Single-chamber processes for a-Si:H solar cell deposition
Source abstract
Abstract
Abstract For deposition of a-Si:H p–i–n solar cells, a single-chamber plasma enhanced chemical vapor deposition process at the frequency of 13.56 MHz is developed. A 40×40 cm² deposition chamber, which represents typical industry reactors equipped with showerhead electrodes is employed. Various methods are applied to reduce the boron-cross contamination from the boron-doped p-layer into the intrinsic layer, which is considered to reduce solar cell efficiency by losses especially in the short wavelength range. Three different device configurations and four different chamber treatment methods are studied, aimed to reach stable device efficiencies comparable to multi-chamber systems at minimum chamber treatment effort and treatment time. An ex-situ CO2–plasma treatment applied after deposition of the p-doped layer is found to be effective to reduce boron-cross contamination. However, this CO2-treatment is a time-consuming process step for production. We found a less time consuming treatment: by a chamber evacuation to 9×10−7 mbar subsequent to p-layer deposition. Initial and stable efficiencies of 10.2% and 7.7%, respectively, were obtained. This latter treatment results in a sharp drop of the boron concentration from ∼5×1020 cm−3 in the p-doped layer to ∼1017 cm−3 in the intrinsic layer. For comparison of different reactor geometries and their influence on the cross-contamination we used a small-area (10×10 cm2) lab-type reactor.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Thin-Film Transistor Technologies · Silicon and Solar Cell Technologies · Silicon Nanostructures and Photoluminescence
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. a-Si:H/μc-Si:H stacked cell from VHF-deposition in a single chamber reactor with 9% stabilized efficiency10.1016/S0927-0248(97)00008-1 ↗
2. Manufacturing of large area single junction a-Si:H solar modules with 10.7% efficiency10.1016/0022-3093(93)91090-P ↗
3. M. Kubon, N. Schultz, M. Kohler, C. Beneking, H. Wagner, Modification of TCO–p interface in a-Si:H solar cells by intermediate layers and plasma treatments, in: Proceedings of the 12th European Photovoltaic Solar Energy Conference, Amsterdam, 1994, pp. 1268–1270.
4. T. Repmann, W. Appenzeller, B. Sehrbrock, H. Stiebig, B. Rech, Advanced PECVD process for thin-film silicon solar cells on glass, in: Proceedings of the 19th European Photovoltaic Solar Energy Conference, Paris, France, 2004, pp. 1334–1339.
5. High-efficiency p–i–n a-Si:H solar cells with low boron cross-contamination prepared in a large-area single-chamber PECVD reactor10.1016/j.tsf.2003.11.036 ↗
6. Reduction of the boron cross-contamination for plasma deposition of p–i–n devices in a single-chamber large area radio-frequency reactor10.1016/j.tsf.2004.05.034 ↗
7. J. Ballutaud, A.A. Howling, L. Sansonnes, Ch. Hollenstein, U. Kroll, I. Schoenbaecher, C. Bucher, M. Poppeller, J. Weichart, A. Buelech, F. Jomard, Plasma deposition of p–i–n devices using a single PECVD chamber: study of the boron concentration, in: Proceedings of the 29th EPS Conference on Plasma Physics and Controlled Fusion, Montreux, Switzerland, vol. 26B, 2002, p. 2.029.
8. Hydrogen-plasma reactive flushing for a-Si:H p–i–n solar cell fabrication10.1557/PROC-149-471 ↗
9. J. Woerdenweber, T. Merdzhanova, A.J. Flikweert, T. Zimmermann, U. Zastrow, L. Niessen, W. Reetz, H. Stiebig, W. Beyer, A. Gordijn, Single-chamber process for deposition of thin-film silicon solar cells without plasma treatment, in: Proceedings of the 25th European Photovoltaic Solar Energy Conference and 5th World Conference on Photovoltaic Energy Conversion, Valencia, Spain 2010, pp. 2978–2982.
10. Fast deposition of a-Si:H layers and solar cells in a large-area (40×40cm2) VHF-GD reactor10.1557/PROC-557-121 ↗
11. In situ study of the thermal decomposition of B2H6 by combining spectroscopic ellipsometry and Kelvin probe measurements10.1063/1.344122 ↗
12. Improvement in stabilized efficiency of a-Si:H solar cells through optimized p/i-interface layers10.1016/0927-0248(95)00127-1 ↗
13. J. Xi, D. Shugar, H. Volltrauer, Large area module performance and identification and control of p–i interface correlated device degradation and further improvements in stabilized efficiencies of single-junction a-Si solar cells, in: Proceedings of the First World Conference and Exhibition on Photovoltaic Solar Energy Conversion, 1994, pp. 401–404.
14. Sakai · Journal of Applied Physics · 1990 · 67 · 349410.1063/1.345340 ↗
15. T. Yoshida, S. Fujikake, H. Shimabukuro, Y. Ichikawa, H. Sakai, Open-circuit voltage of p–i–n a-Si based solar cells, in: Proceedings of the 20th IEEE PVSC, 1998 pp. 335–339.10.1109/PVSC.1988.105717 ↗
16. Amorphous silicon p–i–n solar cells with graded interface10.1063/1.97430 ↗
17. Recent developments of silicon thin film solar cells on glass substrates10.1016/S0040-6090(98)01793-3 ↗