journal article·2024-10

Does Sn2+ play well with Zn2+ as their molten chloride salts react with Cr–Al–B MAB phase?

Xianman Zhang, Qi Hu, Zhenhai Zheng, Wei Wen, Hongfeng Luo

Publisher page

Abstract

Novel Zn-MAX phases like Ti 2ZnC were synthesized in the literature by the reaction between Lewis acid salts like ZnCl 2 and the MAX phase. The interactions between the Cr–Al–B MAB phase contained in the PLS coating formed during HDA of Fe–Cr–B cast steel and five types of molten chloride salts (ZnCl 2 and SnCl 2) were investigated. The results showed that the Cr-(Al, Zn)–B and Cr-(Al, Sn)–B MAB phase solid solution were formed as the PLS coating reacted with the molten ZnCl 2 and SnCl 2, respectively, through topochemical reaction. Zn and Sn could not coexist in the A-site Cr–Al–B MAB phase solid solution, and the replacement ability of Sn 2+ contained in molten salt was much stronger than that of Zn 2+. Zn and Sn whiskers could spontaneously grow on the Cr-(Al, Zn)–B and Cr-(Al, Sn)–B MAB phase solid solution respectively.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Basic properties of eutectic chloride salts NaCl-KCl-ZnCl2 and NaCl-KCl-MgCl2 as HTFs and thermal storage media measured using simultaneous DSC-TGA10.1016/j.solener.2018.01.067 ↗
2. Corrosion behavior of metallic alloys in molten chloride salts for thermal energy storage in concentrated solar power plants: a review10.1007/s11705-018-1720-0 ↗
3. Design and development of novel LiCl-NaCl-KCl-ZnCl2 eutectic chlorides for thermal storage fluids in concentrating solar power (CSP) applications10.1016/j.solmat.2022.111678 ↗
4. 2D and 3D cellular simulation on the corrosion behaviour of Ni-based alloy in ternary molten salt of NaCl-KCl-ZnCl210.1016/j.solmat.2022.111694 ↗
5. Electrochemical study on the hot corrosion behavior of Ni16Cr13Co4Mo alloy in molten NaCl-KCl and NaCl-KCl-Na2SO410.1016/j.corsci.2022.110247 ↗
6. Molten chloride salt technology for next-generation CSP plants: compatibility of Fe-based alloys with purified molten MgCl2-KCl-NaCl salt at 700 °C10.1016/j.apenergy.2022.119708 ↗
7. Temperature-dependent morphological evolution during corrosion of the Ni-20Cr alloy in molten salt revealed by multiscale imaging10.1021/acsami.2c23207 ↗
8. Corrosion behavior and mechanism of 316 stainless steel in NaCl-KCl-ZnCl2 molten salts at high temperature, Mater
9. Processing of MAX phases: from synthesis to applications10.1111/jace.17544 ↗
10. Advances in the synthesis of 2D MXenes10.1002/adma.202103148 ↗
11. Element replacement approach by reaction with Lewis acidic molten salts to synthesize nanolaminated MAX phases and MXenes10.1021/jacs.9b00574 ↗
12. Lewis acid molten salt etched porous lamellar Ti2AlC powders for enhanced microwave absorption10.1016/j.ceramint.2023.12.156 ↗
13. Chemical scissor-mediated structural editing of layered transition metal carbides10.1126/science.add5901 ↗
14. Room-temperature deintercalation and self-extrusion of Ga from Cr2GaN10.1126/science.284.5416.937 ↗
15. Spontaneous growth of metal whiskers on surfaces of solids: a review10.1016/j.jmst.2015.04.001 ↗
16. Mechanisms behind the spontaneous growth of Tin whiskers on the Ti2SnC ceramics10.1016/j.actamat.2019.12.027 ↗
17. Isotope study reveals atomic motion mechanism for the formation of metal whiskers in MAX phase10.1016/j.actamat.2020.11.017 ↗
18. Selective growth of tin whiskers from its alloy on Ti2SnC10.1016/j.jmst.2020.02.081 ↗
19. Interface energy-driven indium whisker growth on ceramic substrates10.1007/s10854-021-06250-5 ↗
20. Indium (In) whisker growth from MAB phase Ti2InB210.1007/s10854-023-10723-0 ↗
21. In-situ growth of ZnO whiskers on Ti2ZnC MAX phases10.3390/ma16103610 ↗
22. Influence of Cr on the interfacial boride reaction between Fe-Cr-B cast steel and molten aluminium10.1016/j.corsci.2019.108098 ↗
23. Influence of thermal diffusion treatment on microstructure evolution and corrosion behavior of hot-dipped Al coated Fe-Cr-Si-B cast steel10.1016/S1003-6326(23)66200-4 ↗
24. Effects of Zn and Si on the microstructure evolution of the Cr-Al-B MAB phase contained in the periodic layered structure formed in-situ10.1016/j.ceramint.2023.08.202 ↗
25. On the effect of thermal diffusion treatment on the hot-dipped Al-Si alloy coating on Fe-Cr-B cast steel10.1016/j.conbuildmat.2023.134631 ↗
26. Hot-dip aluminizing of Fe-Cr-B cast steel in Al-Ti-B alloy melt10.1016/j.jmrt.2024.02.141 ↗
27. Spontaneous growth of Sn whisker on the hot-dipping Al-Sn alloy coating on Fe-Cr-B cast steel10.1016/j.matchar.2024.114116 ↗
28. Reaction between hot-dip aluminized coating on Fe-Cr-B cast steel and molten ZnCl2 salt10.1007/s12666-024-03342-8 ↗
29. Peculiarities of the synthesis of ternary Fe-Al-Sn intermetallic compound from mechanically alloyed materials10.1007/s11661-020-05938-3 ↗
30. Investigating corrosion behavior of Ni and Ni-20Cr in molten ZnCl210.1016/j.corsci.2020.109105 ↗
31. Fe surfaces corroded by molten ZnCl210.1002/maco.201911346 ↗
32. Insights into the dual-roles of alloying elements in the growth of Sn whiskers10.1016/j.jmst.2021.11.043 ↗
33. Atomistic simulation of the diffusion behavior in Al-Fe