Improvement in stability of poly(3-hexylthiophene-2,5-diyl)/[6,6]-phenyl-C61-butyric acid methyl ester bulk heterojunction solar cell by using UV light irradiation
Source abstract
Abstract
Abstract A study of organic solar cells based on photoactive blends of the conjugated regioregular-poly(3-hexylthiophene-2,5-diyl) (P3HT) and [6,6]-phenyl-C61-butyric acid methyl ester (PCBM) with different UV-light treatments is presented. As expected, air exposure of an unencapsulated P3HT:PCBM solar cell is observed to result in rapid degradation of device efficiency. In order to ease this degradation, we found that exposing poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) (PEDOT:PSS) to UV light may reduce the degradation and preserve good performance. Samples with PEDOT:PSS exposed to UV light show better long-run stability than the pristine cells. The active layer exposed to UV light shows the poorest performance and degrades rapidly. From the initial value, the efficiency decreased by 56% and 35% for pristine cells and cells with PEDOT:PSS exposed to UV light, respectively. It has been found that device half-life was 650 and 400 h for the samples with and without UV treatment, respectively. The trend in device performance was explained by observed changes in work function of the PEDOT:PSS layer and decreased absorption intensity of P3HT:PCBM.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Organic Electronics and Photovoltaics · Conducting polymers and applications · Perovskite Materials and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. High-efficiency solution processable polymer photovoltaic cells by self-organization of polymer blends10.1038/nmat1500 ↗
2. Thermally stable efficient polymer solar cells with nanoscale control of the interpenetrating network morphology10.1002/adfm.200500211 ↗
3. Efficient tandem polymer solar cells fabricated by all-solution processing10.1126/science.1141711 ↗
4. Large area plastic solar cell modules10.1016/j.mseb.2006.06.008 ↗
5. Production of large-area polymer solar cells by industrial silk screen printing, lifetime considerations and lamination with polyethyleneterephthalate10.1016/j.solmat.2004.02.031 ↗
6. A complete process for production of flexible large area polymer solar cells entirely using screen printing—first public demonstration10.1016/j.solmat.2008.12.001 ↗
7. Stability and photodegradation mechanisms of conjugated polymer/fullerene plastic solar cells10.1016/S0927-0248(99)00094-X ↗
8. Degradation of bulk heterojunction solar cells operated in an inert gas atmosphere: a systematic study10.1016/S0379-6779(00)01504-6 ↗
9. Production aspects of organic photovoltaics and their impact on the commercialization of devices10.1557/mrs2005.10 ↗
10. Stability/degradation of polymer solar cells10.1016/j.solmat.2008.01.005 ↗
11. Water-induced degradation of polymer solar cells studied by H2 18O labeling10.1021/am800039w ↗
12. A roll-to-roll process to flexible polymer solar cells: model studies, manufacture and operational stability studies10.1039/b823001c ↗
13. Analysis of the failure mechanism for a stable organic photovoltaic during 10000h of testing10.1002/pip.794 ↗
14. Effects of photo-oxidation on the performance of poly[2-methoxy-5-(3,7-dimethyloctyloxy)-1,4-phenylene vinylene]:[6,6]-Phenyl C61-butyric acid methylester solar cells10.1002/adfm.200500714 ↗
15. Degradation of organic solar cells due to air exposure10.1016/j.solmat.2006.06.041 ↗
16. Aluminum based cathode structure for enhanced electron injection in electroluminescent organic devices10.1063/1.122367 ↗
17. Enhanced electron injection in organic electroluminescence devices using an Al/LiF electrode10.1063/1.118344 ↗
18. Patterns of efficiency and degradation of composite polymer solar cells10.1016/j.solmat.2004.02.028 ↗
19. Stability and photodegradation mechanisms of conjugated polymer/fullerene plastic solar cells10.1016/S0927-0248(99)00094-X ↗
20. Accurate efficiency determination and stability studies of conjugated polymer/fullerene solar cells10.1016/S0040-6090(01)01589-9 ↗
21. Mechanisms of photodegradation of poly(3-alkylthiophenes) in solution10.1021/ma00063a047 ↗
22. Light-induced degradation of the active layer of polymer-based solar cells10.1016/j.polymdegradstab.2009.11.021 ↗
23. Increasing the work function of poly(3,4-ethylenedioxythiophene) doped with poly(4-styrenesulfonate) by ultraviolet irradiation10.1063/1.2777147 ↗
24. Effects of ultraviolet irradiation on energy band structure and conductivity of polyaniline10.1063/1.2809399 ↗
25. Electrochemical oxidation of poly(3,4-ethylenedioxythiophene)—“in situ” conductivity and spectroscopic investigations10.1016/S0379-6779(99)00271-4 ↗
26. High-conductivity poly(3,4-ethylenedioxythiophene):poly(styrene sulfonate) film and its application in polymer optoelectronic devices10.1002/adfm.200400016 ↗
27. Indium zinc oxide ohmic contact to poly(3,4-ethylenedioxythiophene) poly(styrenesulfonate) induced by UV light10.1016/j.orgel.2009.03.014 ↗