Light and elevated temperature induced degradation in gallium-doped silicon: A complete parametric description
Source abstract
Abstract
Despite extensive research on light and elevated temperature induced degradation (LeTID), a complete quantitative description of all relevant subprocesses is still lacking. In particular, the phenomenon of temporary recovery, which opposes the degradation transition, is poorly understood. In this study, we treat gallium-doped Czochralski silicon wafers at varying temperatures and minority charge carrier densities, measuring the resulting changes in effective lifetime. By studying temporary recovery in isolation from degradation and regeneration, we find that the rate of temporary recovery increases as temperature decreases. This is quantified by a negative activation energy of E a BA = − 0.6 eV . This reversed Arrhenius behavior imposes restrictions on the reaction scheme, suggesting that temporary recovery is a multi-step process involving at least two distinct subreactions. The dependence of temporary recovery on the minority charge carrier density was found to follow a power law with an exponent around x BA = 1.9 . For degradation and regeneration, we derive activation energies close to 0.8 eV . This similarity of the temperature dependence is consistent with a recently proposed atomistic model, where both degradation and regeneration occur by atomic hydrogen binding to another complex. In total, we have provided all kinetic parameters required for describing LeTID in gallium-doped silicon with the well-known three-state model. Our findings thereby not only enhance the understanding of the underlying processes involved in LeTID, but also enable the precise modelling of the degradation rate and extent. These results lay the groundwork for complex outdoor yield models that incorporate weather data.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Advancements in Semiconductor Devices and Circuit Design
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Fischer · 2025
2. Philipps · 2024
3. Status and perspectives of crystalline silicon photovoltaics in research and industry10.1038/s41578-022-00423-2 ↗
4. Silicon-based passivating contacts: the TOPCon route10.1002/pip.3522 ↗
5. Antimony-doped Cz silicon wafers: the next generation of n-type wafers for solar cells?
6. Influence of dopant elements on degradation phenomena in B- and Ga-Doped czochralski-grown silicon10.1002/solr.202100147 ↗
7. Light induced degradation of rear passivated mc-Si solar cells
8. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
9. Light-induced lifetime degradation in high-performance multicrystalline silicon: detailed kinetics of the defect activation10.1016/j.solmat.2017.08.007 ↗
10. Kinetics of carrier-induced degradation at elevated temperature in multicrystalline silicon solar cells10.1016/j.solmat.2017.05.066 ↗
11. Temperature dependent degradation and regeneration of differently doped mc-Si materials10.1016/j.egypro.2017.09.085 ↗
12. Lifetime instabilities in gallium doped monocrystalline PERC silicon solar cells10.1016/j.solmat.2019.110299 ↗
13. Investigation on the light and elevated temperature induced degradation of gallium-doped Cz-Si10.1016/j.solener.2021.07.023 ↗
14. Light and elevated temperature induced degradation and recovery of gallium-doped Czochralski-silicon solar cells10.1038/s41598-022-11831-3 ↗
15. Light-induced degradation and regeneration in n-type silicon10.1016/j.egypro.2015.07.090 ↗
16. Long-term carrier lifetime instabilities in n-type FZ- and Cz-silicon under illumination at elevated temperature10.1016/j.solmat.2024.113169 ↗
17. Impact of LeTID in industrial P- and Sb-doped Cz-Si ingots with melt recharging
18. Lifetime degradation and regeneration in multicrystalline silicon under illumination at elevated temperature10.1063/1.4944839 ↗
19. A four-state kinetic model for the carrier-induced degradation in multicrystalline silicon: introducing the reservoir state10.1016/j.solmat.2018.04.024 ↗
20. Recovery of LeTID by low intensity illumination: reaction kinetics, completeness and threshold temperature10.1016/j.egypro.2017.09.090 ↗
21. Review on hydrogen in silicon solar cells: from its origin to its detrimental effects10.1016/j.solmat.2025.113432 ↗
22. Deciphering the role of hydrogen in the degradation of silicon solar cells under light and elevated temperature10.1002/solr.202400457 ↗
23. Impact of hydrogen in Ga-Doped silicon on maximum LeTID defect density10.1002/solr.202300501 ↗
