Corrosion behaviour of the 347H stainless steel in molten NaCl-KCl-AlCl3 salts containing aluminum at 500 °C
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Molten salt chemistry and electrochemical processes · Thermodynamic and Structural Properties of Metals and Alloys · Thermal Expansion and Ionic Conductivity
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Dissolution characteristics of Al-Si alloys in AlCl3-NaCl-KCl molten salt at 423 K
2. Formation of porous gold electrodeposits by pulse technique in AlCl3-NaCl-KCl molten salt containing AuCl
3. Fast-charging aluminium-chalcogen batteries resistant to dendritic shorting10.1038/s41586-022-04983-9 ↗
4. A review of the thermophysical properties and potential of ionic liquids for thermal applications10.1039/D1TA03656D ↗
5. Survey of properties of key single and mixture halide salts for potential application as high temperature heat transfer fluids for concentrated solar thermal power systems10.3934/energy.2014.2.133 ↗
6. Corrosion behavior of metallic alloys in molten chloride salts for thermal energy storage in concentrated solar power plants: a review10.1007/s11705-018-1720-0 ↗
7. Corrosion behavior of Ni-Al alloys beneath chlorides melt salt at 700 oC10.1016/j.solener.2019.04.045 ↗
8. Corrosion behavior and mechanism of 316 stainless steel in NaCl-KCl-FeCl3 molten salt and vapor at 300°C10.1002/maco.202313895 ↗
9. Corrosion evaluation and resistance study of alloys in chloride salts for concentrating solar power plants10.1007/s12598-023-02506-7 ↗
10. High temperature corrosion behaviour of the 316 stainless steel in NaCl-KCl-AlCl3 molten salt and its vapour10.1016/j.corsci.2023.111768 ↗
11. Corrosion behaviours of Ni-Mo-Cr alloy and 316 stainless steel in molten NaCl-KCl-AlCl3 salts at high temperature10.1080/1478422X.2022.2148855 ↗
12. Effect of thickness on degradation of austenitic 347H steel by direct-fired supercritical CO2 power cycle environment10.1016/j.corsci.2021.109795 ↗
13. Oxidation behaviour of T91/347H welds10.1016/j.jmatprotec.2018.05.020 ↗
14. Solar thermal irradiation cycles and their influence on the corrosion behaviour of stainless steels with molten salt used in concentrated solar power plants10.1016/j.solmat.2022.112141 ↗
15. Corrosion in the molten fluoride and chloride salts and materials development for nuclear applications10.1016/j.pmatsci.2018.05.003 ↗
16. Lai · 2007 · 409
17. Corrosion behavior of 20G and TP347H in molten LiCl-NaCl-KCl salt10.3390/nano14121026 ↗
18. Corrosion of alloys in a chloride molten salt (NaCl-LiCl) for solar thermal technologies10.1016/j.solmat.2016.05.052 ↗
19. In-situ MgO generation method: a new strategy for mitigating the corrosivity of molten chloride salt10.1016/j.corsci.2022.110145 ↗
20. Corrosion behavior of iron-based and Ni-based alloys melted in NaCl-MgCl2-KCl mixed molten salt under vacuum atmosphere10.1016/j.jmrt.2023.12.121 ↗
21. Electronic structure and magnetic properties of Fe2YSi (Y=Cr, Mn, Fe, Co, Ni) Heusler alloys: a theoretical and experimental study10.1088/0022-3727/40/22/039 ↗
22. Investigation of the structural competing and atomic ordering in Heusler compounds Fe2NiSi and Ni2FeSi under strain condition
23. Thermal decomposition of aluminum chloride hexahydrate10.1021/ie058005y ↗