journal article·2018-09Open access

Detailed structural and electrical characterization of plated crystalline silicon solar cells

C. Dang, R. Labie, E. Simoen, J. Poortmans

Abstract

Abstract In this paper a detailed study on the electrical characteristics of Ni/Cu/Ag plated p-type Passivated Emitter Rear Contact (PERC) silicon solar cells is reported. By comparing the cell performance of different cell groups, pseudo Fill Factor (pFF) degradation by laser-induced defects, is observed. High-power (hard) laser ablated cells exhibit a lower efficiency and faster degradation with thermal ageing. We also present structural and electrical characterization to further visualize and identify the responsible defects, which turn out to be laser-ablation-induced dislocations, penetrating the silicon emitter and base. Increasing the laser fluence gives rise to a higher dislocation density. These dislocations are further confirmed as active generation-recombination centers by Deep Level Transient Spectroscopy (DLTS) analysis. The laser ablation induced dislocations are unavoidable because even at insufficient laser fluence (0.48 J/cm2) to fully open the dielectric stack, the density is already at the level of 106/cm2. A substitutional nickel peak is also detected by DLTS, suggesting nickel diffusing into the silicon base during the sinter step. Whereas no copper levels are found in the p-type silicon base by DLTS even after thermal aging at 235 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Integrated Circuits and Semiconductor Failure Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. C. Muschelknautz, A. Henning, et al, Standard Printing Techniques – Pushing the Envelope to 75 mg Paste per Cell, in: Proceedings of the 4th metallization workshop.
2. T. Falcon, Ultra-fine Line Printing for Silicon Solar Cells: Mesh Screens or Metal Stencils? in: Proceedings of the 3rd Metallization workshop, 2011.
3. Impact of the unique physical properties of copper in silicon on characterization of copper diffusion barriers10.1002/1521-3951(200011)222:1<261::AID-PSSB261>3.0.CO;2-5 ↗
4. Electroless Cu for VLSI10.1557/S0883769400047308 ↗
5. Nickel silicide formation using excimer laser annealing10.1016/j.egypro.2012.07.101 ↗
6. Physics of copper in silicon10.1149/1.1421348 ↗
7. Quick determination of copper-metallization long-term impact on silicon solar cells10.1149/1.3466984 ↗
8. Copper penetration in laser-doped selective-emitter silicon solar cells with plated nickel barrier layers10.1016/j.solmat.2014.07.026 ↗
9. Characterization of copper diffusion in silicon solar cells10.1016/j.egypro.2015.03.292 ↗
10. Long term stability of copper front side contacts for crystalline silicon solar cells10.1016/j.solmat.2014.12.024 ↗
11. Meco Plating system. 〈https://www.besi.com/products-technology/product-details/product/meco-cpl/show/〉 (Accessed 6 November 2017).
12. R. A. Sinton, A. Cuevas, A quasi-steady-state open-circuit voltage method for solar cell characterization, in: Proceedings of the 16th European PVSEC (2000) pp. 1152–1155.
13. A new preferential etch for defects in silicon crystals10.1149/1.2133401 ↗
14. J. Deckers, X. Loozen, N. Posthuma, B. O’Sullivan, M. Debucquoy, S. Singh, M. Aleman, M. Recaman, I. Gordon, P. Verlinden, R. Mertens, J. Poortmans, Injection dependent emitter Jo measurement under metallized areas using Photoconductance Decay, in: Proceedings of the 28th European PVSEC (2013) pp. 806–810.
15. Deep level transient Fourier spectroscopy (DLTFS) – A technique for the analysis of deep level properties10.1016/0038-1101(88)90071-8 ↗
16. Recombination saturation effects in silicon solar cells10.1109/16.310107 ↗
17. Micro characterization of laser structured solar cells with plated Ni-Ag contacts10.1016/j.solmat.2013.05.036 ↗
18. Investigation of ablation mechanisms for selective laser ablation of silicon nitride layers10.1016/j.egypro.2011.06.188 ↗
19. Laser induced defects in laser doped solar cells10.1002/pip.1043 ↗
20. Atlas for characterization of defect in silicon. Siltronic, Postfach, Germany, 2004.
21. Impact of surface topography and laser pulse duration for laser ablation of solar cell front side passivating SiNx layers10.1063/1.3493204 ↗
22. Investigation of laser ablation induced defects in crystalline silicon solar cells10.1016/j.egypro.2014.08.040 ↗
23. Copper-hydrogen complexes in silicon10.1103/PhysRevB.65.165203 ↗
24. Electrical levels in nickel doped silicon10.1063/1.4901003 ↗
25. E. Simoen, J. Lauwaert, H. Vrielinck, Analytical Techniques for Electrically Active Defect Detection, Semiconductors and Semimetals, Eds L. Romano, V. Privitera, C. Jagadish, 91 (2015) pp. 205–250.10.1016/bs.semsem.2014.12.001 ↗
26. Recombination activity of contaminated dislocations in silicon: a model describing electron-beam-induced current contrast behavior10.1103/PhysRevB.63.115208 ↗
27. Dissociative diffusion of nickel in silicon and self-diffusion of silicon10.1143/JJAP.6.573 ↗
28. Diffusion of nickel in silicon10.1002/pssb.19670200210 ↗
29. The observation of pseudodiffusion of nickel in single-crystal silicon by in-depth Auger electron spectroscopy10.1016/0040-6090(77)90215-2 ↗
30. Some characteristics of diffusion and electrotransport of nickel in silicon
31. Junction leakage generation by NiSi thermal instability characterized using damage-free n+/p silicon diodes10.1143/JJAP.43.5166 ↗
32. Substrate orientation dependence of NiSi junction leakage induced by anisotropic Ni migration in crystal Si10.1143/JJAP.46.1830 ↗
33. Impurities in silicon solar cells10.1109/T-ED.1980.19922 ↗
34. Modeling of light-induced degradation due to Cu precipitation in p-type silicon. II. Comparison of simulations and experiments
35. R. Labie, J. L. Hernandez, J. Govaerts et al., Cu plated i-perc cells: ageing and humidity reliability tests, in: Proceedings of the 26 European PVSEC (2011) pp. 1195–1198.
36. Study of annealing temperature for Ni/Cu/Ag plated front contact single crystalline solar cells10.1109/JPHOTOV.2016.2576683 ↗
37. Eliminate Kirkendall voids in solder reactions on nanotwinned copper10.1016/j.scriptamat.2012.10.024 ↗
38. 1/f noise measurement for faster evaluation of electromigration in advanced microelectronic interconnections