Assessing the stability of p+ and n+ polysilicon passivating contacts with various capping layers on p-type wafers
Source abstract
Abstract
Polysilicon (poly-Si)-on-oxide passivating contact structures (POLO/TOPCon) enable high-efficiency solar cells as they simultaneously provide a very high level of surface passivation and a high conductance for either electrons or holes. The ease of incorporation with existing manufacturing lines and their tolerance for high-temperature processing has increased the wide acceptance of this structure in the PV industry. In this report, we explore the effects of short high-temperature annealing required for effective hydrogenation and formation of ohmic screen-printed contacts across a wide temperature range (636 °C–846 °C) on the stability of passivating contact structures. We study this on p-type c-Si substrates with phosphorus-doped (n-type) or boron-doped (p-type) polysilicon contacts capped with either an AlOx or SiNx coating. Our experimental results show that irrespective of the poly-Si doping type, AlOx-capped samples suffer a loss in surface passivation across the investigated temperature range, while SiNx-capped samples show an improvement at lower annealing temperatures. Above 744 °C, severely ruptured blisters occur for the samples coated with a SiNx layer, leading to lift-off of the poly layer in extreme cases, and in all cases, significant surface passivation losses, up to 99%. A study of the long-term stability of these fired samples under 1-sun illumination @ 140 °C shows that they suffer from both bulk and surface-like instabilities. Two degradation cycles were observed: the first, a boron-oxygen light-induced degradation (BO-LID) observed after 5 min, with capture cross-section ratios of 15.8–19.2, and a slower secondary degradation, similar to light and elevated temperature-induced degradation (LeTID), with maximum degradation reached after ∼ 14 days. The presence of a silicon nitride layer does not appear to influence the kinetics of post-degradation recovery. Our results suggest that the effect of firing may be influenced by the polarity of the bulk c-Si or perhaps the chemistry of the SiNx film and highlight that passivating contact structures based on p-type c-Si may offer better long-term stability than those based on n-type c-Si.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. International Technology Roadmap for Photovoltaic (ITRPV), itrpv.vdma.org; 13th edition, 2022. pp. .1-81.
2. Towards 28%-efficient Si single-junction solar cells with better passivating POLO junctions and photonic crystals10.1016/j.solmat.2021.111560 ↗
3. Metallisation of boron‐doped polysilicon layers by screen printed silver pastes10.1002/pssr.201700334 ↗
4. Laser contact openings for local poly-Si-metal contacts enabling 26.1%-efficient POLO-IBC solar cells10.1016/j.solmat.2018.06.020 ↗
5. Design rules for high-efficiency both-sides-contacted silicon solar cells with balanced charge carrier transport and recombination losses10.1038/s41560-021-00805-w ↗
6. Degradation and regeneration of n+-doped poly-Si surface passivation on p-type and n-type cz-Si under illumination and dark annealing10.1109/JPHOTOV.2020.2964987 ↗
7. Long-term stability study of the passivation quality of polysilicon-based passivation layers for silicon solar cells
8. Investigating the degradation behaviours of n+-doped Poly-Si passivation layers: an outlook on long-term stability and accelerated recovery
9. 26.1%-efficient POLO-IBC cells: quantification of electrical and optical loss mechanisms10.1002/pip.3098 ↗
10. Firing stability of tube furnace-annealed n-type poly-Si on oxide junctions
11. Impact of firing and capping layers on long-term stability of doped poly-Si passivating contact layers10.1063/5.0089658 ↗
12. Rapid mitigation of carrier-induced degradation in commercial silicon solar cells
13. Development of advanced hydrogenation processes for silicon solar cells via an improved understanding of the behaviour of hydrogen in silicon10.1002/pip.3240 ↗
14. Evidence for a light-induced degradation mechanism at elevated temperatures in commercial N-type silicon heterojunction solar cells
