Abstract
Abstract Illuminated solar cells are susceptible to various degradation mechanisms that can act to reduce the total energy yield when deployed. One potentially severe form is an increase in carrier recombination in the surface regions. This effect has been reported at both the undoped rear surface and phosphorous diffused emitter of PERC solar cells. This work investigates the influence of a range of surface conditions on the surface-related degradation (SRD) behaviour in PERC solar cells. It is shown that SRD is strongly affected by the doping profile of phosphorous emitters, the use of thin thermal oxides with SiNx:H dielectric passivation layers, the substrate material, and the configuration of the rear surface passivation. It finds that more lightly doped emitters result in more front side SRD, with its extent increasing with the introduction of the SiO2/SiNx:H surface passivation layers. Czochralski silicon (Cz-Si) wafers were observed to be significantly more susceptible to surface degradation than multi-crystalline silicon (mc-Si) wafers, which we attribute to less trapping of hydrogen in the bulk of those substrates. On the rear side of PERC cells, surface degradation was only observed in structures that incorporated the combination of SiO2/SiNx:H rear layers. No SRD was observed in the existing Al2O3/SiNx:H technology used in the industrial PERC cells studied. However, the results presented have implications for future commercial solar cell technologies, which are transitioning towards lightly doped emitters and commonly incorporate thermal oxides for surface passivation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Photovoltaic System Optimization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. 2021
2. Light induced degradation of rear passivated mc-Si solar cells
3. Eliminating light- and elevated temperature-induced degradation in P -type PERC solar cells by a two-step thermal process10.1016/j.solmat.2020.110470 ↗
4. Minority carrier lifetime degradation in boron-doped Czochralski silicon10.1063/1.1389076 ↗
5. Fundamental boron-oxygen-related carrier lifetime limit in mono- and multicrystalline silicon10.1002/pip.586 ↗
6. A new approach to prevent the negative impact of the metastable defect in boron doped CZ silicon solar cells
7. Performance-limiting oxygen-related defects in silicon solar cells10.1149/1.2355764 ↗
8. Hydrogen passivation of B-O defects in Czochralski silicon10.1016/j.egypro.2013.07.317 ↗
9. Advanced hydrogenation of dislocation clusters and boron-oxygen defects in silicon solar cells10.1016/j.egypro.2015.07.113 ↗
10. Rapid stabilization of high-performance multicrystalline P-type silicon PERC cells10.1109/JPHOTOV.2016.2606704 ↗
11. Impact of the firing temperature profile on light induced degradation of multicrystalline silicon10.1002/pssr.201600272 ↗
12. Evaluating the impact of SiNx thickness on lifetime degradation in silicon10.1109/JPHOTOV.2019.2896671 ↗
13. Carrier-induced degradation in multicrystalline silicon: dependence on the silicon nitride passivation layer and hydrogen released during firing10.1109/JPHOTOV.2017.2783851 ↗
14. Influence of Al2O3 and SiNx passivation layers on LeTID, 32nd
15. Possible candidates for impurities in mc-Si wafers responsible for light-induced lifetime degradation and regeneration10.1002/solr.201700159 ↗
16. Light and elevated temperature induced degradation in p-type and n-type cast-grown multicrystalline and mono-like silicon10.1016/j.solmat.2018.03.002 ↗
17. Electronic properties of the metastable defect in boron-doped Czochralski silicon: unambiguous determination by advanced lifetime spectroscopy10.1063/1.1544431 ↗
18. Instability of dielectric surface passivation quality at elevated temperature and illumination10.1016/j.egypro.2016.07.061 ↗
19. Investigating possible causes of light induced degradation in boron-doped float-zone silicon
20. Degradation of surface passivation and bulk in p-type monocrystalline silicon wafers at elevated temperature10.1109/JPHOTOV.2018.2878791 ↗
21. Tan · 2020
22. Hydrogen induced degradation: a possible mechanism for light- and elevated temperature- induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
23. On the defect physics behind light and elevated temperature-induced degradation (LeTID) of multicrystalline silicon solar cells
24. Review of light-induced degradation in crystalline silicon solar cells10.1016/j.solmat.2015.11.047 ↗
