Correlation study between LeTID defect density, hydrogen and firing profile in Ga-doped crystalline silicon
Source abstract
Abstract
Light- and elevated Temperature-induced Degradation (LeTID) remains a challenge for the long-term stability of silicon-based solar cells. Despite numerous publications and studies on the subject, only a link with the hydrogen concentration in the silicon bulk has been established. However, the question remains as to how exactly hydrogen interacts with the defect or even forms part of it. In this study, highly sensitive resistivity measurements and photoluminescence/ photoconductance decay measurements are used to establish a precise correlation between the dominant hydrogen species (H 2 and GaH) and the evolving defect concentration in fired Ga-doped silicon coated with an hydrogen-rich amorphous silicon nitride (SiN x :H). The correlation appears to be linear in both species over the range investigated but the data imply that the defect concentration is proportional to H 2 . An investigation of the behavior of GaH during typical degradation conditions confirms that GaH pairs are hydrogen sinks and therefore do not contribute to the formation of LeTID defects. We therefore expect the hydrogen dimer to act as a precursor for LeTID. In addition, the indiffusion of H during the firing step from a SiN x :H layer was investigated and a strong dependence on the peak temperature was found, whereas a weaker dependence on the cooling rate was observed.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Light induced degradation of rear passivated mc-si solar cells
2. Electronic properties and structure of boron–hydrogen complexes in crystalline silicon10.1002/solr.202100459 ↗
3. Atomic structure of defect responsible for light-induced efficiency loss in silicon solar cells in warmer climates
4. C. Mule, P.C. Taylor, A. Meyer, S. Agarwal, W. Nemeth, V. LaSalvia, M. Page, P. Stradins, Atomistic level study of the defect responsible for light- and elevated-temperature-induced degradation in Ga-doped Czochralski Si using electron paramagnetic resonance, in: Proceedings of the 13th SiliconPV 2023, 2023, accepted for publication with TIB Open Publishing.10.1109/PVSC48320.2023.10359921 ↗
5. Influence of dopant elements on degradation phenomena in B- and Ga-doped Czochralski-grown silicon10.1002/solr.202100147 ↗
6. Possible candidates for impurities in mc-si wafers responsible for light-induced lifetime degradation and regeneration10.1002/solr.201700159 ↗
7. A four-state kinetic model for the carrier-induced degradation in multicrystalline silicon: Introducing the reservoir state10.1016/j.solmat.2018.04.024 ↗
8. Evaluating root cause: The distinct roles of hydrogen and firing in activating light- and elevated temperature-induced degradation10.1063/1.5041756 ↗
9. Evaluating the impact of SiNx thickness on lifetime degradation in silicon10.1109/JPHOTOV.2019.2896671 ↗
10. On the defect physics behind light and elevated temperature-induced degradation (LeTID) of multicrystalline silicon solar cells10.1109/JPHOTOV.2019.2937223 ↗
11. Impact of substrate thickness on the degradation in multicrystalline silicon10.1109/JPHOTOV.2020.3038412 ↗
12. Insights into the hydrogen-related mechanism behind defect formation during light- and elevated-temperature-induced degradation
13. Understanding light- and elevated temperature-induced degradation in silicon wafers using hydrogen effusion mass spectroscopy10.1109/JPHOTOV.2021.3104194 ↗
14. The impact of different hydrogen configurations on light- and elevated-temperature- induced degradation10.1109/JPHOTOV.2023.3236185 ↗
15. Easy-to-apply methodology to measure the hydrogen concentration in boron-doped crystalline silicon10.1016/j.solmat.2019.109970 ↗
16. Methodology and error analysis of direct resistance measurements used for the quantification of boron–hydrogen pairs in crystalline silicon10.1109/JPHOTOV.2021.3074463 ↗
17. Neutralization of shallow acceptor levels in silicon by atomic hydrogen10.1103/PhysRevLett.51.2224 ↗
18. Deactivation of the boron acceptor in silicon by hydrogen10.1063/1.94287 ↗
19. Vibrational characteristics of acceptor-hydrogen complexes in silicon10.1063/1.97978 ↗
20. Temperature gradient image analysis to optimize an ultrafast regeneration of boron–oxygen-related defects10.1109/JPHOTOV.2021.3063659 ↗
21. The dissociation of gallium–hydrogen pairs in crystalline silicon during illuminated annealing
22. On the meaning(fullness) of the intensity unit ‘suns’ in light induced degradation experiments
23. Direct and indirect determination of hydrogen-boron complexes in float-zone silicon wafers10.1063/5.0089274 ↗
24. Laser-fired rear contacts for crystalline silicon solar cells10.1002/pip.422 ↗
25. On the lifetime-equivalent defect density: Properties, application, and pitfalls10.1109/JPHOTOV.2019.2922470 ↗
26. Influence of the high-temperature ”firing” step on high-rate plasma deposited silicon nitride films used as bulk passivating antireflection coatings on silicon solar cells10.1116/1.1609481 ↗
27. Influence of hydrogen effusion from hydrogenated silicon nitride layers on the regeneration of boron-oxygen related defects in crystalline silicon10.1063/1.4833243 ↗
28. On the permeation of hydrogen and helium in single crystal silicon and germanium at elevated temperatures10.1016/S0031-8914(56)90039-8 ↗
29. On the solubility and diffusion coefficient of tritium in single crystals of silicon10.1016/0020-708X(68)90067-7 ↗
30. Kinetic analysis of hydrogen evolution from reactively sputtered amorphous silicon-hydrogen alloys10.1103/PhysRevB.22.6213 ↗
31. Fourier transform infrared study of rapid thermal annealing of a-Si:N:H(D) films prepared by remote plasma-enhanced chemical vapor deposition10.1116/1.579794 ↗
32. Dissociation reactions of hydrogen in remote plasma-enhanced chemical-vapor-deposition silicon nitride10.1116/1.1398538 ↗
33. Hydrogen solubility and defects in silicon
34. Solubility of hydrogen in silicon at 1300°c10.1063/1.108602 ↗
35. Formation, dissociation, and diffusion of various hydrogen dimers in silicon10.1002/pssb.201600779 ↗
36. Impact of hydrogen-rich silicon nitride material properties on light-induced lifetime degradation in multicrystalline silicon
37. Study on boron–hydrogen pairs in bare and passivated float-zone silicon wafers
38. Light- and elevated-temperature-induced degradation-affected silicon cells from a utility-scale photovoltaic system characterized by deep-level transient spectroscopy10.1109/JPHOTOV.2022.3158545 ↗
39. Electronic properties of light- and elevated temperature-induced degradation in float-zone silicon10.1109/JPHOTOV.2022.3195098 ↗
40. Study on boron–hydrogen pairs in bare and passivated float-zone silicon wafers
41. Statistics of the recombinations of holes and electrons10.1103/PhysRev.87.835 ↗
42. Electron-hole recombination in germanium10.1103/PhysRev.87.387 ↗
43. Parameterisation of injection-dependent lifetime measurements in semiconductors in terms of shockley-read-hall statistics: An application to oxide precipitates in silicon10.1063/1.4725475 ↗
44. Recombination parameters of lifetime-limiting carrier-induced defects in multicrystalline silicon for solar cells10.1063/1.4977906 ↗
45. Lifetime spectroscopy investigation of light-induced degradation in p-type multicrystalline silicon PERC10.1109/JPHOTOV.2016.2606699 ↗
46. Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon10.1016/j.solmat.2017.08.003 ↗
47. Understanding the light-induced degradation at elevated temperatures: Similarities between multicrystalline and floatzone p-type silicon10.1002/pip.2954 ↗