journal article·2024-07Open access

Multi-principal element alloys for concentrating solar power based on molten salt

R. Carbajales, C. Sobrino, P. Alvaredo

Abstract

Multi-principal element alloys (MPEAs) are characterized by good stability at elevated temperatures, positioning them as a promising alloy family for applications in extreme environments. In particular, their suitability for use in concentrating solar-thermal power (CSP) technology, where exposure to harsh conditions is prevalent, is highly attractive. In this study, the potential of employing MPEAs in components subjected to different environments, including solar salt (composed of 40%KNO3 and 60%NaNO3) at 560 °C, an air atmosphere at 780 °C, and a chloride mixture (46%MgCl2/ 39%KCl/ 15%NaCl) at the same temperature, is investigated. The investigated materials encompass an original Co-free composition, AlCrFeMoNiTi, and a eutectic composition, AlCoCrFeNi. MPEAs were obtained by arc melting, and their corrosion behavior and stability in the specified environments were thoroughly examined.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Material Properties and Applications · Pigment Synthesis and Properties · Material Science and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (88)

Show source-provided references
1. Life cycle assessment (LCA) of a concentrating solar power (CSP) plant in tower configuration with different storage capacity in molten salts10.1016/j.est.2022.105219 ↗
2. Viswanathan · 2022
3. Innovative working fluids for parabolic trough collectors
4. State of the art on high temperature thermal energy storage for power generation. Part 1-Concepts, materials and modellization10.1016/j.rser.2009.07.035 ↗
5. Modeling the total ternary phase diagram of NaNO3–KNO3–NaNO2 using the binary subsystems data10.1007/s10765-019-2577-2 ↗
6. Concentrating solar power at higher limits: first studies on molten nitrate salts at 600 °C in a 100 kg-scale hot tank10.1016/j.solmat.2023.112412 ↗
7. Progress in research and development of molten chloride salt technology for next generation concentrated solar power plants10.1016/j.eng.2020.06.027 ↗
8. Effect of nanoparticle dispersion on specific heat capacity of a binary nitrate salt eutectic for concentrated solar power applications10.1016/j.ijthermalsci.2013.02.003 ↗
9. Purification strategy and effect of impurities on corrosivity of dehydrated carnallite for thermal solar applications10.1039/C9RA09352D ↗
10. Corrosion of 304 stainless, inconel 625, and Haynes 230 in a chloride salt-based thermal storage medium10.1007/s11665-019-04508-y ↗
11. Mainstreaming commercial CSP systems: a technology review10.1016/j.renene.2019.03.049 ↗
12. Bradshaw
13. Corrosion behavior of stainless and low-chromium steels and IN625 in molten nitrate salts at 600 °c10.1016/j.solmat.2015.08.011 ↗
14. Corrosion behaviors of 316 stainless steel and Inconel 625 alloy in chloride molten salts for solar energy storage10.1515/htmp-2020-0077 ↗
15. Corrosion of stainless steel 316 in eutectic molten salts for thermal energy storage10.1016/j.solener.2018.03.053 ↗
16. Corrosion of stainless steels and low-Cr steel in molten Ca(NO3)2-NaNO3-KNO3 eutectic salt for direct energy storage in CSP plants10.1016/j.solmat.2015.05.004 ↗
17. High-temperature corrosion performance of austenitic stainless steels type AISI 316L and AISI 321H, in molten Solar Salt10.1016/j.solener.2018.11.019 ↗
18. Perspectives on selected alloys in contact with eutectic melts for thermal storage: nitrates, carbonates and chlorides10.1016/j.solener.2021.06.069 ↗
19. Effect of temperature and impurity content to control corrosion of 316 stainless steel in molten KCl-MgCl2 salt
20. High temperature corrosion in molten solar salt: the role of chloride impurities10.1002/maco.201609300 ↗
21. 316L stainless steel corrosion in molten salts NaNO3 KNO3 NaNO2 simulating storage conditions
22. The corrosion behaviour of stainless steels and Ni-based alloys in nitrate salts under thermal cycling conditions in concentrated solar power plants10.1016/j.solener.2021.12.072 ↗