25. Different extent and behaviour of LeTID in the past and current PERC silicon solar cells, Asia-Pacific
26. Degradation of surface passivation on crystalline silicon and its impact on light-induced degradation experiments10.1109/JPHOTOV.2017.2755072 ↗
27. Bulk and surface-related degradation in lifetime samples made of Czochralski silicon passivated by plasma-enhanced chemical vapor deposited layer stacks
28. Bulk and surface instabilities in boron doped float-zone samples during light induced degradation treatments10.1016/j.egypro.2017.09.349 ↗
29. A detailed study on light-induced degradation of Cz-Si PERC-type solar cells: evidence of rear surface-related degradation10.1109/JPHOTOV.2018.2850521 ↗
30. Hydrogen induced degradation: a possible mechanism for light- and elevated temperature- induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
31. Hydrogen-induced degradation: explaining the mechanism behind light- and elevated temperature-induced degradation in n- and p-type silicon10.1016/j.solmat.2019.110353 ↗
32. Temperature dependent degradation and regeneration of differently doped mc-Si materials10.1016/j.egypro.2017.09.085 ↗
33. Contactless determination of current-voltage characteristics and minority-carrier lifetimes in semiconductors from quasi-steady-state photoconductance data10.1063/1.117723 ↗
34. Generalized analysis of quasi-steady-state and quasi-transient measurements of carrier lifetimes in semiconductors10.1063/1.371633 ↗
35. Improved parameterization of Auger recombination in silicon10.1016/j.egypro.2012.07.034 ↗
36. Degradation of carrier lifetime in Cz silicon solar cells10.1016/S0927-0248(00)00098-2 ↗
37. The effect of emitter recombination on the effective lifetime of silicon wafers10.1016/S0927-0248(98)00179-2 ↗
38. Statistics of the recombination of holes and electrons10.1103/PhysRev.87.835 ↗
39. Annealing prior to contact firing: a potential new approach to suppress LeTID10.1016/j.solmat.2019.109938 ↗
40. The role of metal-catalyzed chemical etching black silicon in the reduction of light- and elevated temperature-induced degradation in P-type multicrystalline wafers
41. Assessing the impact of thermal profiles on the elimination of light- and elevated-temperature-induced degradation10.1109/JPHOTOV.2018.2874769 ↗
42. Influence of emitter layers on LETID kenetics in multicrystalline silicon, 35th
43. Sperber · 2019
44. Delay of regeneration by adding aluminum in boron doped crystalline Si
45. Interpretation of recombination at c-Si/SiNx interfaces by surface damage10.1063/1.3437643 ↗
46. Hydrogen-induced platelets in disordered silicon10.1016/0038-1098(96)00283-9 ↗
47. Hydrogen-induced platelets in silicon: separation of nucleation and growth10.4028/www.scientific.net/MSF.83-87.33 ↗
48. Study of the composition of hydrogenated silicon nitride SiNx:H for efficient surface and bulk passivation of silicon10.1016/j.solmat.2009.01.023 ↗
49. Passivation and depassivation of silicon dangling bonds at the Si/SiO 2 interface by atomic hydrogen, Appl
50. Hydrogen induced passivation of Si interfaces by Al2 O 3 films and SiO2/Al2 O3 stacks10.1063/1.3497014 ↗
51. Surface passivation of silicon solar cells using plasma-enhanced chemical-vapour-deposited SiN films and thin thermal SiO2/plasma SiN stacks10.1088/0268-1242/16/3/308 ↗
52. An examination of three common assumptions used to simulate recombination in heavily doped silicon
53. A freeware 1D emitter model for silicon solar cells
54. Determination of Si-SiO2 interface recombination parameters using a gate-controlled point-junction diode under illumination10.1109/16.2441 ↗
55. Role of hydrogen: formation and passivation of meta-stable defects due to hydrogen in silicon10.1063/1.5049329 ↗
56. High speed regeneration of BO-defects: improving long term solar cell performance within seconds
57. Hahn · 2016 · vol. 242 · 80
58. On improved passivation stability on highly-doped crystalline silicon and the long-term stability of regenerated Cz-Si10.1016/j.solmat.2018.05.031 ↗
59. Long-term stability of aluminum oxide based surface passivation schemes under illumination at elevated temperatures10.1109/JPHOTOV.2017.2713411 ↗
60. Controlling light- and elevated-temperature-induced degradation with thin film barrier layers10.1109/JPHOTOV.2019.2945199 ↗
61. Influence of hydrogen on the regeneration of boron-oxygen related defects in crystalline silicon10.1063/1.4804310 ↗
62. Reducing LETID with an adjustment of the AlOx-SiNy:H laser system, 37th