journal article·2024-03

High-temperature dynamic corrosion mechanisms of austenitic stainless and carbon steels in nitrates for concentrating solar power

Pu Yang, Zhongyue Deng, Bingqing Chen, Yueshe Wang

Publisher page

Abstract

Abstract: In this paper, to simulate the dynamic corrosion mechanisms of metals exposed to a high-temperature molten salt mixture of NaNO 3–KNO 3 , the experimental samples made of commonly used stainless steel alloys such as 304 (with/without welds) and Q275 were suspended, along with stirring blades, in a specially designed stirred kettle to obtain their corrosion characteristics. For the experimental samples, the Q275 surface exhibited significant quantities of Fe 3O 4 and Fe 2O 3, while 304 generated FeCr 2O 4, Cr 2O 3, and MgFe 2O 4 with protective effects. The microstructure of the welding zone in 304 exhibited considerable disparities compared to that of the base material, consequently leading to augmented susceptibility towards localized corrosion. The uneven distribution of chromium in the welding zone resulted in intergranular corrosion and alterations in the crystal structure. Moreover, experimental studies have demonstrated that NO 3 - in the molten salt undergoes decomposition to generate oxygen ions, which contribute to the corrosion reaction. Notably, under all test conditions, the corrosion rate of samples exhibited the following ranking: 304 (without welds) < 304 (with welds) < Q275.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Phase Change Materials Research · Thermography and Photoacoustic Techniques · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Corrosion behavior of stainless and low-chromium steels and IN625 in molten nitrate salts at 600 °C10.1016/j.solmat.2015.08.011 ↗
2. Corrosion performance of Ni-based structural alloys for applications in molten-salt based energy systems: experiment & numerical validation10.1016/j.corsci.2021.109607 ↗
3. Corrosion behavior of nitrogen-containing low-nickel weld Cladding in KCl-MgCl2 eutectic molten salt at 900 °C10.3390/ma15248831 ↗
4. State of the art on high temperature thermal energy storage for power generation. Part 1—concepts, materials and modellization10.1016/j.rser.2009.07.035 ↗
5. Are unexpected chloride ions in molten salt really harmful to stainless steel?10.1016/j.est.2022.105317 ↗
6. Engineering aspects of a molten salt heat transfer fluid in a trough solar field10.1016/S0360-5442(03)00191-9 ↗
7. Influence of MgCl2 content on corrosion behavior of GH1140 in molten NaCl-MgCl2 as thermal storage medium10.1016/j.solmat.2017.11.014 ↗
8. Advanced heat transfer fluids for direct molten salt line-focusing CSP plants10.1016/j.pecs.2018.02.002 ↗
9. The effect of laser surface melting of stainless steel grade AISI 316L welded joint on its corrosion performance in molten Solar Salt
10. Corrosion in molten nitrate-nitrite salts10.1007/BF03259692 ↗
11. Corrosion properties of a ternary nitrate/nitrite molten salt in concentrated solar technology10.1016/j.renene.2015.01.072 ↗
12. Thermal influence in corrosion properties of Chilean solar nitrates10.1016/j.solener.2014.07.027 ↗
13. Corrosion performance of alloy 800H and alloy 625 for potential use as molten salts solar receiver materials in concentrating solar power tower plants10.1016/j.est.2022.105824 ↗
14. Lessons learned from corrosion of materials with molten salts during molten salt tank preheating
15. Corrosion of iron–nickel–chromium alloys in high temperature carbonate salt under argon atmosphere
16. Corrosion resistance of iron-chromium-aluminium steel in eutectic molten salts under thermal cycling conditions10.1016/j.corsci.2020.108798 ↗
17. Experimental research of high temperature dynamic corrosion characteristic of stainless steels in nitrate eutectic molten salt10.1016/j.solener.2020.09.034 ↗
18. Evaluation of corrosion resistance of A516 Steel in a molten nitrate salt mixture using a pilot plant facility for application in CSP plants10.1016/j.solmat.2016.12.002 ↗
19. Dynamic corrosion behavior of 316L stainless steel in quaternary nitrate-nitrite salts under different flow rates
20. Effect of flow rate and SiO2 nanoparticle on dynamic corrosion behavior of stainless steels in molten salt for thermal energy storage10.1016/j.corsci.2021.109952 ↗
21. Investigation on static and dynamic corrosion behaviors of thermal energy transfer and storage system materials by molten salts in concentrating solar power plants10.1002/maco.201810362 ↗
22. Effect of dynamic conditions on high-temperature corrosion of ternary carbonate salt for thermal energy storage applications
23. Laser-texturing of stainless steel as a corrosion mitigation strategy for high-temperature molten salts applications under dynamic conditions
24. Evaluation of flow accelerated corrosion and mechanical performance of martensitic steel T91 for a ternary mixture of molten salts for CSP plants
25. Dynamic corrosion testing of metals in solar salt for concentrated solar power
26. Comparative review of different influence factors on molten salt corrosion characteristics for thermal energy storage
27. Corrosion behavior and mechanism of austenitic stainless steels in a new quaternary molten salt for concentrating solar power10.1016/j.solmat.2019.01.024 ↗
28. Nitrate on localized corrosion of carbon steel and stainless steel in aqueous solutions10.1016/j.electacta.2020.137660 ↗
29. Corrosion of mild steel in molten sodium nitrate–potassium nitrate eutectic10.1179/bcj.1976.11.1.44 ↗
30. Corrosion and electrochemical investigations for stainless steels in molten Solar Salt: the influence of chloride impurity10.1016/j.est.2021.102675 ↗
31. High temperature corrosion studies on friction welded low alloy steel and stainless steel in air and molten salt environment at 650°C10.1016/j.matdes.2011.08.034 ↗
32. Hot corrosion of Inconel 625 wrought alloy and weld overlay on carbon steel by gas metal arc welding in 47 PbSO4-23 ZnO-13 Pb3O4-7 PbCl2-5 CdO-5 Fe2O3 molten salt mixture10.1016/j.corsci.2021.109348 ↗
33. Effect of laser surface melting on intergranular corrosion behaviour of aged austenitic and duplex stainless steels10.1016/j.corsci.2011.01.048 ↗
34. High-temperature corrosion behavior of austenitic stainless steel in quaternary nitrate molten salt nanofluids for concentrated solar power
35. High-temperature stability of nitrate/nitrite molten salt mixtures under different atmospheres10.1016/j.apenergy.2018.05.101 ↗
36. Microkinetics of the reactionNO3-⇌NO2-+0.5 O2in molten sodium nitrate and potassium nitrate salt
37. Synergistic effect of Cl− and F− on the corrosion behavior and mechanism of 316 stainless steel in NaNO3-based molten salts and vapor10.1016/j.est.2023.107243 ↗