Long-term stability study of the passivation quality of polysilicon-based passivation layers for silicon solar cells
Source abstract
Abstract
Abstract We investigate the stability of the effective lifetime τeff and the recombination current density parameter J0 in n-type silicon samples with symmetric phosphorus doped poly-Si/SiOx structures, and identify factors that contribute to the passivation degradation behavior. It is found that the surface passivation quality of phosphorus doped polysilicon passivating contacts degrades upon dark annealing and light soaking at temperatures between 75 °C and 200 °C, which can lead to a pronounced increase of the recombination current density parameter J0 (one-side) from below 10 fA/cm2 to 50 fA/cm2 or above. The degradation is only detected on fired wafers, whereas the surface passivation quality is found to be stable in the non-fired sister samples. Surprisingly, a recovery of τeff and J0 is observed after the degradation. The degradation and regeneration behaviors depend strongly on temperature and light intensity, and the presence of silicon nitride (SiNx) capping layers during the light soaking. Increasing the annealing temperature dramatically increases the rate of the degradation and the regeneration process, and at the same time reduces the magnitude of the degradation. The regeneration process appears to be affected by the presence of SiNx films during the light soaking treatment. Samples with SiNx films removed after firing suffer a significantly larger degradation upon light soaking without any lifetime regeneration. Grazing incidence X-ray diffraction measurements reveal negligible change in the structural property and crystalline quality of the polysilicon layer during the degradation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Surface recombination velocity of highly doped n-type silicon10.1063/1.363250 ↗
2. The passivated emitter and rear cell (PERC): from conception to mass production10.1016/j.solmat.2015.06.055 ↗
3. Pn Junction applications and transport properties in polysilicon rods10.1016/0038-1101(79)90077-7 ↗
4. Carrier-selective contacts for Si solar cells10.1063/1.4875904 ↗
5. Laser contact openings for local poly-Si-metal contacts enabling 26.1%-efficient POLO-IBC solar cells10.1016/j.solmat.2018.06.020 ↗
6. Passivated rear contacts for high-efficiency n-type Si solar cells providing high interface passivation quality and excellent transport characteristics10.1016/j.solmat.2013.09.017 ↗
7. Fabrication and modeling of high-efficiency front junction N-type silicon solar cells with tunnel oxide passivating back contact10.1109/JPHOTOV.2017.2715720 ↗
8. Stradins · 2014
9. n-Type Si solar cells with passivating electron contact: identifying sources for efficiency limitations by wafer thickness and resistivity variation10.1016/j.solmat.2017.05.042 ↗
10. Mass production of industrial tunnel oxide passivated contacts (i-TOPCon) silicon solar cells with average efficiency over 23% and modules over 345 W10.1002/pip.3180 ↗
11. Effect of the SiO2 interlayer properties with solid-source hydrogenation on passivated contact performance and surface passivation10.1016/j.egypro.2017.09.302 ↗
12. Electron transport and band structure in phosphorus-doped polycrystalline silicon films10.1063/1.3068349 ↗
13. Fabrication and analysis of high-efficiency polycrystalline silicon solar cells10.1109/16.223706 ↗
14. Tunnel oxide passivated contacts as an alternative to partial rear contacts10.1016/j.solmat.2014.06.015 ↗
15. Phosphorus-diffused polysilicon contacts for solar cells10.1016/j.solmat.2015.06.001 ↗
16. Ramspeck · 2012 · 861
17. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
18. Light-induced lifetime degradation in high-performance multicrystalline silicon: detailed kinetics of the defect activation10.1016/j.solmat.2017.08.007 ↗
19. Impact of copper on light-induced degradation in Czochralski silicon PERC solar cells10.1016/j.solmat.2018.07.006 ↗
20. Engineering solutions and root-cause analysis for light-induced degradation in p-type multicrystalline silicon PERC modules10.1109/JPHOTOV.2016.2556981 ↗
21. Degradation and regeneration of n+ doped poly-Si surface passivation on p-type and n-type Cz-Si under illumination and dark annealing10.1109/JPHOTOV.2020.2964987 ↗
22. Effect of carrier-induced hydrogenation on the passivation of the poly-Si/SiOx/c-Si interface
23. Superacid passivation of crystalline silicon surfaces10.1021/acsami.6b07822 ↗
24. Polzin · 2018
25. 22.6% efficient solar cells with polysilicon passivating contacts on n-type solar-grade wafers10.1002/solr.201900297 ↗
26. Quasi-steady-state photoconductance, a new method for solar cell material and device characterization
27. Measurement of the emitter saturation current by a contactless photoconductivity decay method
28. Superacid-derived surface passivation for measurement of ultra-long lifetimes in silicon photovoltaic materials10.1016/j.solmat.2018.03.028 ↗
29. Annealing prior to contact firing: a potential new approach to suppress LeTID10.1016/j.solmat.2019.109938 ↗
30. Light-induced degradation of PECVD aluminium oxide passivated silicon solar cells10.1002/pssr.201409424 ↗
31. Measuring and interpreting the lifetime of silicon wafers10.1016/j.solener.2003.07.033 ↗
32. UV-induced degradation study of multicrystalline silicon solar cells made from different silicon materials10.1016/j.egypro.2013.07.326 ↗
33. Crystalline silicon short-circuit current degradation study: initial results
34. Temperature and light-induced changes in bulk and passivation quality of boron-doped float-zone silicon coated with SiNx:H10.1109/JPHOTOV.2017.2649601 ↗
35. Degradation of surface passivation and bulk in p-type monocrystalline silicon wafers at elevated temperature10.1109/JPHOTOV.2018.2878791 ↗
36. Feldmann · 2019
37. Lifetime degradation and regeneration in multicrystalline silicon under illumination at elevated temperature10.1063/1.4944839 ↗
38. Kersten · 2016 · 1830
39. Light beam induced current of light-induced degradation in high-performance multicrystalline Al-BSF cells10.1016/j.egypro.2017.09.327 ↗
40. Effect of low-temperature annealing on defect causing copper-related light-induced degradation in p-type silicon10.1016/j.egypro.2017.09.314 ↗
41. Hydrogen induced degradation: a possible mechanism for light- and elevated temperature-induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
42. Carrier-induced degradation in multicrystalline silicon: dependence on the silicon nitride passivation layer and hydrogen released during firing10.1109/JPHOTOV.2017.2783851 ↗
43. Impact of the firing temperature profile on light induced degradation of multicrystalline silicon10.1002/pssr.201600272 ↗
44. Firing temperature profile impact on light induced degradation in multicrystalline silicon10.1016/j.egypro.2017.09.082 ↗
45. Impact of hydrogen-rich silicon nitride material properties on light-induced lifetime degradation in multicrystalline silicon10.1002/pssr.201900201 ↗
46. LeTID in p-type and n-type mono-like and float-zone silicon, and their dependence on SiNx film properties
47. Hydrogenation of phosphorus-doped polycrystalline silicon films for passivating contact solar cells10.1021/acsami.8b19989 ↗
48. Hydrogen passivation of poly-Si/SiOx contacts for Si solar cells using Al 2O3 studied with deuterium10.1063/1.5031118 ↗
49. Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon10.1016/j.solmat.2017.08.003 ↗
50. Degradation of surface passivation on crystalline silicon and its impact on light-induced degradation experiments10.1109/JPHOTOV.2017.2755072 ↗
51. Removal of hydrogen and deposition of surface charge during rapid thermal annealing
52. Solubility of hydrogen in silicon at 1300 °C10.1063/1.108602 ↗
53. The interaction of hydrogen with deep level defects in silicon