.1016/j.solmat.2016.03.040 ↗
35. M. Seibt, V. Kveder, Gettering Processes and the Role of Extended Defects, in: Advanced Silicon Materials for Photovoltaic Applications, John Wiley & Sons, Ltd, n.d.: pp. 127-188. https://onlinelibrary.wiley.com/doi/abs/10.1002/9781118312193.ch4.10.1002/9781118312193.ch4 ↗
36. Oxygen precipitation in silicon10.1063/1.359479 ↗
37. Precipitation of oxygen in dislocation-free silicon10.1002/pssa.2210560123 ↗
38. Infrared Spectroscopical and TEM investigations of oxygen precipitation in silicon crystals with medium and high oxygen concentrations10.1002/pssa.2210850116 ↗
39. Oxygen donor formation and oxygen precipitation in czochralski silicon due to heat treatment at 600 to 800oC10.1002/pssa.2210900254 ↗
40. Oxide micro-precipitates in As-grown CZ silicon10.1149/1.2123679 ↗
41. Formation of nuclei of oxygen precipitates in CZ silicon crystals during crystal growth process10.1149/1.2095710 ↗
42. Oxygen distribution on a multicrystalline silicon ingot grown from upgraded metallurgical silicon10.1016/j.solmat.2010.09.013 ↗
43. Competitive gettering of iron in silicon photovoltaics: oxide precipitates versus phosphorus diffusion10.1063/1.4892015 ↗