Drift characteristics of mobile ions in SiNx films and solar cells
Source abstract
Abstract
Abstract Low temperature (30–200 °C) drift characteristics of mobile ions in PECVD SiNx films and solar cells were determined for the first time using a non-contact ion-drift spectrometry technique adopted from silicon integrated circuit (IC) metrology. The results demonstrate drift of Na+ ions in PECVD SiNx films that begin at temperatures as low as 50 °C. This is a seemingly contrasting behavior as compared to SiNx films used in microelectronics where it provides excellent protection as a diffusion barrier. The present study was carried out on SiNx films and final solar cells intentionally contaminated with Na, K, and Cu. In non-contact ion-drift spectrometry an electric field across the dielectric is created by charge deposited on the dielectric surface with a corona discharge in air. Temperature stress is applied by ramping the temperature with time at a controlled rate. Ion drift decreases the dielectric voltage that is monitored with a vibrating Kelvin-probe. Voltage versus time, voltage versus temperature, and corresponding derivative characteristics are used to quantify drift velocity, ion concentration and drift activation energy. The latter produces characteristic ion peaks in the derivative spectra dV/dT versus temperature. The metrology version for mobile ion mapping is based on whole-wafer corona bias-temperature stress at selected temperatures corresponding to drift of different ions. The mapping is a powerful means for ion source identification, such as Na from cell encapsulation glass. It shall prove advantageous for further clarification of the role of Na in potential induced degradation (PID) effects i.e. the polarization effect and the potential induced shunting (PIS).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrostatic Discharge in Electronics · Thin-Film Transistor Technologies · High voltage insulation and dielectric phenomena
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. M. Schutze et al., Investigation of potential induced degradation of silicon photovoltaic modules, in: Proceedings of the 26th EUPVSEC, Hamburg, Germany, 2011, pp. 3097.10.1109/PVSC.2011.6186080 ↗
2. On the mechanism of potential-induced degradation in crystalline silicon solar cells10.1002/pssr.201206276 ↗
3. Micro structural root cause analysis of pontential induced degradation in c-si solar cells10.1016/j.egypro.2012.07.020 ↗
4. Explanation of potential-induced degradation of the shunting type by Na decoration of stacking faults in Si solar cells10.1016/j.solmat.2013.06.015 ↗
5. Sodium diffusion in plasma-deposited amorphous oxygen-doped silicon nitride (aSi-ON:H) films10.1063/1.340144 ↗
6. Chemical vapor deposition
7. F.A. Stevie et al., “Monitoring of sodium ions in SiO2 using corona charging”, in: Proceedings of the Electrochemical Society, vols. 97–12, p. 357.
8. J. lagowski et al., “Method and system for elevated temperature measurement with probes designed for room temperature measurement” U.S. Patent 6.771, 091B2, August 3, 2004.
9. H. Nagel et al., “Crystalline Si solar cells and modules featuring excellent stability against potential-induced degradation”, in: Proceedings of the 26th EUPVSEC, Hamburg, Germany, 2011, pp. 3107–3112.
10. M. Junghanel et al., “Solar cell manufacturing method and testing method”, US patent 20110308602A1, December 22, 2011.
11. M. Wilsonet al., “Importance of defect photoionization in silicon-rich SiNx dielectrics for high PID resistance “, in: Proceedings of the 39th IEEE Photovoltaic Specialist Conference, Tampa, FL, USA, June 16–21, 2013, pp. 0218–0222.10.1109/PVSC.2013.6744134 ↗
12. S. Kochet al., “Work towards simulation model for the potential induced degradation effect on crystalline silicon cells”, in: Proceedings of the 28th EU PVSEC, Paris, France, 2013, pp. 1665–1671.
13. Fast Noncontact Diffusion-process Monitoring