15. Investigation of light-induced degradation in N-Type silicon heterojunction solar cells during illuminated annealing at elevated temperatures10.1016/j.solmat.2020.110752 ↗
16. Optimum hydrogen injection in phosphorus-doped polysilicon passivating contacts10.1021/acsami.1c17342 ↗
17. Firing stability of tube furnace-annealed n-type poly-Si on oxide junctions10.1002/pip.3459 ↗
18. Measurement of the emitter saturation current by a contactless photoconductivity decay method
19. Comparison of firing stability between p- and n-type polysilicon passivating contacts10.1002/pip.3544 ↗
20. Choi S, Kwon O, Hong Min K, et al. Formation and Suppression of Hydrogen Blisters in Tunnelling Oxide Passivating Contact for Crystalline Silicon Solar Cells. doi:10.1038/s41598-020-66801-4.10.1038/s41598-020-66801-4 ↗
21. Nemeth B, Young DL, Page MR, et al. INVITED FEATURE PAPER Polycrystalline Silicon Passivated Tunneling Contacts for High Efficiency Silicon Solar Cells. doi:10.1557/jmr.2016.77.10.1557/jmr.2016.77 ↗
22. Fırat · 2022
23. Optimum hydrogen injection in phosphorus-doped polysilicon passivating contacts10.1021/acsami.1c17342 ↗
24. Peeling behavior of a thin-film on a corrugated surface10.1016/j.ijsolstr.2015.02.003 ↗
25. Study of screen printed metallization for polysilicon based passivating contacts10.1016/j.egypro.2017.09.242 ↗
26. Skin care for healthy silicon solar cells
27. Bonilla · 2017
28. Effect of carrier-induced hydrogenation on the passivation of the poly-Si/SiO x/c-Si interface10.1063/1.5049289 ↗
29. High efficiency n-type silicon solar cells with passivating contacts based on PECVD silicon films doped by phosphorus diffusion10.1016/j.solmat.2019.01.005 ↗
30. Powerful recombination centers resulting from reactions of hydrogen with carbon–oxygen defects in n-type Czochralski-grown silicon
31. Nickel · 2000 · 62
32. Vacancy and vacancy-hydrogen complexes in silicon10.1103/PhysRevB.49.17040 ↗
33. Wenham · 2018 · 1
34. Hydrogen induced degradation: a possible mechanism for light- and elevated temperature- induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
35. On the hydrogenation of Poly-Si passivating contacts by Al2O3 and SiNx thin films
36. undefined. Hydrogen induced passivation of Si interfaces by films and stacks
37. Schmidt · 2004
38. Degradation and regeneration of n+-doped poly-Si surface passivation on p-type and n-type cz-Si under illumination and dark annealing10.1109/JPHOTOV.2020.2964987 ↗
39. Chen · 2020
40. Investigation of carrier lifetime instabilities in Cz-grown silicon
41. A four-state kinetic model for the carrier-induced degradation in multicrystalline silicon: introducing the reservoir state10.1016/j.solmat.2018.04.024 ↗
42. Hydrogen permeation through thin silicon oxide films10.1103/PhysRevB.52.7791 ↗
43. Changes in hydrogen concentration and defect state density at the poly-Si/SiOx/c-Si interface due to firing10.1016/j.solmat.2021.111297 ↗
44. Hydrogen-induced platelets in disordered silicon10.1016/0038-1098(96)00283-9 ↗
45. Defects in c-Si induced by hydrogenation10.1103/PhysRevB.35.4166 ↗
46. Modeling of hydrogen diffusion in n- and p-type silicon10.1103/PhysRevB.40.5867 ↗
47. A unified approach to modelling the charge state of monatomic hydrogen and other defects in crystalline silicon10.1063/1.4906465 ↗
48. Defect engineering of p-type silicon heterojunction solar cells fabricated using commercial-grade low-lifetime silicon wafers10.1002/pip.3230 ↗
49. Trap-limited hydrogen diffusion in doped silicon10.1103/PhysRevB.41.1054 ↗
50. Trap-limited hydrogen diffusion in boron-doped silicon10.1103/PhysRevB.46.2071 ↗
51. undefined. Possible candidates for impurities in mc‐Si wafers responsible for light‐induced lifetime degradation and regeneration
52. Investigation on the light and elevated temperature induced degradation of gallium-doped Cz-Si10.1016/j.solener.2021.07.023 ↗
53. Comparison of firing stability between p‐ and n‐type polysilicon passivating contacts10.1002/pip.3544 ↗
54. Kang · 2021
55. Highly passivating and blister-free hole selective poly-silicon based contact for large area crystalline silicon solar cells10.1016/j.solmat.2019.109912 ↗