Role of headspace environment for phase change carbonates on the corrosion of stainless steel 316L: High temperature thermal storage cycling in concentrated solar power plants

Yanting Yin, Raihan Rumman, Madjid Sarvghad, Stuart Bell, Teng-Cheong Ong, Rhys Jacob, Ming Liu, Ross Flewell-Smith, Shane Sheoran, John Severino, Martin Belusko, Frank Bruno, Geoffrey Will, Theodore A. Steinberg, David A. Lewis, Gunther G. Andersson

Publisher page

Abstract

The mechanisms leading to corrosion in stainless steel containments for thermal energy storage through phase change materials, such as carbonates and chlorides, are crucial for understanding the degradation of these steel alloys. A comprehensive study of this area will allow for down-selection of materials suitable for solar thermal energy storage (TES) operation at an elevated temperature range. Samples of stainless steel (SS) 316L were subjected to a cyclic heat environment of 550–750 °C in air and argon headspace environments, in the presence of a carbonate salt phase change material (PCM). A series of complementary microscopy, spectroscopy and diffractometry analytical techniques were applied to the corroded SS316L. Corrosion rate, interface formation and chemical products with respect to thermal cycling are presented with associated degradation mechanism explained and comparisons are made among different gas environments and varied immersion conditions. In the PCM under ambient air conditions, steel surfaces were mainly corroded by the penetration of oxidants from air, such as H 2 O or O 2 , along grain boundaries. SS316L samples demonstrated more severe degradation when exposed to air with a small fraction of PCM vapour present compared to when they were exposed to liquid or solid PCM. Cycling in Ar resulted in less corrosion in samples as opposed to when they were exposed to an air environment. In an Ar environment corrosion is driven via the formation of chromite, while the SS316L showed a less degradation when exposed to Ar with a small fraction of PCM vapour compared to when it was immersed in PCM. The mechanisms for degradation in air and in Ar are common in that the corrosion products of Cr and Ni dissolve in the PCM thus removing any layer that could protect against corrosion. The present study provides insight into corrosion of stainless-steel when exposed to carbonate salts, in air and inert gas environments, and contributes to down-selection of materials for solar thermal energy storage.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Phase Change Materials Research · Solar Thermal and Photovoltaic Systems · Adsorption and Cooling Systems

