Impact of corrosion on microstructure and mechanical properties of ZrOx/ZrC-ZrN/Zr absorber–reflector tandem solar selective structures
Source abstract
Abstract
Abstract We investigated the impact of corrosion on pristine and thermally treated ZrOx/ZrC-ZrN/Zr absorber–reflector tandem solar selective coatings (ARTSSCs) on stainless steel (SS) and copper (Cu) substrates using microstructure, electrochemical and nanoindentation measurements. Electrochemical measurements are carried out in 3.5 wt% NaCl solution, emulating the corrosion environments, under potentiodynamic polarization states. The corrosion treated samples exhibit strong correlations among microstructural, mechanical properties and their solar thermal responses. The thermally treated ZrOx/ZrC-ZrN/Zr structures on SS substrates show degraded corrosion resistance from 1379 KΩ to 104 KΩ for vacuum and 435 KΩ for air thermal conditions. The measured mechanical properties, such as Young's modulus and hardness, substantiate the observed corrosion mediated degradation of thermally treated structures under both vacuum and air environmental conditions. The solar thermal performance shows degradation for both pristine and thermally treated sample after corrosion and room temperature after corrosion emissivity ‘e27 °C’ values are ~0.28, 0.35, 0.42 for pristine and thermally treated ZrOx/ZrC-ZrN/Zr structures respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Advanced Surface Polishing Techniques · Solar Thermal and Photovoltaic Systems
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Interannual extremes in the rate of rise of atmospheric carbon dioxidesince 198010.1038/375666a0 ↗
2. M. Dresselhaus, G. Crabtree, Basic Research Needs for the Hydrogen Economy, 2003, p. 178.
3. Global Temperature Patterns10.1126/science.280.5372.2027e ↗
4. Review of physical vapor deposited (PVD) spectrally selective coatings for mid- and high-temperature solar thermal applications10.1016/j.solmat.2011.10.028 ↗
5. Review of mid-to high temperature solar selective absorber materials
6. Applications of thin graded-index films to solar absorbers10.1364/AO.16.001438 ↗
7. Thermal stability studies of sputter-deposited multilayer selective absorber coatings10.1016/0040-6090(82)90618-6 ↗
8. Performance and stability of some new high-temperature selective absorber systems based on metal/dielectric multilayers10.1016/0927-0248(94)90001-9 ↗
9. Very low-emittance solar selective surfaces using new film structures10.1063/1.351510 ↗
10. TiAlN/TiAlON/Si3N 4 tandem absorber for high temperature solar selective applications10.1063/1.2387897 ↗
11. Structure, optical properties and thermal stability of pulsed sputter deposited high temperature HfOx/Mo/HfO2 solar selective absorbers10.1016/j.solmat.2010.04.073 ↗
12. High temperature solar selective coatings .〈http://www.google.com/patents/US20100313875〉, 2010 (accessed 06.01.16).
13. Corrosion behavior of nanolayered TiN/NbN multilayer coatings prepared by reactive direct current magnetron sputtering process10.1016/j.tsf.2004.01.096 ↗
14. Improvement of the corrosion resistance of PVD hard coating–substrate systems10.1016/S0257-8972(99)00551-4 ↗
15. Corrosion and tribocorrosion behaviour of cermet and cermet/nanoscale multilayer CrN/NbN coatings10.1016/j.surfcoat.2009.09.046 ↗
16. B. Usmani, V. Vijay, R., Chhibber, A. Dixit, Spectrally selective response of ZrOx/ZrC-ZrN/Zr absorber-reflector tandem structures on stainless steel and copper substrates for high temperature solar thermal applications, Solar Energy 134, (2016) 353–365, 10.1016/j.solener.2016.05.014.
17. Electrochemical polarization10.1149/1.2428653 ↗
18. Corrosion behavior of nanolayered TiN/NbN multilayer coatings prepared by reactive direct current magnetron sputtering process10.1016/j.tsf.2004.01.096 ↗
19. Electrochemical behavior of single layer CrN , TiN , TiAlN coatings and nanolayered TiAlN / CrN multilayer coatings prepared by reactive direct current magnetron sputtering10.1016/j.tsf.2006.03.008 ↗
20. Corrosion resistance of multi-layered plasma-assisted physical vapour deposition TiN and CrN coatings10.1016/S0257-8972(01)01267-1 ↗
21. Growth, structure, and microhardness of epitaxial TiN/NbN superlattices10.1557/JMR.1992.0901 ↗
22. Determination of susceptibility to intergranular corrosion and electrochemical reactivation behaviour of AISI 316L type stainless steel10.1016/j.corsci.2006.01.003 ↗
23. Effect of film thickness and Ti interlayer on the structure and properties of nanocrystalline TiN thin films on AISI D2 steel10.1016/j.surfcoat.2007.01.012 ↗
24. Synthesis and characterization of nanocrystalline ZrNxOy thin films on Si by ion plating10.1016/j.surfcoat.2006.12.007 ↗
25. Corrosion behavior of TiN, TiAlN, TiAlSiN thin films deposited on tool steel in the 3.5wt% NaCl solution10.1016/j.tsf.2007.08.069 ↗
26. Research on the corrosion behavior of TiN–TiAlN multilayer coatings deposited by cathodic-arc ion plating10.5006/1.3287705 ↗
27. Mechanical properties and corrosion resistance of nanocrystalline ZrNxOy coatings on AISI 304 stainless steel by ion plating10.1016/j.surfcoat.2008.05.001 ↗
28. Kubaschewski · 1993
29. Nanomechanical properties of TiC, TiN and TiCN thin films using scanning probe microscopy and nanoindentation10.1016/j.apsusc.2004.01.053 ↗
30. Measurement of hardness and elastic modulus by instrumented indentation Advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
31. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
32. Shackelford · 2001
33. Influence of oxygen impurities on growth morphology, structure and mechanical properties of Ti-Al-N thin films10.1016/j.tsf.2016.01.039 ↗
34. De Hosson · 2006 · 1
35. Structural, optical and mechanical properties of coloured TiNxOy thin films10.1016/S0040-6090(03)01123-4 ↗
36. The deformation and ageing of mild steel10.1088/0370-1301/64/6/305 ↗
37. The cleavage strength of polycrystals
38. Limits to the preparation of superhard nanocomposites: Impurities, deposition and annealing temperature – EMRS 2011 symp Q10.1016/j.tsf.2012.08.048 ↗