Intergranular corrosion of 316H stainless steel induced by SO42− ions in MgCl2–KCl–NaCl molten salt
Source abstract
Abstract
The application of molten chloride salts in next generation concentrated solar power plants is limited by their corrosiveness to structural materials. This work investigated the influence of SO 4 2− ions on the corrosion of 316H stainless steel (SS) in MgCl 2 –KCl–NaCl (45.4-21.6-33 mol.%) molten salt using static immersion tests and microstructural analysis techniques. The results demonstrate that the presence of SO 4 2− ions can significantly accelerate the intergranular corrosion of 316H SS by driving the dissolution of alloying elements Fe, Cr, and Mn. SO 4 2− ions diffuse into the alloy bulk along the grain boundaries, resulting in the intergranular corrosion attack. The chemcial reaction rate of the metal atoms is directly proportional to the concentration of SO 4 2− ions. The corrosion rate of 316H SS in salt with 1000 ppm SO 4 2− (167 μm/year) was more than 10 times that in without SO 4 2− (13.3 μm/year), increasing linearly with increasing SO 4 2− concentration. Furthermore, MgCl 2 , the composition of the molten chloride salt, is involved in the corrosion reaction with SO 4 2−, through Na 2SO 4 + 3Fe + MgCl 2 MgFe 2O 4 + 2NaCl + FeS (△G 700°C = −337 kJ/mol), leading to the severe dissolution of the Fe matrix element in 316H SS. Based on the corrosion mechanism of SO 4 2− ions in chloride salts, several promising research directions are proposed for future studies.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Thermodynamic and Structural Properties of Metals and Alloys · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Historical development of concentrating solar power technologies to generate clean electricity efficiently - a review10.1016/j.rser.2014.09.008 ↗
2. Mehos · 2017
3. A comprehensive review of state-of-the-art concentrating solar power (CSP) technologies: current status and research trends10.1016/j.rser.2018.04.097 ↗
4. Th-U cycle performance analysis based on molten chloride salt and molten fluoride salt fast reactors10.1007/s41365-020-00790-x ↗
5. Corrosion of alloys in a chloride molten salt (NaCl-LiCl) for solar thermal technologies10.1016/j.solmat.2016.05.052 ↗
6. Corrosion resistance of alumina forming alloys against molten chlorides for energy production. II: electrochemical impedance spectroscopy under thermal cycling conditions10.1016/j.solmat.2017.03.025 ↗
7. Corrosion monitoring and mitigation techniques on advanced thermal energy storage materials for CSP plants10.1016/j.solmat.2018.12.028 ↗
8. Molten chloride salts for next generation concentrated solar power plants: mitigation strategies against corrosion of structural materials10.1016/j.solmat.2018.12.020 ↗
9. Influence of MgCl2 content on corrosion behavior of GH1140 in molten NaCl-MgCl2 as thermal storage medium10.1016/j.solmat.2017.11.014 ↗
10. Materials compatibility for the next generation of Concentrated Solar Power plants10.1016/j.ensm.2018.02.023 ↗
11. Corrosion in the molten fluoride and chloride salts and materials development for nuclear applications10.1016/j.pmatsci.2018.05.003 ↗
12. Hot corrosion of different alloys in chloride and carbonate molten-salt mixtures under argon atmosphere10.1016/j.solener.2019.07.065 ↗
13. Effect of thermal aging on corrosion behavior of type 316H stainless steel in molten chloride salt10.1016/j.corsci.2021.109784 ↗
14. Engineering molten MgCl2-KCl-NaCl salt for high-temperature thermal energy storage: review on salt properties and corrosion control strategies10.1016/j.solmat.2021.111344 ↗
15. Molten chloride salts for next generation CSP plants: electrolytical salt purification for reducing corrosive impurity level10.1016/j.solmat.2019.04.021 ↗
16. Electrochemical measurement of corrosive impurities in molten chlorides for thermal energy storage10.1016/j.est.2017.12.007 ↗
17. Metallic impurities induced corrosion of a Ni-26W-6Cr alloy in molten fluoride salts at 850 oC10.1016/j.corsci.2020.109079 ↗
18. Effects of impurity elements on SiC grain boundary stability and corrosion10.1007/s41365-021-00963-2 ↗
19. Corrosion behavior of carburized 316 stainless steel in molten chloride salts10.1016/j.solener.2021.05.057 ↗
20. Ni-Mo-Cr alloy corrosion in molten NaCl-KCl-MgCl2 salt and vapour10.1016/j.corsci.2020.109183 ↗
21. Vapor pressure and corrosivity of ternary metal-chloride molten-salt based heat transfer fluids for use in concentrating solar power systems10.1016/j.apenergy.2015.08.131 ↗
22. Effect of SO42- on the corrosion of 316L stainless steel in molten FLiNaK salt10.1016/j.corsci.2018.08.057 ↗
23. Non-uniform corrosion of UNS N10003 alloy induced by trace SO42- in molten FLiNaK salt10.1016/j.corsci.2021.109802 ↗
24. Effects of SO42- ions on the corrosion of GH3535 weld joint in FLiNaK molten salt10.1016/j.jnucmat.2017.05.020 ↗
25. Effect of SO42- ion impurity on stress corrosion behavior of Ni-16Mo-7Cr alloy in FLiNaK salt10.1016/j.jnucmat.2021.152809 ↗
26. Corrosion behaviour of 316H stainless steel in molten FLiNaK eutectic salt containing graphite particles10.1016/j.corsci.2019.108174 ↗
27. Effects of alloying elements on the corrosion behavior of Ni-based alloys in molten NaCl-KCl-MgCl2 salt at different temperatures10.1016/j.corsci.2018.08.021 ↗
28. Assessment of effects of Mg treatment on corrosivity of molten NaCl-KCl-MgCl2 salt with Raman and Infrared spectra
29. Corrosion behavior of Ni-based alloys in molten NaCl-CaCl2 -MgCl2 eutectic salt for concentrating solar power10.1016/j.solmat.2017.05.050 ↗
30. Materials corrosion in molten LiF-NaF-KF salt10.1016/j.jfluchem.2008.05.008 ↗
31. Corrosion behavior of 316SS and Ni-based alloys in a ternary NaCl-KCl-MgCl2 molten salt10.1016/j.solener.2018.06.094 ↗
32. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400-700°C10.1016/S0010-938X(99)00142-0 ↗
33. High temperature corrosion mechanisms and effect of alloying elements for materials used in waste incineration environment10.1016/S0010-938X(01)00058-0 ↗
34. Early-stage corrosion of IN 740H alloy in eutectic NaCl-KCl molten salt at high temperatures10.1016/j.solener.2023.02.010 ↗
35. Corrosion mechanisms of ferritic-martensitic P91 steel and Inconel 600 nickel-based alloy in molten chlorides. Part II: NaCl-KCl-MgCl2 ternary system10.1016/j.solmat.2020.110675 ↗
36. Excellent high temperature corrosion resistance of 304 stainless steel immersed in purified NaCl-MgCl2 eutectic salts10.1016/j.matchemphys.2022.127216 ↗
37. Influence of inclusions on early corrosion development of Ultra-Low carbon bainitic steel in NaCl solution10.5006/1837 ↗
38. Effects of sulfur addition on pitting corrosion and machinability behavior of super duplex stainless steel containing rare earth metals: Part 210.1016/j.corsci.2010.07.002 ↗