journal article·2016-12

Impact of hydrogen on the permanent deactivation of the boron-oxygen-related recombination center in crystalline silicon

Dominic C. Walter, Jan Schmidt

Publisher page

Abstract

Abstract In a series of lifetime experiments, we examine the impact of hydrogen on the permanent deactivation of the boron-oxygen (BO)-related defect center in Czochralski-grown boron-doped silicon. In the first experiment, the hydrogen concentration in the external source is varied by the deposition of dielectric layers containing various hydrogen concentrations (aluminum oxide and silicon nitride layers) before applying a fast-firing step at high temperature (>800 °C). In the second experiment, the sample cooling rate after high-temperature treatment is varied without hydrogen-rich dielectric layer being present and the surface passivation based on aluminum oxide is applied at low temperature afterwards. In both experiments, it is observed that the sample cooling after the high-temperature treatment has the major impact on the dynamics of BO deactivation process and fast cooling rates enable a fast deactivation. No direct impact of the hydrogen content in the dielectric layers being present during the fast-firing step on the dynamics of the BO deactivation is observed. However, the highest lifetimes in excess of 1 ms are only achievable when a hydrogenation step is performed, which we interpret in terms of a hydrogen passivation of background defects of hitherto unknown nature. In a third experiment, we apply an organic passivation layer by spin-coating, which is dried at low temperature (130 °C). We find in this experiment that even without any hydrogen intentionally introduced into the silicon bulk, an effective deactivation of the BO center can be observed, clearly supporting that no hydrogen is required to enable the BO deactivation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Silicon Nanostructures and Photoluminescence · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. J. Schmidt, A.G. Aberle, R. Hezel, Investigation of carrier lifetime instabilities in Cz-grown silicon, in: Proceedings 26th IEEE PVSC, Anaheim, CA (IEEE, New York, 1997), 1997, p. 13.10.1109/PVSC.1997.653914 ↗
2. S.W. Glunz, S. Rein, W. Warta, J. Knobloch, W. Wettling, On the degradation of Cz-Silicon solar cells, in: Proceedings of the 2nd WC-PVSEC, Vienna, Austria (WIP, Munich, 1998), 1998, p. 1343.
3. Fast-forming boron-oxygen-related recombination center in crystalline silicon10.1063/1.2147727 ↗
4. A. Herguth, G. Schubert, M. Kaes, G. Hahn, A new approach to prevent the negative impact of the metastable defect in boron doped Cz silicon solar cells, in: Proceedings of the 32nd IEEE PVSC (4th WCPEC), Waikoloa, USA, 2006, pp.940–943.10.1109/WCPEC.2006.279611 ↗
5. K.A. Münzer, Hydrogenated silicon nitride for regeneration of light induced degradation, in: Proceedings of the 24th EUPVSEC Hamburg, 2009, pp. 1558–1561.
6. Influence of hydrogen on the regeneration of boron-oxygen related defects in crystalline silicon10.1063/1.4804310 ↗
7. Hydrogen passivation of B-O defects in Czochralski silicon10.1016/j.egypro.2013.07.317 ↗
8. Evidence for the role of hydrogen in the stabilization of minority carrier lifetime in boron-doped Czochralski silicon10.1063/1.4919385 ↗
9. Influence of Hydrogen on the mechanism of permanent passivation of boron-oxygen defects in p-type Czochralski silicon10.1109/JPHOTOV.2015.2466457 ↗
10. Light-Induced boron-oxygen recombination centres in silicon: understanding their formation and elimination10.4028/www.scientific.net/SSP.205-206.3 ↗
11. B. Lenkeit, Elektronische und strukturelle Eigenschaften von Plasma-Siliziumnitrid zur Oberflächenpassivierung von siebgedruckten, bifacialen Silizium-Solarzellen (Ph.D.), Hannover, Germany, 2002.
12. Silicon surface passivation by atomic layer deposited Al2O310.1063/1.2963707 ↗
13. Realistic efficiency potential of next-generation industrial Czochralski-grown silicon solar cells after deactivation of the boron–oxygen-related defect center
14. Effect of rapid thermal annealing on recombination centres in boron-doped Czochralski-grown silicon10.1063/1.4863674 ↗
15. A. Herguth, G. Schubert, M. Kaes, G. Hahn, Further investigations on the avoidance of boron-oxygen related degradation by means of regeneration, in: Proceedings of the 22nd EUPVSEC, Milan, Italy, 2007, pp. 893–896.
16. K.R. McIntosh, S.C. Baker-Finch, OPAL 2: Rapid optical simulation of silicon solar cells, in: Proceedings of the 38th IEEE PVSC, Austin, Texas, 2012, pp. 265–271.10.1109/PVSC.2012.6317616 ↗
17. Hydrogen diffusion at moderate temperatures in p-type Czochralski silicon10.1063/1.1812379 ↗
18. Concentration and penetration depth of H introduced into crystalline Si by hydrogenation methods used to fabricate solar cells10.1063/1.2363684 ↗
19. Drastic changes in the electrical resistance of gold-doped silicon produced by a hydrogen plasma10.1149/1.2114270 ↗
20. Hydrogen diffusion and the catalysis of enhanced oxygen diffusion in silicon at temperatures below 500°C10.1063/1.349338 ↗
21. Organic-silicon heterojunction solar cells: open-circuit voltage potential and stability10.1063/1.4827303 ↗