journal article·2023-08

Understanding the impact of the cooling ramp of the fast-firing process on light- and elevated-temperature-induced degradation

Benjamin Hammann, Nicole Aßmann, Jonas Schön, Wolfram Kwapil, Florian Schindler, Sebastian Roder, Eduard V. Monakhov, Martin C. Schubert

Publisher page

Abstract

In current silicon solar cell technologies, hydrogen is incorporated into the solar cell during the fast-firing process. It passivates defects at the surface and in the bulk, but also leads to light- and elevated-temperature-induced degradation (LeTID). Although it is known that the hydrogen content and the LeTID extent can be reduced by employing a slower cooling ramp during the fast-firing process, the exact mechanism behind this phenomenon remains unclear. This study aims at closing this gap by investigating the impact of cooling ramps with different temperature plateaus on hydrogen (complexes) in B-doped FZ-Si wafers. The fired wafers are analyzed with FT-IR spectroscopy, four-point-probe resistivity measurements, and LeTID tests via effective lifetime measurements. Our findings provide evidence that hydrogen not only diffuses into the silicon bulk but can also effuse out of it during the cooling ramp. A one-dimensional hydrogen model is built in Sentaurus TCAD to simulate the in- and out-diffusion of hydrogen and to compare it with the experimental results. The experimentally determined hydrogen concentrations align with our simulation, with the diffusion being dominated by the fast-diffusing neutral hydrogen H 0. Moreover, we find stronger out-diffusion at higher temperatures, resulting in a lower total hydrogen concentration for slower cooling ramps. The extent of LeTID and surface-related degradation (SRD) are found to scale with the final total hydrogen concentration in the bulk. Therefore, modifying the cooling ramp can be an effective tool to optimize the hydrogen content and minimize the impact of degradation phenomena on silicon solar cells.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Impact of silicon nitride film properties on hydrogen in-diffusion into crystalline silicon
2. Study on boron–hydrogen pairs in bare and passivated float‐zone silicon wafers
3. Hydrogen passivation of multicrystalline silicon solar cells10.1016/S0921-5107(98)00288-8 ↗
4. H. C. Sio, S. P. Phang, H. T. Nguyen, Z. Hameiri, D. Macdonald, Hydrogenation in multicrystalline silicon: the impact of dielectric film properties and firing conditions, Prog. Photovoltaics Res. Appl., DOI: 10.1002/pip.3199.10.1002/pip.3199 ↗
5. Chen · 2018 · 1677
6. Development of advanced hydrogenation processes for silicon solar cells via an improved understanding of the behaviour of hydrogen in silicon
7. Influence of hydrogen on the regeneration of boron-oxygen related defects in crystalline silicon10.1063/1.4804310 ↗
8. Thermal activation of hydrogen for defect passivation in poly-Si based passivating contacts10.1016/j.solmat.2021.111267 ↗
9. Light induced degradation of rear passivated mc-Si solar cells
10. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
11. Understanding the light-induced degradation at elevated temperatures: similarities between multicrystalline and floatzone p-type silicon10.1002/pip.2954 ↗
12. Carrier-induced degradation in multicrystalline silicon: dependence on the silicon nitride passivation layer and hydrogen released during firing10.1109/JPHOTOV.2017.2783851 ↗
13. Evaluating root cause: the distinct roles of hydrogen and firing in activating light- and elevated temperature-induced degradation10.1063/1.5041756 ↗
14. On the defect physics behind light and elevated temperature-induced degradation (LeTID) of multicrystalline silicon solar cells10.1109/JPHOTOV.2019.2937223 ↗
15. Degradation of surface passivation on crystalline silicon and its impact on light-induced degradation experiments10.1109/JPHOTOV.2017.2755072 ↗
16. Degradation of surface passivation and bulk in p-type monocrystalline silicon wafers at elevated temperature10.1109/JPHOTOV.2018.2878791 ↗
17. Thermal processes and their impact on surface‐related degradation
18. Hydrogen-induced degradation: explaining the mechanism behind light- and elevated temperature-induced degradation in n- and p-type silicon10.1016/j.solmat.2019.110353 ↗
19. Insights into the hydrogen‐related mechanism behind defect formation during light‐ and elevated‐temperature‐induced degradation10.1002/pssr.202000584 ↗
