Eliminating light- and elevated temperature-induced degradation in P-type PERC solar cells by a two-step thermal process
Source abstract
Abstract
Abstract Light- and elevated temperature-induced degradation (LeTID) can have a severe impact on the carrier lifetime of silicon substrates used in solar cell production and thus remains a crucial challenge for manufacturers. In this work, we introduce a two-step annealing process to mitigate LeTID in multi-crystalline silicon (mc-Si) passivated emitter and rear cell (PERC) solar cells. We demonstrate that the first annealing step (450 °C) with a slow belt speed (0.5 m/min) plays a primary role in mitigating LeTID in the cells, but also results in an increase in contact resistance. The application of a second annealing step at a similar temperature (400–500 °C) with a faster belt speed (1.4 m/min) recovers the contact resistance whilst maintaining the stability of the cell. Applying this approach to the p-type mc-Si PERC solar cells resulted in a reduction of efficiency loss during light soaking from ~6%rel (control) to ~1%rel (treated sample). This finding is significant for p-type mc-Si solar cell manufacturers, as the process can be applied to finished cells using a standard belt firing furnace to stabilise cell efficiency for long term operation in the field.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. Light induced degradation of rear passivated mc-Si solar cells
2. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
3. Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon10.1016/j.solmat.2017.08.003 ↗
4. Temperature dependent degradation and regeneration of differently doped mc-Si materials10.1016/j.egypro.2017.09.085 ↗
5. Light and elevated temperature induced degradation in p-type and n-type cast-grown multicrystalline and mono-like silicon10.1016/j.solmat.2018.03.002 ↗
6. Mass production of p-type Cz silicon solar cells approaching average stable conversion efficiencies of 22 %10.1016/j.egypro.2017.09.308 ↗
7. Dependence of LeTID on brick height for different wafer suppliers with several resistivities and dopants
8. Magazine
9. Role of post-metallization anneal sequence and forming gas anneal to mitigate light and elevated temperature induced degradation of multicrystalline silicon solar cells10.1016/j.solmat.2019.02.036 ↗
10. REC Group · 2019
11. Degradation and regeneration in mc-Si after different gettering steps10.1002/pip.2832 ↗
12. Light-induced degradation variation in industrial multicrystalline PERC silicon solar cells10.1063/1.5049332 ↗
13. Kinetics of carrier-induced degradation at elevated temperature in multicrystalline silicon solar cells10.1016/j.solmat.2017.05.066 ↗
14. Impact of hydrogen-rich silicon nitride material properties on light-induced lifetime degradation in multicrystalline silicon10.1002/pssr.201900201 ↗
15. Recovery of LeTID by low intensity illumination: reaction kinetics, completeness and threshold temperature10.1016/j.egypro.2017.09.090 ↗
16. Lifetime spectroscopy investigation of light-induced degradation in p-type multicrystalline silicon PERC10.1109/JPHOTOV.2016.2606699 ↗
17. Understanding the light-induced degradation at elevated temperatures: similarities between multicrystalline and floatzone p-type silicon10.1002/pip.2954 ↗
18. Lifetime degradation in multicrystalline silicon under illumination at elevated temperature: indications for the involvement of hydrogen10.1063/1.5049320 ↗
19. Evolution of LeTID defects in p-type multicrystalline silicon during degradation and regeneration10.1109/JPHOTOV.2017.2695496 ↗
20. Hydrogen-induced degradation
21. Impact of the firing temperature profile on light induced degradation of multicrystalline silicon10.1002/pssr.201600272 ↗
22. Evaluating root cause: the distinct roles of hydrogen and firing in activating light- and elevated temperature-induced degradation10.1063/1.5041756 ↗
23. A four-state kinetic model for the carrier-induced degradation in multicrystalline silicon : introducing the reservoir state10.1016/j.solmat.2018.04.024 ↗
