Corrosion effects of Na2CO3/NaCl molten salt eutectic on 316L stainless steel under isothermal and cycling conditions

Kaleb Lippiatt, Stuart Bell, Geoffrey Will, Ted Steinberg

Abstract

Using phase-change materials in thermal energy storage systems for concentrating solar thermal plants can significantly reduce the volume of storage media and, therefore, the cost of the system. However, this approach introduces new material compatibility issues between the thermal energy storage material and the containment vessel in the form of corrosion and thermal transients, which are inherent in these systems. Rods and sheet coupons of stainless steel 316L were corroded for up to 768 h in 59.4/40.6 wt% Na2CO3/NaCl eutectic salt under isothermal (650 °C) and cycled conditions (between 600 and 650 °C). The testing methodologies correspond to actual service conditions, as isothermal degradation may not represent material loss under typical solar thermal cycling conditions. Mass losses were calculated via the Dynamic Gravimetric Analysis technique while Scanning Electron Microscopy utilizing Energy Dispersive Spectroscopy was used to analyze the corrosion layers. Isothermal mass loss plateaued at 75 mg/cm2 at 96 h with no further measurable loss after this time, while cycled samples had a fast initial mass loss rate of 60 mg/cm2 in the first 96 h and lost 0.0331 mg/cm2 every hour thereafter. The results indicate that isothermal samples corrode more slowly than the predominant industry cases of thermal cycling. Spalling is responsible for the degradation in both sets; the continual temperature changes in the cycled samples lead to additional stresses, exacerbating the effect.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Phase Change Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Thermal energy storage technologies for concentrated solar power – a review from a materials perspective10.1016/j.renene.2019.10.127 ↗
2. An innovative empirical method for the accurate identification of the eutectic point of binary salts for solar thermal energy storage
3. Techno-economic analysis on the design of sensible and latent heat thermal energy storage systems for concentrated solar power plants10.1016/j.renene.2021.06.069 ↗
4. Review on concentrating solar power plants and new developments in high temperature thermal energy storage technologies10.1016/j.rser.2015.09.026 ↗
5. Experimental verification of theoretically estimated composition and enthalpy of fusion of eutectic salt mixtures10.1016/j.solmat.2017.09.033 ↗
6. Optimized salt selection for solar thermal latent heat energy storage
7. Gomez · 2011
8. High-temperature phase change material (PCM) selection for concentrating solar power tower applications
9. Novel Na2SO4-NaCl-ceramic composites as high temperature phase change materials for solar thermal power plants (Part I)10.1016/j.solmat.2017.12.034 ↗
10. Eutectic Na2CO3–NaCl salt: a new phase change material for high temperature thermal storage10.1016/j.solmat.2016.04.002 ↗
11. Corrosion of stainless steel 316 in eutectic molten salts for thermal energy storage10.1016/j.solener.2018.03.053 ↗
12. Corrosion of steel alloys in eutectic NaCl+Na2CO3 at 700°C and Li2CO3 + K2CO3 + Na2CO3 at 450°C for thermal energy storage10.1016/j.solmat.2017.05.063 ↗
13. Ahmed · 2009
14. High temperature corrosion studies on friction welded low alloy steel and stainless steel in air and molten salt environment at 650 °C10.1016/j.matdes.2011.08.034 ↗
15. Corrosion behavior of 316SS and Ni-based alloys in a ternary NaCl-KCl-MgCl2 molten salt10.1016/j.solener.2018.06.094 ↗
16. Corrosion behaviors of 316 stainless steel and Inconel 625 alloy in chloride molten salts for solar energy storage10.1515/htmp-2020-0077 ↗
17. Hot corrosion behavior of commercial alloys in thermal energy storage material of molten MgCl2/KCl/NaCl under inert atmosphere10.1016/j.solmat.2018.04.025 ↗
18. Corrosion of iron–nickel–chromium alloys in high temperature carbonate salt under argon atmosphere10.1016/j.solmat.2023.112317 ↗
19. Role of headspace environment for phase change carbonates on the corrosion of stainless steel 316L: high temperature thermal storage cycling in concentrated solar power plants10.1016/j.solmat.2022.112170 ↗
20. The corrosion behaviour of stainless steels and Ni-based alloys in nitrate salts under thermal cycling conditions in concentrated solar power plants10.1016/j.solener.2021.12.072 ↗
21. Effect of thermal cycling on the corrosion behaviour of stainless steels and Ni-based alloys in molten salts under air and argon10.1016/j.solener.2022.04.041 ↗
22. Bradshaw · 2001
23. C-276 nickel alloy corrosion in eutectic Na2CO3/NaCl molten salt under isothermal and thermal cycling conditions10.1016/j.solmat.2022.111695 ↗
24. Corrosion resistance of 625 nickel superalloy exposed to isothermal and thermal cycling conditions in a chloride/carbonate salt10.1016/j.solener.2022.11.034 ↗
25. Damage analysis of 601 nickel superalloy in eutectic Na2CO3/NaCl molten salt under isothermal and thermal cycling conditions10.1016/j.solener.2019.09.030 ↗
26. A eutectic salt high temperature phase change material: thermal stability and corrosion of SS316 with respect to thermal cycling10.1016/j.solmat.2017.05.047 ↗
27. Corrosion resistance of alumina forming alloys against molten chlorides for energy production. II: electrochemical impedance spectroscopy under thermal cycling conditions10.1016/j.solmat.2017.03.025 ↗
28. Corrosion evaluation of eutectic chloride molten salt for new generation of CSP plants. Part 1: thermal treatment assessment10.1016/j.est.2019.101125 ↗
29. Investigation on static and dynamic corrosion behaviors of thermal energy transfer and storage system materials by molten salts in concentrating solar power plants10.1002/maco.201810362 ↗
30. Study of corrosion by Dynamic Gravimetric Analysis (DGA) methodology. Influence of chloride content in solar salt10.1016/j.solmat.2016.07.027 ↗
31. 2017
32. An improved technique for molten salt corrosion sample preparation10.1016/j.solmat.2021.111057 ↗
33. Microstructural study of the influence of KCl and HCl on preformed corrosion product layers on stainless steel10.1007/s11085-017-9763-z ↗
34. Comparison of corrosion performance of grade 316 and grade 347H stainless steels in molten nitrate salt10.1063/1.4949258 ↗
35. A comparative study on the high temperature corrosion of TP347H stainless steel, C22 alloy and laser-cladding C22 coating in molten chloride salts10.1016/j.corsci.2014.03.012 ↗
36. Corrosion of iron stainless steels in molten nitrate salt10.1016/j.egypro.2014.03.095 ↗
37. Corrosion mechanism of SS316L exposed to NaCl/Na2CO3 molten salt in air and argon environments10.1016/j.corsci.2021.109966 ↗
38. High-temperature corrosion behaviour of metal alloys in commercial molten salts10.1016/j.solener.2020.03.010 ↗
39. Corrosion behavior of stainless and low-chromium steels and IN625 in molten nitrate salts at 600 °C10.1016/j.solmat.2015.08.011 ↗
40. Molten salt corrosion
41. Solar thermal irradiation cycles and their influence on the corrosion behaviour of stainless steels with molten salt used in concentrated solar power plants10.1016/j.solmat.2022.112141 ↗
42. Effect of dynamic conditions on high-temperature corrosion of ternary carbonate salt for thermal energy storage applications10.1016/j.solmat.2022.111666 ↗