Identification of the most relevant metal impurities in mc n-type silicon for solar cells
Source abstract
Abstract
Abstract In general, the charge carrier lifetime in n -type silicon is less sensitive to common dissolved metals compared to p -type silicon. However, in experiments it was observed that metal impurities limit the lifetime in n -type multicrystalline (mc) silicon even if high purity feedstock was used. By evaluating Neutron Activation Analysis (NAA) and Inducitvely Coupled Plasma Mass Spectrometry (ICP-MS) at blocks grown with high purity feedstock, we identified the main currently unavoidable metal impurities present in n -type mc silicon. In addition, we measured the charge carrier lifetime on surface-passivated wafers after different solar cell processes. The measurements were compared to simulations in order to identify the limitations by different impurities and to evaluate the influence of metal precipitates. We found that Cr i is an important defect in good grains of as-grown wafers. Dissolved Co can have a severe impact on lifetime after process steps with fast cooling. The lower lifetime in the edge region of the blocks is attributed to FeSi 2 precipitates, which explains the poor gettering response of the edge region in contrast to grains in the block center. From the results obtained for FeSi 2 -precipitates, we concluded that Cu 3 Si- and NiSi 2 -precipitates located at crystal defects may be responsible for significant recombination in the block center.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Recombination activity of interstitial iron and other transition metal point defects in p- and n-type crystalline silicon10.1063/1.1812833 ↗
2. Defect generation, advanced crystallization, and characterization methods for high-quality solar-cell silicon10.1002/pssa.201200639 ↗
3. Characterization of high-efficiency multi-crystalline silicon in industrial production10.1016/j.solmat.2013.06.013 ↗
4. Development of high-performance multicrystalline silicon for photovoltaic industry10.1002/pip.2437 ↗
5. Potential gain in multicrystalline silicon solar cell efficiency by n-type doping10.1109/JPHOTOV.2014.2377554 ↗
6. Significant minority carrier lifetime improvement in red edge zone in n-type multicrystalline silicon10.1016/j.solmat.2013.02.026 ↗
7. Effect of iron in silicon feedstock on p- and n-type multicrystalline silicon solar cells10.1063/1.3021355 ↗
8. Impact of iron precipitates on carrier lifetime in as-grown and phosphorus-gettered multicrystalline silicon wafers in model and experiment10.1109/JPHOTOV.2014.2304355 ↗
9. Impurity-related limitations of next-generation industrial silicon solar cells10.1109/JPHOTOV.2012.2210030 ↗
10. Impact of impurities from crucible and coating on mc-silicon quality – the example of iron and cobalt10.1109/JPHOTOV.2013.2279116 ↗
11. W. Kwapil, A. Zuschlag, I. Reis, I. Schwirtlich, S. Meyer, R. Zierer, et al., Influence of crucible and coating on the contamination of directionally solidified silicon: first results of the German research network “SolarWinS”, in: Proceedings of the 27th EUPVSEC, 2012, pp. 627–635.
12. Minority carrier lifetime imaging of silicon wafers calibrated by quasi-steady-state photoluminescence10.1016/j.solmat.2010.12.016 ↗
13. Harmonically modulated luminescence: bridging gaps in carrier lifetime metrology across the PV processing chain10.1109/JPHOTOV.2014.2362304 ↗
14. Imaging interstitial iron concentrations in boron-doped crystalline silicon unsing photoluminescence10.1063/1.2903895 ↗
15. Imaging of metastable defects in silicon10.1109/JPHOTOV.2011.2169942 ↗
16. Imaging of chromium point defects in p-type silicon10.1063/1.3459892 ↗
17. Reassessment of the recombination parameters of chromium in n- and p-type crystalline silicon and chromium–boron pairs in p-type crystalline silicon10.1063/1.4881497 ↗
18. Iron and its complexes in silicon10.1007/s003390050968 ↗
19. Understanding the distribution of iron in multicrystalline silicon after emitter formation: theoretical model and experiments10.1063/1.3553858 ↗
20. Experimental and theoretical study of heterogeneous iron precipitation in silicon10.1063/1.2472271 ↗
21. Re-emission of iron originally gettered by oxygen precipitates in a silicon wafer10.1063/1.354905 ↗
22. Gettering of iron in silicon by boron implantation
23. Imaging as-grown interstitial iron concentration on boron-doped silicon bricks via spectral photoluminescence10.1109/JPHOTOV.2014.2326714 ↗
24. Predictive simulation of doping processes for silicon solar cells10.1016/j.egypro.2013.07.283 ↗
25. Mechanisms of transition-metal gettering in silicon10.1063/1.1289273 ↗
26. Analysis of simultaneous boron and phosphorus diffusion gettering in silicon10.1002/pssa.201026333 ↗
27. The impact of different diffusion temperature profiles on iron concentrations and carrier lifetimes in multicrystalline silicon wafers10.1109/JPHOTOV.2012.2231726 ↗
28. Chromium distribution in multicrystalline silicon: comparison of simulations and experiments10.1002/pip.1252 ↗
29. Precipitation kinetics of solid solutions of chromium in silicon
30. Transition metals in silicon10.1007/BF00617708 ↗
31. Cobalt related defect levels in silicon analyzed by temperature- and injection-dependent lifetime spectroscopy10.1063/1.2433743 ↗
32. Gettering in silicon photovoltaics: current state and future perspectives10.1002/pssa.200664516 ↗
33. Carrier recombination at metallic precipitates in p- and n-type silicon10.1109/JPHOTOV.2015.2438634 ↗
34. Hydrogen-induced defects in cobalt-doped n-type silicon10.1088/0268-1242/11/1/007 ↗
35. Graff · 1999
36. P. Rosenits, D. Macdonald, Lifetime studies on manganese implanted silicon, in: Proceedings of the 21st EUPVSEC, Dresden, Germany, 2006, pp. 953–956.
37. Determination of bulk lifetime and surface recombination velocity of silicon ingots from dynamic photoluminescence10.1109/JPHOTOV.2013.2264622 ↗
38. Preventing light-induced degradation in multicrystalline silicon10.1063/1.4871404 ↗
39. Research on efficiency limiting defects and defect engineering in silicon solar cells – results of the German research cluster solarfocus10.1002/pssc.201000338 ↗
40. Metallic impurities in mono and multi-crystalline silicon and their gettering by phosphorus diffusion10.1149/1.2980302 ↗