Accelerated corrosion of stainless steel and Ni-based alloys in molten NaNO3-KNO3 salt vapour phases
Source abstract
Abstract
The corrosion behaviour of four commonly used corrosion-resistant alloys in eutectic nitrate salt (NaNO₃/KNO₃) and its vapour phase was examined at 565 °C for 28 days. The findings revealed significantly higher corrosion rates in the vapour phase compared to the liquid phase. Samples exposed to vapour salt exhibited severe surface damage, including spallation of the outer oxide layer, whereas those in the liquid phase showed lower chromium depletion at the corroding interface. Double oxide layer was found on both stainless steels and Ni-based alloy but with different thickness and oxide layer composition. Loose and porous Fe-Na oxide layer formed on stainless steels in vapour tended to peel off and accelerated the corrosion rate by exposing the inner layer/bulk material to corrosive environment directly. A thinner oxide layer was found on Ni-based alloy. This was identified as a dense and protective inner NiO layer with Fe oxide particles distributed above the layer. These findings highlight the critical importance of considering the potential for salt vapour corrosion during material selection for practical applications, even if most salts are of low vapour pressure. • Comparative corrosion behaviour of four CRA was studied in molten salt and vapour. • Corrosion rate of alloys was higher in vapour of nitrate salts than in its molten form. • Increased corrosion rate in the vapour phase is due to spallation of oxides. • Corrosion mitigation was found when sample immersed into liquid salt. • TEM-HAADF was used to identify the double layer formed on Ni-based alloy.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Phase Change Materials Research · Pigment Synthesis and Properties · Thermodynamic and Structural Properties of Metals and Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. The corrosion behaviour of stainless steels and Ni-based alloys in nitrate salts under thermal cycling conditions in concentrated solar power plants10.1016/j.solener.2021.12.072 ↗
2. Review on system and materials requirements for high temperature thermal energy storage. Part 1: general requirements10.1016/j.rser.2016.11.119 ↗
3. A comprehensive review of state-of-the-art concentrating solar power (CSP) technologies: current status and research trends10.1016/j.rser.2018.04.097 ↗
4. Effect of thermal cycling on the corrosion behaviour of stainless steels and Ni-based alloys in molten salts under air and argon10.1016/j.solener.2022.04.041 ↗
5. Solar thermal irradiation cycles and their influence on the corrosion behaviour of stainless steels with molten salt used in concentrated solar power plants10.1016/j.solmat.2022.112141 ↗
6. Sensible energy storage options for concentrating solar power plants operating above 600 °C10.1016/j.rser.2019.01.062 ↗
7. Selection principles and thermophysical properties of high temperature phase change materials for thermal energy storage: a review10.1016/j.rser.2017.05.271 ↗
8. Corrosion of steel alloys in molten NaCl + Na2SO4 at 700 °C for thermal energy storage10.1016/j.solmat.2017.11.017 ↗
9. Ni-Mo-Cr alloy corrosion in molten NaCl-KCl-MgCl2 salt and vapour10.1016/j.corsci.2020.109183 ↗
10. Corrosion behaviour of 316 stainless steel in NaCl-KCl-MgCl2 salt vapour at 700°C10.1016/j.corsci.2021.109921 ↗
11. Corrosion of Inconel 601 in molten salts for thermal energy storage10.1016/j.solmat.2017.07.036 ↗
12. Corrosion of steel alloys in eutectic NaCl+Na 2 CO 3 at 700 °C and Li 2 CO 3 + K 2 CO 3 + Na 2 CO 3 at 450 °C for thermal energy storage10.1016/j.solmat.2017.05.063 ↗
13. Investigation of the early stage corrosion characteristics of molten (nitrate) salt – oxide – metal interfaces, and the links to interfacial thermo-mechanical stress10.1016/j.corsci.2023.111282 ↗
14. Corrosion behavior of Fe-Cr-Ni alloys in molten NaNO3-KNO3 salt mixture and vapor
15. Corrosion behavior and mechanism of austenitic stainless steels in a new quaternary molten salt for concentrating solar power10.1016/j.solmat.2019.01.024 ↗
16. Corrosion of steel alloys in eutectic NaCl+Na2CO3 at 700°C and Li2CO3 + K2CO3 + Na2CO3 at 450°C for thermal energy storage10.1016/j.solmat.2017.05.063 ↗
17. A eutectic salt high temperature phase change material: thermal stability and corrosion of SS316 with respect to thermal cycling10.1016/j.solmat.2017.05.047 ↗
18. Damage analysis of 601 nickel superalloy in eutectic Na2CO3/NaCl molten salt under isothermal and thermal cycling conditions10.1016/j.solener.2019.09.030 ↗
19. Materials corrosion for thermal energy storage systems in concentrated solar power plants10.1016/j.rser.2018.01.010 ↗
20. Corrosion performance of Ni-based structural alloys for applications in molten-salt based energy systems: experiment & numerical validation10.1016/j.corsci.2021.109607 ↗
21. Cyclic hot corrosion behavior and mechanism of GH4738 superalloy in mixed molten salt10.1016/j.jmrt.2024.08.162 ↗
22. Residual stress analysis in thermally grown oxide scales developed on Nb-alloyed refractory austenitic stainless steels10.1016/j.corsci.2020.109066 ↗