journal article·2024-08

Influence of the medium-temperature light soaking process on the passivation and electronic performance of the N-TOPCon solar cells

Qinqin Wang, Siwen Gu, Kaiyuan Guo, Hui Peng, Wangping Wu, Jianning Ding

Publisher page

Abstract

Hydrogen (H) passivation is one of ideal candidates to reduce interfacial and bulk defects for providing good passivation by the light soaking process. Herein, we investigate the influence of the medium-temperature light soaking process on the passivation and electronic performance of the N-TOPCon solar cells. The medium-temperature light soaking process had the significant impact on the metallization-induced recombination of the p ++ layer and the Si substrate with a corroded silver (Ag) at a depth of >165 nm. During the light soaking process, the breaking the bending of (Si:H 2) n bonds causes H transitions from a bound state in the Si–H bond to a free state. In this state, H captures movable Ag and boron atoms on the wafer`s surface for passivation. The mechanism for enhancing the passivation on the metallization-induced recombination under the metal contact ( J 0 , metal) of SiO x/n + -poly-Si layer, the emitter dark saturation current density under the passivation layer ( J 0) of p + layer, and SiO x/n +-poly-Si layer is to prevent the formation of new defects by removing excess H. An efficiency gain of 0.87 % was observed after the light soaking process, attributed to the increase in open circuit voltage ( V oc ), short circuit current density ( J sc), and fill fact (FF) values by 10 mV, 0.15 mA/cm 2 , and 1.5 %, respectively. The partial gain of FF comes from the effect of medium-temperature enhanced metal contact. This research contributes to a profound understanding of the mechanism behind improving the medium-temperature light soaking process improvement and offers a feasible strategy for enhancing the efficiency N-TOPCon solar cells. After optimizing the front surface recombination and the medium-temperature light soaking processes, we manufactured industrial-grade TOPCon cells with in-house efficiency ( E ff), V oc, J sc, and FF values as high as 25.8 %, 729 mV, 42.1 mA/cm 2, and 84 %, respectively.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · solar cell performance optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Investigating the viability of PERC solar cells fabricated on Ga- instead of B-doped monocrystalline silicon wafer10.1016/j.solmat.2021.111134 ↗
2. Spectroscopic investigation of shallow hole traps in Ga- and B-doped czochralski silicon: insight into light-induced degradation10.1021/acsaem.2c02852 ↗
3. Silicon heterojunction solar cell with interdigitated back contacts for a photoconversion efficiency over 2610.1038/nenergy.2017.32 ↗
4. The rapidly reversible processes of activation and deactivation in amorphous silicon heterojunction solar cell under extensive light soaking10.1007/s10854-020-05146-0 ↗
5. Device physics underlying silicon heterojunction and passivating-contact solar cells: a topical review10.1002/pip.2959 ↗
6. Passivating contacts for crystalline silicon solar cells10.1038/s41560-019-0463-6 ↗
7. Tunnel oxide passivated rear contact for large area n-type front junction silicon solar cells providing excellent carrier selectivity10.3934/matersci.2016.1.180 ↗
8. Passivated rear contacts for high-efficiency n-type Si solar cells providing high interface passivation quality and excellent transport characteristics10.1016/j.solmat.2013.09.017 ↗
9. Impact of boron doping on electrical performance and efficiency of n-TOPCon solar cell10.1016/j.solener.2021.08.075 ↗
10. High-efficiency n-TOPCon bifacial solar cells with selective poly-Si based passivating contacts10.1016/j.solmat.2023.112458 ↗
11. Jinko Solarn (n.d.). https://www.jinkosolar.com/en/site/newsdetail/1827 (accessed March 17, 2023).
12. Surface passivation of crystalline silicon solar cells: present and future10.1016/j.solmat.2018.06.047 ↗
13. Boron tube diffusion process parameters for high-efficiency n-TOPCon solar cells with selective boron emitters10.1016/j.solmat.2023.112231 ↗
14. Passivating contacts for crystalline silicon solar cells10.1038/s41560-019-0463-6 ↗
15. Passivating contacts for crystalline silicon solar cells: from concepts and materials to prospects10.1109/JPHOTOV.2018.2797106 ↗
16. Carrier population control and surface passivation in solar cells10.1016/j.solmat.2018.04.026 ↗
17. n-type Si solar cells with passivating electron contact: identifying sources for efficiency limitations by wafer thickness and resistivity variation10.1016/j.solmat.2017.05.042 ↗
18. Screen printed, large area bifacial selective emitter N-PERT cells using single-step implantation through laser patterned dielectric layer
