Addressing sodium ion-related degradation in SHJ cells by the application of nano-scale barrier layers
Source abstract
Abstract
Silicon heterojunction (SHJ) solar cells are renowned for their high efficiency. However, SHJ solar cells are susceptible to various contaminants, leading to significant performance degradation when exposed to damp-heat conditions (e.g., 85 °C and 85% relative humidity). Sodium (Na) has been identified as one of the main contributors to degradation in silicon solar modules subjected to damp-heat conditions. This work investigates the role of an ultra-thin AlOx capping layer (∼10 nm) in preventing the failure in SHJ cells caused by Na-related contaminants. NaCl is applied directly to the solar cell, and the unencapsulated cell undergoes a damp heat test at 85 °C and 85% relative humidity (DH85). It is found that without the AlOx barrier layer, the SHJ cells experience a relative reduction in power of ∼30%rel after only 20 h at DH85. Both the front and rear sides of the cell degrade when exposed to NaCl. This is primarily due to a deterioration of the Ag contact resulting in increased series resistance (Rs), and decrease in fill factor (FF), and an increase in recombination, leading to a significant drop in open-circuit voltage (Voc), particularly when NaCl is applied on the rear side. However, when an AlOx barrier layer is applied to the SHJ cells, the performance losses caused by NaCl are significantly reduced to only ∼3.3%rel. The loss in Voc on the rear side is completely suppressed, and there is only a slight increase in Rs of ∼50%rel compared to ∼300%rel increase in Rs for cells without the AlOx barrier layer. These findings indicate that the ultra-thin AlOx barrier layer provides effective protection for SHJ cells against Na ions, mitigating both Rs and recombination losses. This AlOx barrier layer depositing method is compatible with existing industrial mass-production ALD tools and thus presents a viable solution at the cell level for SHJ cells.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Photovoltaic System Optimization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Polysilicon passivated junctions: the next technology for silicon solar cells?10.1016/j.joule.2021.02.013 ↗
2. Mass production of crystalline silicon solar cells with polysilicon‐based passivating contacts: an industrial perspective10.1002/pip.3618 ↗
3. High-efficiency silicon heterojunction solar cells: materials, devices and applications10.1016/j.mser.2020.100579 ↗
4. Passivating contacts and tandem concepts: approaches for the highest silicon-based solar cell efficiencies10.1063/1.5139202 ↗
5. Passivating contacts for crystalline silicon solar cells10.1038/s41560-019-0463-6 ↗
6. Solar cell efficiency tables (Version 61)10.1002/pip.3646 ↗
7. Silicon heterojunction solar cells with up to 26.81% efficiency achieved by electrically optimized nanocrystalline-silicon hole contact layers
8. The value of stability in photovoltaics10.1016/j.joule.2021.10.019 ↗
9. Long‐term performance and reliability of silicon heterojunction solar modules10.1002/pip.3688 ↗
10. The effect of moisture on the degradation mechanism of multi-crystalline silicon photovoltaic module10.1016/j.microrel.2013.07.047 ↗
11. The degradation of multi-crystalline silicon solar cells after damp heat tests10.1016/j.microrel.2014.07.071 ↗
12. Moisture induced degradation in field-aged multicrystalline silicon photovoltaic modules10.1016/j.solmat.2023.112407 ↗
13. Four failure modes in silicon heterojunction glass-backsheet modules10.1016/j.solmat.2023.112358 ↗
14. The causes and effects of degradation of encapsulant ethylene vinyl acetate copolymer (EVA) in crystalline silicon photovoltaic modules: a review10.1016/j.rser.2017.06.039 ↗
15. EVA degradation mechanisms simulating those in PV modules
16. Investigation of the degradation and stabilization of EVA-based encapsulant in field-aged solar energy modules10.1016/S0141-3910(96)00162-0 ↗
17. Comprehensive study of the degradation of an intumescent EVA-based material during combustion10.1023/A:1004758218104 ↗
18. Impact of acetic acid exposure on metal contact degradation of different crystalline silicon solar cell technologies10.1016/j.solmat.2022.112089 ↗
19. Crystalline Si photovoltaic modules functionalized by a thin polyethylene film against potential and damp-heat-induced degradation10.1039/C4RA13360A ↗
20. Electrochemical degradation modes in bifacial silicon photovoltaic modules
21. Degradation studies of polyolefins incorporating transparent nanoparticulate zinc oxide UV stabilizers10.1023/A:1020121700825 ↗