23. Dynamic corrosion testing of metals in solar salt for concentrated solar power10.1016/j.solmat.2021.111331 ↗
24. Kruizenga · 2013
25. Corrosion of iron stainless steels in molten nitrate salt10.1016/j.egypro.2014.03.095 ↗
26. Corrosion of stainless steels and carbon steel by molten mixtures of commercial nitrate salts10.1361/10599490417542 ↗
27. Bradshaw · 2001
28. Corrosion resistance of alumina forming alloys against molten chlorides for energy production. II: electrochemical impedance spectroscopy under thermal cycling conditions10.1016/j.solmat.2017.03.025 ↗
29. Corrosion resistance of alumina-forming alloys against molten chlorides for energy production. I: pre-oxidation treatment and isothermal corrosion tests10.1016/j.solmat.2017.02.019 ↗
30. Corrosion of alumina-forming austenitic steel in molten nitrate salts by gravimetric analysis and impedance spectroscopy10.1002/maco.201307422 ↗
31. Evaluation of corrosion resistance of A516 Steel in a molten nitrate salt mixture using a pilot plant facility for application in CSP plants10.1016/j.solmat.2016.12.002 ↗
32. Molten salt corrosion of stainless steels and low-Cr steel in CSP plants10.1007/s11085-012-9310-x ↗
33. Corrosion behavior of a dual-phase FeNiCrCuAl high entropy alloy in supercritical water10.1016/j.corsci.2022.110617 ↗
34. Critical Assessment: critical Assessment 14: high entropy alloys and their development as structural materials10.1179/1743284714Y.0000000749 ↗
35. A review on High-Temperature Applicability: a milestone for high entropy alloys
36. Microstructure and corrosion properties of CrMnFeCoNi high entropy alloy coating10.1016/j.apsusc.2016.11.176 ↗
37. Molten salt corrosion behavior of dual-phase high entropy alloy for concentrating solar power systems10.3390/e25020296 ↗
38. Gao · 2016
39. Phase Stability in High Entropy Alloys: Formation of Solid-Solution Phase or Amorphous Phase10.1016/S1002-0071(12)60080-X ↗
40. Effect of aluminum on the microstructure and properties of two refractory high-entropy alloys10.1016/j.actamat.2014.01.029 ↗
41. Effect of Mo on high-temperature strength of refractory complex concentrated alloys: a perspective of electronegativity difference10.1016/j.jallcom.2022.164186 ↗
42. Effect of molybdenum additives on corrosion behavior of (CoCrFeNi)100-xMox high-entropy alloys10.3390/e20120908 ↗
43. Effect of molybdenum content on the microstructure and corrosion behavior of FeCoCrNiMox high-entropy alloys10.1016/j.jmst.2019.10.020 ↗
44. Microstructural characterization of eutectic and near-eutectic AlCoCrFeNi high-entropy alloys10.1016/j.jallcom.2019.153558 ↗
45. Y-doped AlCoCrFeNi2.1 eutectic high-entropy alloy with excellent oxidation resistance and structure stability at 1000°C and 1100°C10.1016/j.corsci.2020.109191 ↗
46. Rapid solidification of AlCoCrFeNi2.1 high-entropy alloy10.1016/j.jallcom.2021.163350 ↗
47. Effects of nickel content on the microstructure, microhardness and corrosion behavior of high-entropy AlCoCrFeNix alloys10.1038/s41598-020-78108-5 ↗
48. Understanding the links between the composition-processing-properties in new formulations of heas sintered by sps10.3390/met11060888 ↗
49. Microstructural origins of high strength and high ductility in an AlCoCrFeNi2.1 eutectic high-entropy alloy10.1016/j.actamat.2017.07.041 ↗
50. Processing of a new high entropy alloy: AlCrFeMoNiTi10.1080/00325899.2018.1457862 ↗
51. Turchi
52. Corrosion and electrochemical investigations for stainless steels in molten Solar Salt: the influence of chloride impurity10.1016/j.est.2021.102675 ↗
53. Study of corrosion by Dynamic Gravimetric Analysis (DGA) methodology. Influence of chloride content in solar salt10.1016/j.solmat.2016.07.027 ↗
54. Corrosion monitoring of 321H in contact with a quaternary molten salt for parabolic trough CSP plants10.1016/j.corsci.2020.109070 ↗
55. Corrosion behavior of vm12-shc steel in contact with solar salt and ternary molten salt in accelerated fluid conditions10.3390/en14185903 ↗