24. LeTID mitigation via an adapted firing process in p-type PERC cells from SMART cast-monocrystalline, czochralski and high-performance multicrystalline silicon10.1002/pip.3467 ↗
25. Impact of substrate thickness on the degradation in multicrystalline silicon10.1109/JPHOTOV.2020.3038412 ↗
26. Impact of the firing temperature profile on light induced degradation of multicrystalline silicon10.1002/pssr.201600272 ↗
27. Process influences on LeTID in Ga-doped silicon10.1016/j.solmat.2023.112451 ↗
28. Evidence of an identical firing-activated carrier-induced defect in monocrystalline and multicrystalline silicon10.1016/j.solmat.2017.08.003 ↗
29. LeTID mitigation via an adapted firing process in p-type PERC cells from gallium-doped czochralski silicon10.1016/j.solmat.2023.112529 ↗
30. Understanding the impact of the cooling ramp of the fast-firing process on light- and elevated-temperature-induced degradation10.1016/j.solmat.2023.112462 ↗
31. Impact of fast-firing conditions on Light- and elevated-temperature-induced degradation (LeTID) in Ga-Doped Cz–Si
32. Possible candidates for impurities in mc-Si wafers responsible for light-induced lifetime degradation and regeneration10.1002/solr.201700159 ↗
33. Evaluating the impact of SiNx thickness on lifetime degradation in silicon10.1109/JPHOTOV.2019.2896671 ↗
34. Impact of hydrogen-rich silicon nitride material properties on light-induced lifetime degradation in multicrystalline silicon10.1002/pssr.201900201 ↗
35. Atomic-layer-deposited Al2O3 as effective barrier against the diffusion of hydrogen from sinx:h layers into crystalline silicon during rapid thermal annealing10.1002/pssr.202000367 ↗
36. Controlling Light- and elevated-temperature-induced degradation with thin film barrier layers10.1109/JPHOTOV.2019.2945199 ↗
37. On the role of AlOx thickness in AlOx/SiNy:H layer stacks regarding Light- and elevated temperature-induced degradation and hydrogen diffusion in c-Si10.1109/JPHOTOV.2021.3075850 ↗
38. Temporary recovery of the defect responsible for Light- and elevated temperature-induced degradation: insights into the physical mechanisms behind LeTID10.1109/JPHOTOV.2020.3025240 ↗
39. 2020
40. Carrier lifetime degradation and regeneration in Gallium- and boron-doped monocrystalline silicon materials10.1109/JPHOTOV.2021.3070474 ↗
41. Why is gallium-doped silicon (sometimes) stable? Kinetics of light and elevated temperature induced degradation10.1016/j.solmat.2024.112986 ↗
42. UV-Induced degradation of industrial PERC, TOPCon, and HJT solar cells: the next big reliability challenge?10.1002/solr.202400628 ↗
43. Stability of industrial gallium-doped czochralski silicon PERC cells and wafers10.1016/j.solmat.2023.112645 ↗
44. Review and recent development in combining photoluminescence-and electroluminescence-imaging with carrier lifetime measurements via modulated photoluminescence at variable temperatures
45. Minority carrier lifetime imaging of silicon wafers calibrated by quasi-steady-state photoluminescence10.1016/j.solmat.2010.12.016 ↗
46. Self-consistent calibration of photoluminescence and photoconductance lifetime measurements10.1063/1.2119411 ↗
47. Minority carrier lifetime in silicon wafers from quasi-steady-state photoluminescence10.1063/1.3485216 ↗
48. Self-sufficient minority carrier lifetime in silicon from quasi-steady-state photoluminescence10.1002/pssa.201228383 ↗
49. Light induced curing (LIC) of passivation layers deposited on native silicon oxide10.1016/j.egypro.2012.07.075 ↗
50. High lifetime Ga-Doped Cz-Si for carrier-selective junction solar cells10.1002/solr.202200613 ↗
51. On the recombination centers of iron-gallium pairs in Ga-doped silicon10.1063/1.5000358 ↗
52. Johnson · 1992 · 4
53. System performance loss due to LeTID10.1016/j.egypro.2017.09.260 ↗
54. LID and LETID evolution of PV modules during outdoor operation and indoor tests10.1051/epjpv/2021009 ↗
55. Light and elevated temperature induced degradation (LeTID) in a utility-scale photovoltaic system10.1109/JPHOTOV.2020.2989168 ↗
56. Long-term impact of light- and elevated temperature-induced degradation on photovoltaic arrays10.1557/s43577-022-00438-8 ↗
57. The rates of chemical reactions
58. Negative activation energy for the Cl(Br)O + NO → Cl(Br) + NO2 reactions10.1021/j150608a019 ↗
59. Negative activation energies and curved arrhenius plots. 1. Theory of reactions over potential well10.1021/j150669a073 ↗
60. Negative activation energies and curved arrhenius plots. 2. OH + CO10.1021/j150669a074 ↗
61. The effectiveness of N2O in depleting stratospheric ozone10.1029/2012GL052143 ↗
62. Why are some reactions slower at higher temperatures?10.1021/ed400086w ↗