20. Impact of the firing temperature profile on light induced degradation of multicrystalline silicon10.1002/pssr.201600272 ↗
21. LeTID mitigation via an adapted firing process in p‐type PERC cells from SMART cast‐monocrystalline, Czochralski and high‐performance multicrystalline silicon10.1002/pip.3467 ↗
22. Light and elevated temperature induced degradation in p-type and n-type cast-grown multicrystalline and mono-like silicon10.1016/j.solmat.2018.03.002 ↗
23. The impact of different hydrogen configurations on light- and elevated-temperature-induced degradation10.1109/JPHOTOV.2023.3236185 ↗
24. Temperature gradient image analysis to optimize an ultrafast regeneration of boron–oxygen-related defects10.1109/JPHOTOV.2021.3063659 ↗
25. Thermal activation and deactivation of grown-in defects limiting the lifetime of float-zone silicon10.1002/pssr.201600080 ↗
26. Atomic‐layer‐Deposited Al 2 O 3 as effective barrier against the diffusion of hydrogen from SiN x :H layers into crystalline silicon during rapid thermal annealing10.1002/pssr.202000367 ↗
27. On the role of AlO x thickness in AlO x/SiN y : H layer stacks regarding light- and elevated temperature-induced degradation and hydrogen diffusion in c-Si10.1109/JPHOTOV.2021.3075850 ↗
28. M. Mehler, F. Geml, A. Schmid, A. Zuschlag, G. Hahn, Effect of Different AlOx Passivation Layers Deposited by APCVD and ALD on LeTID, DOI: 10.4229/WCPEC-82022-1CV.3.5.
29. Hydrogen-related defects measured by infrared spectroscopy in multicrystalline silicon wafers throughout an illuminated annealing process10.1063/1.5142476 ↗
30. Methodology and error analysis of direct resistance measurements used for the quantification of boron–hydrogen pairs in crystalline silicon10.1109/JPHOTOV.2021.3074463 ↗
31. Concentration of atomic hydrogen diffused into silicon in the temperature range 900–1300 °C10.1063/1.104726 ↗
32. Interactions of hydrogen molecules with bond-centered interstitial oxygen and another defect center in silicon10.1103/PhysRevB.56.13118 ↗
33. Deactivation of the boron acceptor in silicon by hydrogen10.1063/1.94287 ↗
34. Neutralization of acceptors in silicon by atomic hydrogen10.1063/1.95030 ↗
35. Hydrogen solubility and defects in silicon10.4028/www.scientific.net/MSF.143-147.861 ↗
36. Hydrogen molecules in boron-doped crystalline silicon10.1088/0268-1242/14/1/011 ↗
37. Easy-to-apply methodology to measure the hydrogen concentration in boron-doped crystalline silicon10.1016/j.solmat.2019.109970 ↗
38. Contactless determination of current–voltage characteristics and minority‐carrier lifetimes in semiconductors from quasi‐steady‐state photoconductance data10.1063/1.117723 ↗
39. On the lifetime-equivalent defect density: properties, application, and pitfalls10.1109/JPHOTOV.2019.2922470 ↗
40. Doping dependence of the carrier lifetime crossover point upon dissociation of iron-boron pairs in crystalline silicon10.1063/1.2358126 ↗
41. Effect of dissociation of iron-boron pairs in crystalline silicon on solar cell properties10.1002/pip.594 ↗
42. Influence of highly doped layers on hydrogen in-diffusion into crystalline silicon10.1016/j.solmat.2022.112056 ↗
43. A unified approach to modelling the charge state of monatomic hydrogen and other defects in crystalline silicon10.1063/1.4906465 ↗
44. Modelling of hydrogen transport in silicon solar cell structures under equilibrium conditions10.1063/1.5016854 ↗
45. Temporary recovery of the defect responsible for light- and elevated temperature-induced degradation: insights into the physical mechanisms behind LeTID10.1109/JPHOTOV.2020.3025240 ↗
46. Dynamics of hydrogen in silicon at finite temperatures from first principles10.1002/pssb.202100670 ↗
47. Bond-centered hydrogen in silicon studied by in situ deep-level transient spectroscopy10.1103/PhysRevB.60.1716 ↗
48. Acceptor state of monoatomic hydrogen in silicon and the role of oxygen
49. Independent subsystems of atomic hydrogen in silicon responsible for boron passivation and for dimer production
50. Very low surface recombination velocity on p-type c-Si by high-rate plasma-deposited aluminum oxide10.1063/1.3250157 ↗
51. B. Hammann, B. Steinhauser, A. Fell, R. Post, T. Niewelt, W. Kwapil, A. Wolf, A. Richter, H. Höffler, M. C. Schubert, Quantifying surface recombination—improvements in determination and simulation of the surface recombination parameter J0s, IEEE J. Photovoltaics. 2023 Early Access, DOI: 10.1109/JPHOTOV.2023.3265859.10.1109/JPHOTOV.2023.3265859 ↗