56. High-temperature stability of nitrate/nitrite molten salt mixtures under different atmospheres10.1016/j.apenergy.2018.05.101 ↗
57. Talekar
58. Correlations between growth kinetics and microstructure for scales formed by high-temperature oxidation of pure nickel. II. Growth kinetics10.1023/A:1020102604090 ↗
59. Oxidation behavior of an austenitic steel (Fe, Cr and Ni), the 310 h, in a deaerated supercritical water static system10.3390/met11040571 ↗
60. High-strength and high-ductility AlCoCrFeNi2.1 eutectic high-entropy alloy achieved via precipitation strengthening in a heterogeneous structure10.1016/j.scriptamat.2020.04.035 ↗
61. Solidification microstructure of AlCoCrFeNi2.1 eutectic high entropy alloy ingots10.2320/matertrans.F-M2017851 ↗
62. Evolution of microstructure and mechanical properties during annealing of heavily rolled AlCoCrFeNi2.1 eutectic high-entropy alloy10.1016/j.msea.2021.142558 ↗
63. Quantification of microstructure in a eutectic high entropy alloy AlCoCrFeNi2.1
64. Screening tests of sodium nitrate and potassium nitrate decomposition10.1016/0038-092X(82)90082-2 ↗
65. Isothermal and cyclic oxidation of MoAlB in air from 1100°C to 1400°C10.1149/2.1891713jes ↗
66. Oxidation of metals
67. Us · 2016
68. High temperature oxidation resistance of electrodeposited Reduced Graphene Oxide (RGO) reinforced copper coating10.1016/j.surfcoat.2018.04.025 ↗
69. Long-term oxidation behaviour and thermal stability of heat-resistant stainless steel claddings deposited on AISI 316 stainless steel by the GTAW process10.1016/j.surfcoat.2021.127605 ↗
70. Kruizenga · 2013
71. Dissolution susceptibility of the oxide species formed on mild steel during its oxidation in molten NaNO3-KNO3 eutectic mixture10.1361/105994902770344114 ↗
72. Surface degradation mechanisms in a eutectic high entropy alloy at microstructural length-scales and correlation with phase-specific work function10.1038/s41529-019-0079-0 ↗
73. Corrosion behavior of high entropy alloys and their application in the nuclear industry—an overview
74. Corrosion behavior of the AlCoCrFeNi2.1 eutectic high-entropy alloy in chloride-containing sulfuric acid solutions at different temperatures
75. Corrosion behavior of AlCoCrFeNi2.1 eutectic high-entropy alloy in Cl--containing solution10.1016/j.jallcom.2022.168609 ↗
76. Effect of molybdenum on the corrosion of low alloy steels in synthetic seawater10.2320/matertrans.M2016222 ↗
77. Molybdenum effects on the stability of passive films unraveled at the nanometer and atomic scales10.1038/s41529-023-00418-6 ↗
78. Sodium molybdate as a corrosion inhibitor for aluminium in H3PO4 solution10.1016/j.corsci.2011.05.002 ↗
79. Molten Sodium Nitrite-potassium Nitrite Eutectic: the Reactions of Some Compounds of Chromium10.1016/S0020-1693(00)92574-X ↗
80. Oxidation behavior of 316L austenitic stainless steel in high temperature air with long-term exposure10.1088/2053-1591/ab96fa ↗
81. Influence of water vapor and flow rate on the high-temperature oxidation of 304L; Effect of chromium oxide hydroxide evaporation10.1023/A:1004642310974 ↗
82. Oxidation behavior of austenitic stainless steel 316L and 310S in air and supercritical water10.1115/1.4031817 ↗
83. Oxidation behavior of 316L austenitic stainless steel in high temperature air with long-term exposure10.1088/2053-1591/ab96fa ↗
84. J. Stella, A. Sánchez, A. Ruiz, Morfologías de Oxidación a altas temperaturas de una Superaleación sinterizada ni-Al-Cr, Revista Latinoamericana de Metalurgia y Materiales 28 (2008) 18–28. http://ve.scielo.org/scielo.php?script=sci_arttext&pid=S0255-69522008000100003&lng=es&nrm=iso&tlng=es (accessed July 6, 2023).
85. High temperature corrosion in SOFC environments10.1016/0167-2738(92)90092-4 ↗
86. Corrosion in molten salts
87. Corrosion and passive behavior of AlxCrFeNi3−x (x = 0.6, 0.8, 1.0) eutectic high entropy alloys in chloride environment10.1016/j.corsci.2022.110666 ↗
88. Corrosion properties of AlxCoCrFeNiTi0·5 high entropy alloys in 0·5M H2SO4 aqueous solution10.1179/1432891714Z.000000000778 ↗