19. A laser induced forward transfer process for selective boron emitters10.1016/j.solmat.2016.12.026 ↗
20. BBr3 diffusion with second deposition for laser-doped selective emitters from borosilicate glass10.1016/j.solmat.2018.06.042 ↗
21. Boron laser doping using spin on dopant for textured crystalline silicon solar cell
22. Selective boron emitters using laser-induced forward transfer versus laser doping from borosilicate glass10.1109/JPHOTOV.2017.2717338 ↗
23. Advanced BBr3 diffusion with second deposition step for selective emitter formation by laser doping
24. High efficiency selective boron emitter formed by wet chemical etch-back for n-type screen-printed Si solar cells10.1063/1.4973626 ↗
25. High-efficiency n-type silicon PERT bifacial solar cells with selective emitters and poly-Si based passivating contacts10.1016/j.solener.2019.09.085 ↗
26. N-type polysilicon passivating contact combined with hydrogen-containing TCO as the interconnected structure for perovskite/silicon tandem solar cells10.1016/j.solmat.2022.111622 ↗
27. Effective hydrogenation of poly-Si passivating contacts by atomic-layer-deposited nickel oxide10.1109/JPHOTOV.2022.3206895 ↗
28. Laser induced localised hydrogen passivation10.1016/j.solener.2015.09.012 ↗
29. On the hydrogenation of Poly-Si passivating contacts by Al2O3 and SiNx thin films
30. Thermal activation of hydrogen for defect passivation in poly-Si based passivating contacts10.1016/j.solmat.2021.111267 ↗
31. Improved interface passivation by optimizing a polysilicon film under different hydrogen dilution in N-type TOPCon silicon solar cells10.1039/D2RA01286C ↗
32. Optimum hydrogen injection in phosphorus-doped polysilicon passivating contacts10.1021/acsami.1c17342 ↗
33. A density functional theory study on the passivation mechanisms of hydrogenated Si/Al2O3 interfaces10.1063/1.5123492 ↗
34. Passivation effect of ultra-thin SiNx films formed by catalytic chemical vapor deposition for crystalline silicon surface
35. Review of advanced hydrogen passivation for high efficient crystalline silicon solar cells10.1016/j.mssp.2018.01.019 ↗
36. Role of hydrogen in modifying a-Si:H/c-Si interface passivation and band alignment for rear-emitter silicon heterojunction solar cells10.1007/s10854-020-03486-5 ↗
37. Hydrogenation of phosphorus-doped polycrystalline silicon films for passivating contact solar cells10.1021/acsami.8b19989 ↗
38. Plasma hydrogen passivation for crystalline silicon thin-films
39. Improved amorphous/crystalline silicon interface passivation by hydrogen plasma treatment10.1063/1.3641899 ↗
40. The application of Poly-Si/SiOx contacts as passivated top/rear contacts in Si solar cells10.1016/j.solmat.2016.09.015 ↗
41. On the recombination behavior of p+ type polysilicon on oxide junctions deposited by different methods on textured and planar surfaces10.1002/pssa.201700058 ↗
42. Hydrogen-assisted defect engineering of doped Poly-Si films for passivating contact solar cells
43. Overcoming the challenges of hydrogenation in silicon solar cells10.1071/CH18271 ↗
44. The role of hydrogenation and gettering in enhancing the efficiency of next-generation Si solar cells: an industrial perspective
45. Hydrogen-induced degradation
46. Wenham · 2015
47. 23.83% efficient mono-PERC incorporatin advanced hydrogenation10.1002/pip.3243 ↗
48. Large-area boron-doped 1.6 Ω cm p-Type Czochralski silicon heterojunction solar cells with a stable open-circuit voltage of 736 mV and efficiency of 22.0
49. Investigations on accelerated processes for the boron-oxygen defect in p-type Czochralski silicon10.1016/j.solmat.2015.11.013 ↗
50. Effect of carrier-induced hydrogenation on the passivation of the Poly-Si/SiOx/c-Si interface10.1063/1.5049289 ↗
51. Statistical ray optics10.1364/JOSA.72.000899 ↗
52. Light-induced activation of boron doping in hydrogenated amorphous silicon for over 25% efficiency silicon solar cells10.1038/s41560-022-01018-5 ↗
53. Intensive light soaking improves electricity generation of silicon heterojunction solar cells by the anomalous Staebler–Wronski effect10.35848/1882-0786/ac8784 ↗
54. Reassessment of silicon heterojunction cell performance under operating conditions10.1016/j.solmat.2022.111951 ↗
55. Boron tube diffusion process parameters for high-efficiency n-TOPCon solar cells with selective boron emitters10.1016/j.solmat.2023.112231 ↗
56. Light injection annealing efficiency enhancement of N-type TOPCon crystalline silicon solar cell
57. Short wavelength photons destroying Si-H bonds and its influence on high efficiency silicon solar cells and modules
58. Lifetime degradation and regeneration in multicrystalline silicon under illumination at elevated temperature10.1063/1.4944839 ↗
59. Hydrogen passivation of multicrystalline silicon solar cells10.1016/S0921-5107(98)00288-8 ↗