On the compatibility of liquid sodium as heat transfer fluid for advanced concentrated solar thermal energy systems
Source abstract
Abstract
The use of liquid sodium as a heat transfer fluid has shown great promise and application in nuclear power generation and it is now being utilized in concentrated solar thermal power (CSP) applications, owing to its favorable thermodynamic properties. Its implementation, however, comes with a unique array of technical issues in CSP applications, primarily the incompatibility of structural materials with liquid sodium in these operational environments. In this review, major damage mechanisms will be discussed, with a focus on their relevance to advanced CSP plants. Such mechanisms include corrosion, liquid metal embrittlement, carburization/de-carburization, erosion, creep, and thermal fatigue. The degradation factors such as impurities in the sodium (e.g. oxygen) and the dissolution of the structural material's alloying elements (Cr, Mn, Ni and Si, etc.) are also discussed. This review presents a holistic overview of these inter-connected mechanisms, and most importantly explores potential solutions to mitigate these issues, including better structural material candidates, robust plant operational parameters/design, better service life predictions, and improved purification and monitoring methods for stringent control of impurities. The future directions of research are also discussed to ensure the successful use of liquid sodium in the next generation of CSP technology.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Solar Thermal and Photovoltaic Systems · Nuclear reactor physics and engineering · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Sodium-cooled fast reactor
2. Materials compatibility for the next generation of Concentrated Solar Power plants10.1016/j.ensm.2018.02.023 ↗
3. A review of sodium receiver technologies for central receiver solar power plants10.1016/j.solener.2015.09.023 ↗
4. Critical components in supercritical CO2 Brayton cycle power blocks for solar power systems: degradation mechanisms and failure consequences
5. Liquid metals as efficient high-temperature heat-transport fluids10.1002/ente.201600721 ↗
6. Assessment of liquid metal technology status and research paths for their use as efficient heat transfer fluids in solar central receiver systems10.1016/j.solener.2013.03.025 ↗
7. Heat transfer fluids for concentrating solar power systems – a review10.1016/j.apenergy.2015.01.125 ↗
8. Liquid sodium versus Hitec as a heat transfer fluid in solar thermal central receiver systems10.1016/j.solener.2012.05.001 ↗
9. 10 - liquid metal corrosion in nuclear reactor and accelerator driven systems
10. Advances in central receivers for concentrating solar applications10.1016/j.solener.2017.03.048 ↗
11. Thermoelastic stress in concentrating solar receiver tubes: a retrospect on stress analysis methodology, and comparison of salt and sodium10.1016/j.solener.2017.12.003 ↗
12. 2020
13. Turchi · 2021
14. Improving cavitation erosion resistance of austenitic stainless steel in liquid sodium by hard facing – comparison of Ni and Co based deposits10.1016/j.wear.2015.08.009 ↗
15. The liquid metal embrittlement of 9Cr steel in sodium environments and the role of non-metallic impurities10.1016/0010-938X(94)90066-3 ↗
16. The liquid metal embrittlement of iron and ferritic steels in sodium10.1016/0010-938X(95)92861-E ↗
17. Liquid metal embrittlement of an austenitic stainless steel in liquid sodium10.1016/j.corsci.2014.02.031 ↗
18. Wetting by liquid sodium and fracture path analysis of sodium induced embrittlement of 304L stainless steel10.1557/jmr.2017.435 ↗
19. Corrosion of austenitic stainless steel in liquid sodium
20. FY 2017-progress report on the design and construction of the sodium loop SMT-3
21. Further insights into the mechanisms involved in the corrosion of 316L(N) austenitic steel in oxygenated liquid sodium at 550 °C
22. Mechanism of corrosion of 9Cr and 12Cr ferritic/martensitic steels under oxygen-saturated sodium10.1016/j.corsci.2016.09.001 ↗
23. Wastage and self-plugging by a potential CO2 ingress in a supercritical CO2 power conversion system of an SFR10.1080/18811248.2010.9711667 ↗
24. Potential sodium–CO2 interaction of a supercritical CO2 power conversion option coupled with an SFR: basic nature and design issues10.1016/j.nucengdes.2013.01.002 ↗
25. Na-CO2 interactions experiment (SNAKE). FY 2012 update on facility assembly and sodium loading
26. FY 2014 sodium-supercritical CO2 interactions in the SNAKE experiment facility
27. Gerardi · 2017
28. Bremer · 2018
29. Description of the first observed sodium-CO2 reactions in the sodium CO2 interaction experiment (SNAKE)
30. The interaction of elemental sodium with molten NaNO3-KNO3 at 873 K10.1007/BF02834139 ↗
31. Sodium for fast breeders — production, purification, and quality
32. A new process for the removal of impurities in the cold traps of Liquid Metal Fast Reactors
33. The various sodium purification techniques
34. Sodium coolant purification systems for a nuclear power station equipped with a BN-1200 reactor10.1134/S0040601513050017 ↗
35. Experimental techniques for the purification of sodium
36. Purification of liquid metal systems with sodium coolant from oxygen using getters10.1134/S0040601516050049 ↗
37. Bonin · 2016
38. Liquid metal in-line impurity measuring instruments (sodium) state-of-the-art study
39. Sodium-NaK engineering handbook. Volume III. Sodium systems, safety, handling, and instrumentation.[LMFBR]
40. 2012
41. Experimental investigation of an automatic plugging meter for measuring impurities in sodium
