journal article·2026-06Open access

A novel damp heat-induced failure mechanism in PV modules (with case study in TOPCon)

Haoran Wang, Chandany Sen, Muhammad Umair Khan, Ting Huang, Hao Song, Munan Gao, Ruirui Lv, Yuanjie Yu, Bram Hoex

Abstract

Silicon solar technology continues to dominate the market, with Tunnel Oxide Passivated Contact (TOPCon) technology leading in efficiency. However, as devices approach fundamental performance limits, new failure modes may emerge or existing ones may become more critical, and their long-term reliability remains insufficiently understood. This study investigates the effect of damp heat (DH) exposure on bifacial n-type TOPCon modules with laser-assisted fired contacts, utilising different encapsulants: EVA, POE, and EVA-POE-EVA (EPE). After 2000 h of DH testing, modules showed P max losses ranging from ∼6% rel to ∼16% rel , primarily due to reduced V oc caused by increased rear-side recombination. Modules encapsulated with POE on both sides degraded least (∼8% rel ), while those using white EVA on the rear side suffered higher losses, especially when combined with EPE on the front (∼16% rel ). Material analyses revealed a degradation pathway driven by magnesium (Mg) additives in the white EVA. Under DH exposure, Mg hydrates and generates an alkaline micro-environment that corrodes the SiN x :H layer, facilitating moisture ingress in the poly-Si and SiO x layers. This enhances interfacial hydrogen concentration, leading to depassivation and Mg-rich shunting defects, thereby increasing J 0, rear and reducing V oc . These findings underscore the need to control encapsulant composition by limiting Mg in white EVA and improving cell passivation. The minimodules studied here were specifically fabricated R&D purposes to probe humidity-induced degradation pathways. Through an in-depth understanding of this mechanism and thorough optimisation of cell and encapsulant design, effective mitigation strategies have been integrated upstream of module production, substantially eliminating the risk in commercial modules. • The maximum power (P max ) losses of TOPCon modules ranged from ∼6% rel to ∼16% rel after 2000 h of damp heat testing. • The primary degradation mechanism is a reduction in open-circuit voltage (V oc ) due to increased rear-sided recombination. • Magnesium (Mg)-driven corrosion of SiN x :H was identified as a newly recognised degradation pathway. • Mg hydration formed alkaline micro-environments, causing SiN x :H corrosion and depassivation. • Findings highlight the need for Mg control in white EVA and optimised cell passivation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Photovoltaic System Optimization Techniques · Silicon and Solar Cell Technologies · solar cell performance optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. 2025 · vol. 16
2. The value of stability in photovoltaics10.1016/j.joule.2021.10.019 ↗
3. Is TOPCon ready for EVA? Insights from damp heat testing of glass-backsheet modules10.1016/j.solmat.2025.113650 ↗
4. Corrosion effects in bifacial crystalline silicon PV modules; interactions between metallization and encapsulation10.1016/j.solmat.2023.112321 ↗
5. Buyer aware: three new failure modes in TOPCon modules absent from PERC technology10.1016/j.solmat.2024.112877 ↗
6. Hidden traces: insights into how solar cell handling drives damp-heat failures in HJT and TOPCon modules10.1016/j.solmat.2025.113695 ↗
7. Damp-heat stability investigation of glass-backsheet modules based on TOPCon solar cells10.1016/j.solmat.2025.113764 ↗
8. Four failure modes in silicon heterojunction glass-backsheet modules10.1016/j.solmat.2023.112358 ↗
9. Damp heat induced degradation of silicon heterojunction solar cells with Cu-Plated contacts10.1109/JPHOTOV.2019.2941693 ↗
10. Lower levelized cost of energy achievement of silicon heterojunction solar modules with low water vapor transmission rate encapsulants10.1002/ente.202201466 ↗
11. Determining the degree of crosslinking of ethylene vinyl acetate photovoltaic module encapsulants—A comparative study10.1016/j.solmat.2013.04.022 ↗
12. Energy assessment of photovoltaic modules10.1016/j.solener.2021.02.055 ↗
13. Relationship between cross-linking conditions of ethylene vinyl acetate and potential induced degradation for crystalline silicon photovoltaic modules10.7567/JJAP.54.08KG01 ↗
14. RenewSys India, “EVA v/s POE: a comparative study of solar panel encapsulants,” RenewSys World. Accessed: December. 15, 2025. [Online]. Available: https://www.renewsysworld.com/post/eva-v-s-poe-a-comparative-study-of-solar-panel-encapsulants.
15. Novel EPE co-extruded encapsulating films with UV down-conversion power gain effect for highly efficient solar cells10.1016/j.solmat.2023.112373 ↗
16. Determining the crosslinking and degradation reaction kinetics in photovoltaic encapsulants using accelerated aging
17. Comparison of glass/glass and glass/backsheet PV modules using bifacial silicon solar cells10.1109/JPHOTOV.2015.2405756 ↗