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Durability studies of solar reflectors: a review10.1016/j.rser.2016.04.060 ↗
2. Heat transfer fluids for concentrating solar power systems–a review10.1016/j.apenergy.2015.01.125 ↗
3. Corrosion behaviour of carbon materials exposed to molten lithium chloride–potassium chloride salt10.1016/j.carbon.2013.10.040 ↗
4. Chemical degradation in thermally cycled stainless steel 316 with high-temperature phase change material10.1016/j.solmat.2021.111216 ↗
5. Corrosion interface formation in thermally cycled stainless steel 316 with high-temperature phase change material10.1016/j.solmat.2021.111062 ↗
6. Aluminum and silicon based phase change materials for high capacity thermal energy storage10.1016/j.applthermaleng.2015.05.037 ↗
7. Toward tailoring chemistry of silica-based phase change materials for thermal energy storage10.1016/j.isci.2020.101606 ↗
8. Silicon as a phase change material: performance of h-BN ceramic during multi-cycle melting/solidification of silicon
9. Chemical degradation in thermally cycled stainless steel 316 with high-temperature phase change material
10. Corrosion interface formation in thermally cycled stainless steel 316 with high-temperature phase change material
11. Damage analysis of 601 nickel superalloy in eutectic Na2CO3/NaCl molten salt under isothermal and thermal cycling conditions10.1016/j.solener.2019.09.030 ↗
12. Corrosion mechanism of SS316L exposed to NaCl/Na2CO3 molten salt in air and argon environments10.1016/j.corsci.2021.109966 ↗
13. Aggressive corrosion of C-276 nickel superalloy in chloride/sulphate eutectic salt10.1016/j.solener.2021.09.023 ↗
14. Corrosion of a stainless steel and nickel-based alloys in high temperature supercritical carbon dioxide environment10.1016/j.corsci.2012.11.041 ↗
15. Corrosion of annealed AISI 316 stainless steel in sodium environment10.1016/S0022-3115(98)00041-5 ↗
16. Effects of temperature and partial pressure of CO/O2 on corrosion behaviour of stainless-steel in molten LirNa carbonate salt10.1016/S0378-7753(00)00376-1 ↗
17. Hot corrosion studies of boiler steels exposed to different molten salt mixtures at 950 °C10.1016/j.engfailanal.2019.02.013 ↗
18. Corrosion behaviors of 316 stainless steel and Inconel 625 alloy in chloride molten salts for solar energy storage10.1515/htmp-2020-0077 ↗
19. Elevated temperature molten salt corrosion study of SS304L austenitic boiler steel
20. Study of material compatibility for a thermal energy storage system with phase change material10.3390/en11030572 ↗
21. Investigation on Ti6Al4V-V-Cr-Fe-SS316 multi-layers metallic structure fabricated by laser 3D printing10.1038/s41598-017-08580-z ↗
22. Sigma phase in superduplex stainless steel: formation, kinetics and microstructural path10.1590/1980-5373-mr-2016-0436 ↗
23. Novel solid–solid phase-change cascade systems for high-temperature thermal energy storage10.1016/j.solener.2018.10.085 ↗
24. Investigation into the behaviour of aluminium and steel under melt/freeze cyclic conditions10.1016/j.est.2018.03.001 ↗
25. A eutectic salt high temperature phase change material: thermal stability and corrosion of SS316 with respect to thermal cycling10.1016/j.solmat.2017.05.047 ↗
26. Determination of thermo-physical properties and stability testing of high-temperature phase-change materials for CSP applications10.1016/j.solmat.2015.03.014 ↗
27. Corrosion of steel alloys in eutectic NaCl+Na 2 CO 3 at 700 °C and Li 2 CO 3 + K 2 CO 3 + Na 2 CO 3 at 450 °C for thermal energy storage10.1016/j.solmat.2017.05.063 ↗
28. Characterisation of promising phase change materials for high temperature thermal energy storage
29. Liu · 2021
30. Design of sensible and latent heat thermal energy storage systems for concentrated solar power plants: thermal performance analysis10.1016/j.renene.2019.11.115 ↗
31. Liu · 2016
32. Corrosion of stainless steel 316 in eutectic molten salts for thermal energy storage10.1016/j.solener.2018.03.053 ↗
33. Corrosion behavior of Hastelloy-N alloys in molten salt fluoride in Ar gas or in air10.1080/00223131.2015.1043155 ↗
34. Analysis of corrosion of hastelloy-N, alloy X750, SS316 and SS304 in molten salt high-temperature environment10.3390/en14030543 ↗
35. Thermal energy storage using chloride salts and their eutectics10.1016/j.applthermaleng.2016.07.046 ↗
36. Carburization behavior of AISI 316LN austenitic stainless steel – experimental studies and modeling10.1016/j.jnucmat.2010.05.023 ↗
37. Corrosion effect of phase change materials in solar thermal energy storage application10.1016/j.rser.2017.03.018 ↗
38. Comparative interaction of cold-worked versus annealed inconel 601 with molten carbonate salt at 450°C10.1016/j.corsci.2017.01.004 ↗
39. Bimetallic metal–organic framework derived FeO/TiO2 embedded in mesoporous carbon nanocomposite for the sensitive electrochemical detection of 4-nitrophenol10.1016/j.snb.2018.11.083 ↗
40. In situ growth of NiO nanoparticles on carbon paper as a cathode for rechargeable Li–O2 batteries10.1039/C7RA02932B ↗
41. Thickness determination of corrosion layers on iron using XPS depth profiling10.17222/mit.2016.180 ↗
42. Correlation of changes in electronic and device properties in organic photovoltaic with exposure to air10.1002/admi.202101657 ↗
43. Chromium oxide coatings with the potential for eliminating the risk of chromium ion release in orthopaedic implants10.1098/rsos.170218 ↗
44. Depth sensitive X-ray diffraction as a probe of buried half-metallic inclusions
45. The pilling-bedworth ratio of oxides formed from the precipitated phases in magnesium alloys10.3389/fmats.2021.761052 ↗
46. Mechanistic understanding of the temperature dependence of crack growth rate in alloy 600 and 316 stainless steel through high-resolution characterization10.1016/j.actamat.2018.11.039 ↗
47. Stress assisted oxidative failure of Inconel 601 for thermal energy storage10.1016/j.solmat.2016.10.008 ↗
48. Catalyst residue and oxygen species inhibition of the formation of hexahapto-metal complexes of group 6 metals on single-walled carbon nanotubes
49. Compatibility issues between electrodes and electrolytes in solid-state batteries10.1039/C7EE00534B ↗
50. Solution combustion synthesis of nano-chromia as catalyst for the dehydrofluorination of 1,1-difluoroethane10.1007/s10853-016-0313-x ↗
51. Wetting by liquid sodium and fracture path analysis of sodium induced embrittlement of 304L stainless steel10.1557/jmr.2017.435 ↗
52. Standard Molar Gibbs free energy of formation of NaCrO2 by e.m.f. measurements10.1016/0021-9614(87)90157-1 ↗
53. Thermodynamic properties of the double oxides of Na2O with the oxides of Cr, Ni and Fe
54. Vaporization behavior of Na2CO3 and K2CO310.1016/j.calphad.2019.02.004 ↗
55. Investigation of multiplet splitting of Fe 2p XPS spectra and bonding in iron compounds10.1002/sia.1984 ↗
56. NaCrO2 cathode for high-rate sodium-ion batteries10.1039/C5EE00695C ↗
57. NaCrO2/Coffee waste–derived nitrogen‐doped carbon composite as high‐performance cathode material for sodium ion batteries10.1002/bkcs.11834 ↗
58. A study on electrochemical properties of P2-type Na–Mn–Co–Cr–O cathodes for sodium-ion batteries10.1039/C7QI00778G ↗
59. Acceleration of thermal decomposition of molten nitrates by Cr in steel and promotion of this effect by halogens
60. Inhibiting hot corrosion of molten Li2CO3-Na2CO3-K2CO3 salt through graphitization of construction materials for concentrated solar power