journal article·2020-07

Light and elevated temperature induced degradation in B–Ga co-doped cast mono Si PERC solar cells

Chunlan Zhou, Fangxu Ji, Shangzhi Cheng, Junjie Zhu, Wenjing Wang, Dongli Hu

Publisher page

Abstract

Abstract The utilization of boron-doped Si solar cells based on the structure of a passivated emitter and rear cell (PERC) in the solar industry has increased recently. However, this type of high efficiency solar cell is exposed to a so-called light and elevated temperature induced degradation (LeTID). A suppressing of mc-Si LeTID has been studied through a regeneration treatment at high temperature under illumination or in the dark, but most was about the lifetime samples. In this work, to evaluate the applicability of regeneration and annealing at industrial relevant conditions, industrially made B–Ga co-doped cast-mono Si PERC solar cells were treated in a light soaking tool in which the intensity of light and substrate temperature could be adjusted separately and a rapid thermal process (RTP) system. This treatment was evaluated during a subsequent intentional degradation under conditions of 75 °C with an LED white light source at an intensity of 1 kW/m2. The results showed that properly regenerated samples by high intensity illumination at elevated temperatures suffered from the least degradation, while untreated solar cells had most severe degradation. The RTP method could improve the performance of the solar cells but the RTP-treated samples were less stable than the regenerated samples. It demonstrates the application of a fast (around 20 min) regeneration method could be coupled in mass production. Further, RTP treatment combining with an accelerated regeneration step may be a potential method to provide both the improved performance and high anti-LeTID properties in Si PERC solar cells.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Grant
2. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
3. System performance loss due to LeTID10.1016/j.egypro.2017.09.260 ↗
4. Degradation and regeneration in mc-Si after different gettering steps10.1002/pip.2832 ↗
5. Kinetics of carrier-induced degradation at elevated temperature inmulticrystalline silicon solar cells10.1016/j.solmat.2017.05.066 ↗
6. Modulation of carrier-induced defect kinetics in multi-crystalline silicon PERC cells through dark annealing10.1002/solr.201600028 ↗
7. Light-induced lifetime degradation in high-performance multicrystalline silicon: detailed kinetics of the defect activation10.1016/j.solmat.2017.08.007 ↗
8. A new mc-Si degradation effect called LeTID
9. Rapid passivation of carrier-induced defects in p-type multi-crystalline silicon10.1016/j.solmat.2016.05.022 ↗
10. Investigation of temperature and illumination dependencies of carrier-induced degradation in p-type multi-crystalline silicon
11. Longer hydrogenation duration for large area multi-crystalline silicon solar cells based on high-intensity infrared LEDs10.1016/j.optcom.2019.06.011 ↗
12. In-situ characterization of electron-assisted regeneration of Cz-Si solar cells10.1016/j.solmat.2018.05.023 ↗
13. Rapid stabilization of high-performance multicrystalline P-type silicon PERC cells10.1109/JPHOTOV.2016.2606704 ↗
14. Annealing prior to contact firing: a potential new approach to suppress LeTID10.1016/j.solmat.2019.109938 ↗
15. Low-temperature dark anneal as pre-treatment for LeTID in multicrystalline silicon10.1016/j.solmat.2018.12.021 ↗
16. Light-induced activation and deactivation of bulk defects in boron-doped float-zone silicon10.1063/1.4983024 ↗
17. Light and elevated temperature induced degradation in p-type and n-type cast-grown multicrystalline and mono-like silicon10.1016/j.solmat.2018.03.002 ↗
18. The impact of thermal treatment on light-induced degradation of multicrystalline silicon PERC solar cell10.3390/en12030416 ↗
19. Seed manipulation for artificially controlled defect technique in new growth method for quasi-monocrystalline Si ingot based on casting
20. Deep-level transient spectroscopy characterization of electrical traps in p-type multicrystalline silicon with gettering and hydrogenation process10.1016/j.solener.2018.01.027 ↗
21. Deep level transient spectroscopic investigation of carrier trap defects in p-type mc-Si PERC solar cells after elevated temperature light soaking
22. Electronic properties of light induced recombination centers in boron doped Czochralski silicon10.1063/1.371186 ↗
23. On the impact of dark annealing and room temperature illumination on p-type multicrystalline silicon wafers10.1016/j.solmat.2018.09.018 ↗
24. Effect of dissociation of iron-boron pairs in crystalline silicon on solar cell properties10.1002/pip.594 ↗
25. Recombination activity of iron-gallium and iron-indium pairs in silicon10.1063/1.1929096 ↗
26. Reduced fill factors in multicrystalline silicon solar cells due to injection‐level dependent bulk recombination lifetimes10.1002/1099-159X(200007/08)8:4<363::AID-PIP328>3.0.CO;2-Y ↗
27. Acceleration and mitigation of carrier-induced degradation in p-type multi-crystalline silicon10.1002/pssr.201510437 ↗
28. Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon10.1016/j.solmat.2017.08.003 ↗
29. Two‐step debonding of hydrogen from boron acceptors in silicon10.1063/1.105394 ↗
30. Hydrogen passivation of iron-acceptor pairs in boron and gallium co-doped crystalline silicon
31. Influence of bound hydrogen states on carrier-induced degradation in multi-crystalline silicon
32. Defect formation under high temperature dark-annealing compared to elevated temperature light soaking10.1016/j.solmat.2018.06.043 ↗