42. Method for determination of less than 5 ppm oxygen in sodium samples
43. Reaction of inconel with oxygen-containing sodium10.1016/0022-3115(71)90055-9 ↗
44. Corrosion resistance of ion-plated molybdenum thin-coating on austenitic steel in a flowing sodium environment10.1016/0022-3115(87)90276-5 ↗
45. The downstream effect in the corrosion of metallic materials in a type 316 stainless steel sodium loop system10.1016/0022-3115(86)90196-0 ↗
46. Sodium corrosion behavior of austenitic alloys and selective dissolution of chromium and nickel10.1016/0022-3115(86)90027-9 ↗
47. Characterization of the sodium corrosion behavior of commercial austenitic steels
48. Occurrence and prediction of sigma phase in fuel cladding alloys for breeder reactors10.1016/0022-3115(84)90544-0 ↗
49. Sodium compatibility of ODS steel at elevated temperature10.1016/j.jnucmat.2004.04.312 ↗
50. Effects of nitrogen on corrosion of stainless steels in a liquid sodium environment10.1016/0022-3115(90)90373-U ↗
51. Corrosion behavior and tensile properties of AISI 316LN stainless steel exposed to flowing sodium at 823 K10.1361/105994900770346349 ↗
52. Carburization behavior of AISI 316LN austenitic stainless steel – experimental studies and modeling10.1016/j.jnucmat.2010.05.023 ↗
53. The corrosion of chromium, iron, and stainless steel in liquid sodium10.1016/0022-5088(74)90243-4 ↗
54. Evaluation procedures for irradiation effects and sodium environmental effects for the structural design of Japanese fast breeder reactors10.1115/1.1338119 ↗
55. Effect of flowing sodium on corrosion and tensile properties of AISI type 316LN stainless steel at 823K10.1016/j.jnucmat.2008.01.032 ↗
56. Corrosion behavior and microstructural evolution of ASTM A182 Grade 92 steel in liquid sodium at 650°C10.1016/j.corsci.2015.05.004 ↗
57. Corrosion behavior of surface treated steel in liquid sodium negative electrode of liquid metal battery10.1016/j.jpowsour.2016.01.019 ↗
58. Alkali metal coolants
59. Compatibility of high-purity Fe-(5 to 15)Cr-1Mo ferritic steels in a sodium environment10.1016/0022-3115(87)90496-X ↗
60. Thermal fatigue crack networks parameters and stability: an experimental study10.1016/j.ijsolstr.2004.06.032 ↗
61. Effect of sodium environment on the creep-rupture and low-cycle fatigue behavior of austenitic stainless steels
62. The in-sodium creep behavior of alloys M-813 and Nimonic PE16
63. Influence of sodium environment and load ratio (R) on fatigue crack growth behaviour of a Type 316 LN stainless steel at 813 K10.1016/S0308-0161(96)00049-X ↗
64. A comparison of creep deformation and rupture behaviour of 316L(N) austenitic stainless steel in flowing sodium and in air10.1016/j.proeng.2013.03.338 ↗
65. Influence of liquid sodium on mechanical properties of steels, refractory alloys and ceramics
66. Sodium compatibility of ceramics
67. SiCf/SiC composites as core materials for Generation IV nuclear reactors
68. Stability of ternary oxygen compounds of molybdenum in liquid sodium10.1016/0022-3115(87)90068-7 ↗
69. Macroscopic investigation into the interaction of liquid sodium and a molten carbonate
70. Na-CO2 interactions experiment (SNAKE). FY 2012 update on facility assembly and sodium loading
71. Description of the first observed sodium-CO2 reactions in the sodium CO2 interaction experiment (SNAKE)
72. Corrosion and deposition of steels and nickel-base alloys in liquid sodium
73. Sodium effects on mechanical performance and consideration in high temperature structural design for advanced reactors10.1016/j.jnucmat.2009.03.039 ↗
74. Section II: materials - Part D: properties (customary)
75. Section I: rules for construction of power boilers
76. Section VIII, division 1: rules for construction of pressure vessels
77. 2005
78. Sensitization evaluation of the austenitic stainless steel AISI 304L, 316L, 321 and 34710.1007/s10853-005-5699-9 ↗
79. 2016
80. The potential role of concentrating solar power within the context of DOE's 2030 solar cost targets
81. Concentrated solar power plants: review and design methodology10.1016/j.rser.2013.01.032 ↗
82. Solar power technologies for sustainable electricity generation–A review10.1016/j.rser.2015.10.135 ↗
83. Concentrated solar power (CSP)
84. 2019
85. gov · 2020
86. Research performance progress report Part 1 (RPPR-1)
87. Gen3 CSP: U.S. And Australian cooperative research on 700°C heat transfer systems
88. Materials corrosion for thermal energy storage systems in concentrated solar power plants10.1016/j.rser.2018.01.010 ↗
89. Mainstreaming commercial CSP systems: a technology review10.1016/j.renene.2019.03.049 ↗
90. A review of concentrating solar power plants in the world and their potential use in Serbia10.1016/j.rser.2012.03.042 ↗
91. Modeling and hourly time-scale characterization of the main energy parameters of parabolic-trough solar thermal power plants using a simplified quasi-dynamic model10.3390/en14010221 ↗
92. Inspection and structural health monitoring techniques for concentrated solar power plants10.1016/j.renene.2015.07.090 ↗
93. Archimede solar energy molten salt parabolic trough demo plant: a step ahead towards the new frontiers of CSP10.1016/j.egypro.2015.03.122 ↗
94. Study of China's optimal concentrated solar power development path to 205010.3389/fenrg.2021.724021 ↗
95. Materials for ultrasupercritical coal power plants - boiler materials: Part 110.1361/105994901770345394 ↗
96. AS 1210—2010
97. Oxidation of 316L(N) stainless steel in liquid sodium at 650 °C10.1016/j.jnucmat.2017.12.037 ↗
98. IUPAC-NIST solubility data series. 75. Nonmetals in liquid alkali metals10.1063/1.1391426 ↗
99. Daintith · 2008
100. Smith · 1972