Degradation mechanisms and non-linear thermal cycling effects in a high-temperature light-absorber coating
Source abstract
Abstract
Abstract Absorber coatings in concentrating solar power (CSP) convert focused solar radiation into heat. Competitive and reliable CSP technologies require absorber coatings to be stable at high temperatures for many years of operation, and thus accelerated ageing tests are essential to evaluate and further develop these coatings. However, the ageing mechanisms are largely unknown, with previous studies mainly focusing on isothermal (IT) annealing or rapid-cycling (RC) thermal tests, not the more realistic cycle-and-hold (CH) thermal cycling caused by cloud shading. This investigation reports the effects of IT, CH and RC on degradation of Pyromark 2500 on Inconel 625. CH thermal cycling was a combination of IT (equivalent heating time at T max = 850 ° C ) and RC (equivalent cycles). The results showed non-linear effects because: IT and RC samples were found to be stable (within 100 h or 1260 cycles) in terms of absorptance, despite having some differences in morphology; whereas CH samples experienced a drop in solar-weighted absorptance after 10 h (126 cycles) at T max followed by an increase after 100 h (1260 cycles). SEM and XRD analyses suggested that thermal cycling promoted sintering of the silica binder, producing an amorphous structure between fully formed crystalline grains, which were identified as nickel- and/or manganese-based chromite. The sintering occurred more severely for CH than RC due to holding the temperature at T max . Cracking was also more pronounced in CH than RC and IT, possibly due to stronger coating shrinkage. The results suggest that accelerated ageing tests should consider CH thermal cycling to better analyse coating degradation and predict its lifetime.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Solar Thermal and Photovoltaic Systems · Photovoltaic System Optimization Techniques · Silicon and Solar Cell Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Effect of the optical properties of the coating of a concentrated solar power central receiver on its thermal efficiency10.1016/j.solmat.2016.08.031 ↗
2. Characterization of Pyromark 2500 paint for high-temperature solar receivers10.1115/1.4024031 ↗
3. Solar selective coatings for concentrating solar power central receivers
4. Micro- and nanostructured surfaces for selective solar absorption10.1002/adom.201500063 ↗
5. Development of high absorption, high durability coatings for solar receivers in CSP plants10.1063/1.5067075 ↗
6. Optical properties and thermal stability of Cu spinel oxide nanoparticle solar absorber coatings10.1016/j.solmat.2019.02.032 ↗
7. Optical properties of Pyromark 2500 coatings of variable thicknesses on a range of materials for concentrating solar thermal applications10.1063/1.4984355 ↗
8. Dynamic modeling of solar radiation disturbances based on a biomimetic cloud shading model10.1115/1.4038961 ↗
9. High-solar-absorptance CSP coating characterization and reliability testing with isothermal and cyclic loads for service-life prediction10.1039/C8EE03536A ↗
10. Durability of solar absorber coatings and their cost-effectiveness10.1016/j.solmat.2017.03.010 ↗
11. Influence of application parameters on stability of Pyromark® 2500 receiver coatings10.1063/1.5117514 ↗
12. Burge · 2015
13. A CFD-supported dynamic system-level model of a sodium-cooled billboard-type receiver for central tower CSP applications10.1016/j.solener.2018.11.031 ↗
14. Coating deterioration
15. Failure mechanisms of thermal barrier coatings exposed to elevated temperatures10.1016/0040-6090(82)90019-0 ↗
16. Cracking in and around the thermally grown oxide in thermal barrier coatings: a comparison of isothermal and cyclic oxidation10.1007/s10853-005-3639-3 ↗
17. Aging of solar absorber materials under highly concentrated solar fluxes10.1016/j.solmat.2014.01.010 ↗
18. A numerical thermal approach to study the accelerated aging of a solar absorber material10.1016/j.solener.2012.08.007 ↗
19. Accelerated aging of absorber coatings for CSP receivers under real high solar flux – evolution of their optical properties10.1016/j.solmat.2018.12.030 ↗
20. Copper-alloyed spinel black oxides and tandem-structured solar absorbing layers for high-temperature concentrating solar power systems10.1016/j.solener.2016.03.007 ↗
21. Accelerated life testing of solar absorber coatings: testing procedure and results10.1016/S0038-092X(00)00034-7 ↗
22. Nelson · 1986
23. Characterization of Pyromark 2500 Paint for High-Temperature Solar Receivers
24. Pacheco · 2002
25. Transient analysis of a molten salt central receiver (MSCR) in a solar power plant10.1063/1.4949221 ↗
26. Mixed convection and radiation from an isothermal bladed structure10.1016/j.ijheatmasstransfer.2019.118906 ↗
27. Accelerated aging of a solar absorber material subjected to highly concentrated solar flux10.1016/j.egypro.2014.03.176 ↗
28. Black oxide nanoparticles as durable solar absorbing material for high-temperature concentrating solar power system10.1016/j.solmat.2014.12.004 ↗
29. Coatings for enhanced photothermal energy collection II. Non-selective and energy control films10.1016/0165-1633(79)90026-1 ↗
30. Optimal wavelength scale diffraction gratings for light trapping in solar cells
31. Diffractive gratings to improve TiAlN based spectrally selective solar absorbers10.1063/1.5067043 ↗
32. Inverted nanopyramid texturing for silicon solar cells using interference lithography10.1016/j.mee.2014.04.004 ↗
33. Nanophotonic light trapping in solar cells10.1063/1.4747795 ↗
34. Sai · 2005 · 762
35. Solar selective absorbers based on two-dimensional W surface gratings with submicron periods for high-temperature photothermal conversion10.1016/S0927-0248(02)00364-1 ↗
36. Ni-based chromite spinel for high-performance supercapacitors10.1039/C5RA27931C ↗
37. A salt-assisted combustion method to prepare well-dispersed octahedral MnCr2O4 spinel nanocrystals
38. Magnetization reversal induced by Mn substitution in spinel chromite NiCr2O410.1111/jace.15869 ↗
39. Optical properties and magnetic properties of antisite-disordered Ni1–xCoxCr2O4 spinels10.1016/S1003-6326(17)60099-2 ↗
40. Effect of the particle size on the activity of MoO x C y catalysts for the isomerization of heptane10.1007/s10562-004-3459-0 ↗
41. Predicting Subsurface Enrichment/depletion Processes during High-Temperature Oxidation of Alloy 625 Thin Foils
42. Oxidation kinetics of some nickel-based superalloy foils and electronic resistance of the oxide scale formed in air Part I10.1149/1.1392454 ↗
43. Isothermal oxidation of Inconel 625 superalloy at 800 and 1000 °C: microstructure and oxide layer characterization10.1016/j.matchar.2020.110160 ↗