Effect of heat, UV radiation, and moisture on the decohesion kinetics of inverted organic solar cells
Source abstract
Abstract
Abstract Organic solar cells subjected to environmental stressors such as heat, moisture, and UV radiation can undergo significant mechanical degradation, leading to delamination of layers and device failure. This paper reports the effect these stressors have on the mechanical integrity of active layers and interfaces as measured by subcritical debonding tests, and the in situ evolution of defects and fracture processes is characterized. At elevated temperatures below 50 °C in inert conditions, significant device weakening was observed, an effect we attributed to a temperature-induced P3HT:PCBM delamination mechanism from the underlying ZnO. At 50 °C in ambient conditions with UV exposure—selected to better simulate real-world environments—devices were more resistant to fracture because of an interfacial strengthening effect from increased hydrogen bonding where UV-induced Zn(OH) 2 formation reinforced the interface with P3HT:PCBM. This photoinduced hydroxylation mechanism was determined from a decrease in the Zn/O ratio with increased UVA or UVB exposure, and hydroxylation was shown to directly correlate with the resistance to fracture in devices.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Organic Electronics and Photovoltaics · Thin-Film Transistor Technologies · Silicon and Solar Cell Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Stability of organic solar cells: challenges and strategies10.1039/C5CS00593K ↗
2. Photochemical stability of [small pi]-conjugated polymers for polymer solar cells: a rule of thumb10.1039/c0jm03105d ↗
3. Promising long-term stability of encapsulated ITO-free bulk-heterojunction organic solar cells under different aging conditions10.1016/j.solmat.2014.07.004 ↗
4. Stability of polymer solar cells10.1002/adma.201104187 ↗
5. Progress in understanding degradation mechanisms and improving stability in organic photovoltaics10.1002/adma.201603940 ↗
6. Thermal cycling effect on mechanical integrity of inverted polymer solar cells10.1016/j.solmat.2015.07.019 ↗
7. Decohesion kinetics in polymer organic solar cells10.1021/am506482q ↗
8. Failure modes and fast repair procedures in high voltage organic solar cell installations10.1002/aenm.201301625 ↗
9. Understanding mechanical behavior and reliability of organic electronic materials10.1557/mrs.2017.3 ↗
10. Role of stress factors on the adhesion of interfaces in R2R fabricated organic photovoltaics10.1002/aenm.201501927 ↗
11. Interlayer adhesion in roll-to-roll processed flexible inverted polymer solar cells10.1016/j.solmat.2011.10.012 ↗
12. Water and oxygen induced degradation of small molecule organic solar cells10.1016/j.solmat.2011.01.001 ↗
13. Degradation mechanisms in organic photovoltaic devices10.1016/j.orgel.2011.11.027 ↗
14. Degradation patterns in water and oxygen of an inverted polymer solar cell10.1021/ja106299g ↗
15. Decohesion kinetics of PEDOT:PSS conducting polymer films10.1002/adfm.201302174 ↗
16. Adhesion and debonding of multi-layer thin film structures10.1016/S0013-7944(98)00052-6 ↗
17. Moisture-assisted subcritical debonding of a polymer/metal interface10.1063/1.1427139 ↗
18. Anomalous debonding behavior of a polymer/inorganic interface10.1016/j.actamat.2007.02.012 ↗
19. Fracture of nanoporous thin-film glasses10.1038/nmat1037 ↗
20. Adhesion and subcritical debonding of polymer interfaces for microelectronic packaging10.1557/PROC-515-37 ↗
21. A four-point bending technique for studying subcritical crack growth in thin films and at interfaces10.1557/JMR.1997.0122 ↗
22. Kinetics of crack initiation and growth in organic-containing integrated structures10.1016/j.jmps.2003.09.022 ↗
23. An atomistic model of kinetic crack growth in brittle solids10.1007/BF00543692 ↗
24. Effects of water and other dielectrics on crack growth10.1007/BF00752191 ↗
25. Role of electron- and hole-collecting buffer layers on the stability of inverted polymer: fullerene photovoltaic devices10.1109/JPHOTOV.2013.2287913 ↗
26. An augmented double cantilever beam model for studying crack propagation and arrest10.1007/BF00035958 ↗
27. Phase diagram of P3HT/PCBM blends and its implication for the stability of morphology10.1021/jp804151a ↗
28. The effects of network structure on the resistance of silane coupling agent layers to water-assisted crack growth10.1021/la035920k ↗
29. Influence of substrate on crystallization in polythiophene/fullerene blends10.1016/j.solmat.2010.12.035 ↗
30. Photodegradation of P3HT−A systematic study of environmental factors10.1021/cm102373k ↗
31. The mechanism of photo- and thermooxidation of poly(3-hexylthiophene) (P3HT) reconsidered
32. Effects of long-term UVvisible light irradiation in the absence of oxygen on P3HT and P3HT: PCBM blend10.1016/j.solmat.2010.03.012 ↗
33. Effect of interchain interactions on the absorption and emission of poly(3-hexylthiophene)10.1103/PhysRevB.67.064203 ↗
34. Electronic structure and optical properties of Zn(OH)2: lDA+U calculations and intense yellow luminescence10.1039/C5RA17024A ↗
35. Photoinduced hydroxylation at ZnO surface10.1016/S0040-6090(03)01162-3 ↗
36. Alkyl surface treatments of planar zinc oxide in hybrid organic/inorganic solar cells10.1021/jp211692m ↗