18. The weekend read: bifacial drives PV encapsulant switch
19. Impact of acetic acid exposure on the screen-printed tellurite-based silver contacts
20. Investigation of acetic acid corrosion impact on printed solar cell contacts10.1109/JPHOTOV.2015.2395146 ↗
21. Accelerated damp-heat testing at the cell-level of bifacial silicon HJT, PERC and TOPCon solar cells using sodium chloride10.1016/j.solmat.2023.112554 ↗
22. Assessing the impact of solder flux-induced corrosion on TOPCon solar cells10.1016/j.solmat.2025.113890 ↗
23. The influence of soldering flux on stability of heterojunction and TOPCon solar cells
24. Investigation on effects of the laser-enhanced contact optimization process with Ag paste in a boron emitter for n-TOPCon solar cell
25. Enhancing the reliability of TOPCon technology by laser-enhanced contact firing
26. Laser-enhanced contact optimization on iTOPCon solar cells10.1002/pip.3598 ↗
27. Degradation mechanism of TOPCon solar cells in an ambient acid environment10.1021/acsami.4c21774 ↗
28. An advanced software suite for the processing and analysis of silicon luminescence images10.1016/j.cpc.2017.02.012 ↗
29. Unveiling the origin of metal contact failures in TOPCon solar cells through accelerated damp-heat testing10.1016/j.solmat.2024.113188 ↗
30. Effect of firing temperature on damp heat stability of n-TOPCon solar cells' rear side10.1002/solr.202500299 ↗
31. Detection of finger interruptions in silicon solar cells using line scan photoluminescence imaging10.1109/JPHOTOV.2017.2732220 ↗
32. Mitigating contaminant-induced surface degradation in TOPCon solar cells: mechanisms, impacts, and mitigation10.1016/j.solmat.2025.113558 ↗
33. Vanek
34. ToF-SIMS—An overview
35. Conductive and stable magnesium oxide electron-selective contacts for efficient silicon solar cells10.1002/aenm.201601863 ↗
36. High-performance and stable dopant-free silicon solar cells with magnesium acetylacetonate electron-selective contacts10.1002/pssr.202000103 ↗
37. Changes in hydrogen concentration and defect state density at the poly-Si/SiOx/c-Si interface due to firing10.1016/j.solmat.2021.111297 ↗
38. Hydrogen passivation of poly-Si/SiOx contacts for Si solar cells using Al2O3 studied with deuterium10.1063/1.5031118 ↗
39. Degradation and accelerated recovery of surface passivation in n +, p +, and intrinsic poly ‐Si/SiOx passivating contacts for silicon solar cells10.1002/solr.202500133 ↗
40. Degradation processes and mechanisms of encapsulants
41. Properties and degradation behaviour of polyolefin encapsulants for photovoltaic modules10.1002/pip.3323 ↗
42. Dopant diffusion through ultrathin AlOx and AlOx/SiOx tunnel layer in TOPCon structure and its impact on the passivation quality on c-Si solar cells10.1016/j.solmat.2021.110970 ↗
43. Design rules for high-efficiency both-sides-contacted silicon solar cells with balanced charge carrier transport and recombination losses10.1038/s41560-021-00805-w ↗
44. STEM-EELS investigation of c-Si/a-AlO interface for solar cell applications10.1016/j.micron.2021.103032 ↗
45. Characterization of reaction products and reaction process of MgO–SiO2–H2O system at room temperature10.1016/j.conbuildmat.2014.03.004 ↗
46. Hydration of MgO: reaction kinetics and pH control on brucite crystal morphology10.1021/acs.cgd.4c00243 ↗
47. Stability of SiNx prepared by plasma-enhanced chemical vapor deposition at low temperature10.3390/nano11123363 ↗
48. Moisture-resistant properties of SiNx films prepared by PECVD10.1016/S0040-6090(98)00812-8 ↗
49. Corrosion of silicon nitride materials in aqueous solutions10.1111/jace.12509 ↗
50. MgO nanocube hydroxylation by nanometric water films10.1039/D2NR07140A ↗
51. Control of grain-boundary tunneling barriers in polycrystalline silicon10.1063/1.1509853 ↗
52. Characterization of tunnel barriers in polycrystalline silicon point-contact single-electron transistors10.1143/JJAP.41.2675 ↗
53. Damp-heat degradation and repair of oxide-passivated silicon
54. Hydrogen induced passivation of Si interfaces by Al2O3 films and SiO2/Al2O3 stacks10.1063/1.3497014 ↗
55. Kinetics of H2 passivation of Pb centers at the (111) Si-SiO2 interface10.1103/PhysRevB.38.9657 ↗
56. Migration, incorporation, and passivation reactions of molecular hydrogen at the Si-SiO2 interface10.1103/PhysRevB.70.245320 ↗
57. Understanding the charge transport mechanisms through ultrathin SiOx layers in passivated contacts for high-efficiency silicon solar cells10.1063/1.5081832 ↗
58. Understanding SiOx Layer Breakup in poly-Si/SiOx Passivating Contacts for Si Solar Cells Using Precisely Engineered Surface Textures10.1021/acsaem.1c03676 ↗
59. Detailed study on the role of nature and distribution of pinholes and oxide layer on the performance of tunnel oxide passivated contact (TOPCon) solar cell10.1109/TED.2022.3196327 ↗
60. Charge-carrier dynamics for silicon oxide tunneling junctions mediated by local pinholes
61. Green · 1982