24. Evaluating the impact of SiNx thickness on lifetime degradation in silicon10.1109/JPHOTOV.2019.2896671 ↗
25. Rapid passivation of carrier-induced defects in p-type multi-crystalline silicon10.1016/j.solmat.2016.05.022 ↗
26. Fast regeneration processes to avoid light-induced degradation in multicrystalline silicon solar cells, 2017 IEEE 44th Photovolt
27. Rapid stabilization of high-performance multicrystalline P-type silicon PERC cells10.1109/JPHOTOV.2016.2606704 ↗
28. Engineering solutions and root-cause analysis for light-induced degradation in p-type multicrystalline silicon PERC modules10.1109/JPHOTOV.2016.2556981 ↗
29. Lifetime degradation and regeneration in multicrystalline silicon under illumination at elevated temperature10.1063/1.4944839 ↗
30. Method of producing solar cells
31. Solar cell manufacturing process and solar cell treatment process
32. Carrier-induced degradation in multicrystalline silicon: dependence on the silicon nitride passivation layer and hydrogen released during firing10.1109/JPHOTOV.2017.2783851 ↗
33. Possible candidates for impurities in mc-Si wafers responsible for light-induced lifetime degradation and regeneration10.1002/solr.201700159 ↗
34. Annealing prior to contact firing: a potential new approach to suppress LeTID10.1016/j.solmat.2019.109938 ↗
35. Assessing the impact of thermal profiles on the elimination of light- and elevated-temperature-induced degradation10.1109/JPHOTOV.2018.2874769 ↗
36. Low-T anneal as cure for LeTID in Mc-Si PERC cells
37. Sharma · 2018 · 1
38. Instability of increased contact resistance in silicon solar cells following post-firing thermal processes10.1002/solr.201700129 ↗
39. Hydrogen induced contact resistance in PERC solar cells10.1016/j.solmat.2018.04.036 ↗
40. Impact of extended contact cofiring on multicrystalline silicon solar cell parameters10.1109/JPHOTOV.2016.2621342 ↗
41. The behavior and transport of hydrogen in silicon solar cells observed through changes in contact resistance, 7th world
42. A quasi-steady-state open-circuit voltage method for solar cell characterization
43. A review and comparison of different methods to determine the series resistance of solar cells10.1016/j.solmat.2007.05.026 ↗
44. Contact resistance: its measurement and relative importance to power loss in a solar cell10.1109/T-ED.1984.21584 ↗
45. Contactless determination of current-voltage characteristics and minority-carrier lifetimes in semiconductors from quasi-steady-state photoconductance data10.1063/1.117723 ↗
46. Generalized analysis of quasi-steady-state and quasi-transient measurements of carrier lifetimes in semiconductors10.1063/1.371633 ↗
47. Improved parameterization of Auger recombination in silicon10.1016/j.egypro.2012.07.034 ↗
48. An advanced software suite for the processing and analysis of silicon luminescence images10.1016/j.cpc.2017.02.012 ↗
49. Temperature induced degradation of the contact resistance of Ag-screen printed p-type silicon solar cells
50. J. Asensio-Lozano, G. Vander Voort, The Al-Si phase diagram, TECH NOTES. 5 (n.d.) 5–9.
51. Impact of dark annealing on the kinetics of light- and elevated-temperature-induced degradation
52. Manipulation of hydrogen charge states for passivation of P-type wafers in photovoltaics10.1109/JPHOTOV.2014.2339494 ↗
53. Samadi · 2019 · vol 140007 · 2052
54. Evolution of p-type LeTID defects in multicrystalline silicon during degradation and regeneration
55. On the defect physics behind light and elevated temperature-induced degradation (LeTID) of multicrystalline silicon solar cells
56. Influence of different transition metal contaminations on degradation
57. Nanometer-scale metal precipitates in multicrystalline silicon solar cells10.1063/1.1330552 ↗
58. Direct observation of hydrogen at defects in multicrystalline silicon
59. Hydrogen passivation of multicrystalline silicon
60. Defect passivation on cast-mono crystalline screen-printed cells10.1007/s11708-016-0443-5 ↗
61. Different Extent and Behaviour of LeTID in the Past and Current PERC Silicon Solar Cells