22. The effect of processing conditions on the uv stability of polyolefins10.1016/0014-3057(73)90129-8 ↗
23. Potential-induced degradation in photovoltaic modules: a critical review10.1039/C6EE02271E ↗
24. Sodium accumulation at potential-induced degradation shunted areas in polycrystalline silicon modules10.1109/JPHOTOV.2016.2601950 ↗
25. Comprehensive study of potential-induced degradation in silicon heterojunction photovoltaic cell modules10.1002/pip.3006 ↗
26. Supercharging cell-level potential-induced degradation (PID) testing using a salt-enriched hybrid polymer layer10.1016/j.solmat.2023.112479 ↗
27. Potential‐free sodium‐induced degradation of silicon heterojunction solar cells10.1002/pip.3698 ↗
28. Effects of SiOx barrier layer prepared by plasma-enhanced chemical vapor deposition on improvement of long-term reliability and production cost for Cu-plated amorphous Si/crystalline Si heterojunction solar cells10.1016/j.solmat.2016.12.029 ↗
29. Highly crystallized tungsten doped indium oxide film stabilizes silicon heterojunction solar cells in sodium environment10.1016/j.solmat.2021.111387 ↗
30. The role of Na+ contamination in humidity-induced degradation in silicon HJT cells
31. A novel approach to utilize Al2O3 and polyolefin encapsulant as an optical and electrical materials to mitigate potential-induced of PV modules10.1016/j.optmat.2022.113022 ↗
32. Surface passivation of efficient nanotextured black silicon solar cells using thermal atomic layer deposition10.1021/am402889k ↗
33. High-efficiency c-Si solar cells passivated with ALD and PECVD aluminum oxide10.1109/LED.2010.2049190 ↗
34. Contaminant particles in electronic solder fluxes10.1108/eb037700 ↗
35. The 2020 photovoltaic technologies roadmap10.1088/1361-6463/ab9c6a ↗
36. Detection of visible and latent fingerprints using micro-X-ray fluorescence elemental imaging10.1111/j.1556-4029.2005.00006.x ↗
37. The chlorine abundance of Earth: implications for a habitable planet10.1016/j.epsl.2013.03.005 ↗
38. The budget and cycle of Earth's natural chlorine10.1351/pac199668091689 ↗
39. Chlorine stable isotope composition of the oceanic crust: implications for Earth's distribution of chlorine10.1016/0012-821X(95)00017-7 ↗
40. Accelerated damp-heat testing at the cell-level of bifacial silicon HJT, PERC and TOPCon solar cells using sodium chloride10.1016/j.solmat.2023.112554 ↗
41. Moisture ingress in photovoltaic modules: a review10.1016/j.solener.2021.06.055 ↗
42. Imaging and micro-structural characterization of moisture induced degradation in crystalline silicon photovoltaic modules10.1016/j.solener.2019.11.037 ↗
43. An advanced software suite for the processing and analysis of silicon luminescence images10.1016/j.cpc.2017.02.012 ↗
44. Advanced luminescence based effective series resistance imaging of silicon solar cells10.1063/1.2982588 ↗
45. Atmospheric corrosion of silver in outdoor environments and modified accelerated corrosion chambers10.5006/2079 ↗
46. Effect of chloride on the dissolution rate of silver nanoparticles and toxicity to E. coli10.1021/es400396f ↗
47. The effect of silver chloride formation on the kinetics of silver dissolution in chloride solution10.1016/j.electacta.2010.12.050 ↗
48. Corrosion behavior of silver-coated conductive yarn10.3389/fchem.2023.1090648 ↗
49. Electrochemical corrosion and protection of low-temperature sintered silver nanoparticle paste in NH4Cl solution10.1007/s10854-021-05952-0 ↗
50. Corrosion mechanisms for silver exposed to the atmosphere10.1149/1.2221162 ↗
51. Analysis of Ag corrosion products10.1149/2.055308jes ↗
52. Salt crystallization-assisted degradation of epoxy resin surface in simulated marine environments10.1016/j.porgcoat.2020.105932 ↗
53. Molecular dynamics study on the effect of salt environment on interfacial structure, stress, and adhesion of carbon fiber/epoxy interface10.1080/09276440.2018.1506901 ↗
54. Characterization of Indium−Tin oxide interfaces using X-ray photoelectron spectroscopy and redox processes of a chemisorbed probe molecule: effect of surface pretreatment conditions10.1021/la011101t ↗
55. Towards highly electrically conductive and thermally insulating graphene nanocomposites: Al2O3–graphene10.1039/C3RA45069D ↗
56. Structural and XPS characterization of ALD Al2O3 coated porous silicon10.1016/j.vacuum.2014.12.015 ↗
57. Improvement of Al2O3 films on graphene grown by atomic layer deposition with pre-H2O treatment10.1021/am501690g ↗
58. X-ray photoelectron spectroscopic study of hydrated aluminas and aluminas10.1557/JMR.1994.2919 ↗
59. High performance In2O3 thin film transistors using chemically derived aluminum oxide dielectric10.1063/1.4816060 ↗