journal article·2019-06Open access

Compatibility of SiC--and MAX phase-based ceramics with a KNO3-NaNO3 molten solar salt

K. Van Loo, T. Lapauw, N. Ozalp, E. Ström, K. Lambrinou, J. Vleugels

Abstract

Abstract In this work, several ceramic materials were exposed together with two reference structural materials (i.e., 316 L stainless steel and Inconel 600) to a molten solar salt (40 wt% KNO3 and 60 wt% NaNO3) for 1000 h at 600 °C to investigate their compatibility with the molten salt medium, thus assessing their potential use in concentrated solar power (CSP) applications. The exposed ceramics included different SiC grades (solid state-sintered, liquid phase-sintered, and silicon-infiltrated) and MAX phase-based materials (Maxthal® 211 & 312 (nominally, Ti2AlC & Ti3SiC2, respectively), Cr2AlC, Nb4AlC3, (Nb,Zr)4AlC3, and a cermet comprising 40 vol% Fe and 60 vol% (Nb,Zr)4AlC3). All SiC grades were chemically stable in the molten salt, whereas all Nb-containing MAX phase ceramics were severely oxidized. Comparing the two Maxthal® grades showed that the 312 was chemically more stable than the 211, and both grades formed a Na-based oxide scale. Interestingly, Cr2AlC showed practically no interaction with the molten salt during the performed exposure, forming a stable, sub-micrometre-thick Cr7C3 scale. Hence, it may be considered as promising structural/coating material candidate for the targeted CSP application.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Phase Change Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Concentrating solar power10.1021/acs.chemrev.5b00397 ↗
2. Concentrated solar power plants: review and design methodology10.1016/j.rser.2013.01.032 ↗
3. Solar thermal-powered desalination: a viable solution for a potential market10.1016/j.desal.2017.12.025 ↗
4. Optimizing the supercritical CO2 Brayton cycle for concentrating solar power application
5. Vilella · 2014
6. Assessment of a molten salt heat transfer fluid in a parabolic trough solar field10.1115/1.1565087 ↗
7. Characterization of thermal performance, flux transmission performance and optical properties of MAX phase materials under concentrated solar irradiation10.1016/j.solmat.2018.03.018 ↗
8. Corrosion behavior of stainless and low-chromium steels and IN625 in molten nitrate salts at 600 °C10.1016/j.solmat.2015.08.011 ↗
9. Corrosion of silicon carbide in gases and alkaline melts10.1111/j.1151-2916.1976.tb09514.x ↗
10. Corrosion characteristics of silicon carbide and silicon nitride10.6028/jres.098.040 ↗
11. Oxidation transitions for SiC part I. Active-to-passive transitions10.1111/jace.12108 ↗
12. Progress in corrosion resistant materials for supercritical water reactors10.1016/j.corsci.2009.07.007 ↗
13. Barsoum · 2013
14. Corrosion of ternary carbides by molten lead10.1016/j.jnucmat.2007.04.054 ↗
15. Heinzel · 2016 · vol. 482 · 114
16. Compatibility of Ti3SiC2 with liquid Pb and PbBi containing oxygen10.1016/j.jnucmat.2009.03.004 ↗
17. Oxidation properties of ” solar salt ”
18. Overview of molten salt storage systems and material development for solar thermal power plants
19. Molten salts database for energy applications10.1016/j.cep.2013.07.008 ↗
20. Direct laser sintering of reaction bonded silicon carbide with low residual silicon content10.1016/j.jeurceramsoc.2018.04.055 ↗
21. (Nbx, Zr1– x)4AlC3 MAX phase solid solutions: processing, mechanical properties, and density functional theory calculations10.1021/acs.inorgchem.6b00484 ↗
22. Solid state sintering of SiC-ceramics10.4028/www.scientific.net/MSF.624.71 ↗
23. Aqueous colloidal processing of SiC with Y3Al5O12 liquid-phase sintering additives10.1016/j.jeurceramsoc.2013.01.030 ↗
24. Microstructural evolution in liquid-phase-sintered SiC: Part I, effect of starting powder10.1111/j.1151-2916.2001.tb00880.x ↗
25. High temperature corrosion in molten solar salt: the role of chloride impurities10.1002/maco.201609300 ↗
26. Corrosion resistance of stainless steels during thermal cycling in alkali nitrate
27. Bogaerts · 2015
28. Stern · 1982
29. Dissolution of Cr2O3(s) and the behavior of chromium in concentrated NaOH solutions10.1021/ie302096e ↗
30. A review of steel corrosion by liquid lead and lead-bismuth10.1016/j.corsci.2009.03.013 ↗
31. Corrosion of stainless steels in lead-bismuth eutectic up to 600°C10.1016/j.jnucmat.2004.07.012 ↗
32. Corrosion behaviour of steels in lead-bismuth at 823 K10.1016/j.jnucmat.2004.07.013 ↗
33. Interaction of molten salts in the systems SiO2 - Al2O3 ( Interação de sais fundidos no sistema SiO2 - Al2O3)10.1590/S0366-69132013000400013 ↗
34. Molchanov · 1957
35. Effect of heating rates and composition on the thermal decomposition of nitrate based molten salts10.1016/j.egypro.2015.03.075 ↗
36. Low-melting CaCl2 - NaCl - Al2O3 electrolyte for direct electrochemical reduction solid Al2O310.2174/1874088X01105010083 ↗
37. Lee · 2004 · 5
38. Preparation and crystal structures of the first alkali rich sodium aluminates Na7Al3O8 and Na5AlO410.1039/c39810000379 ↗
39. Hot corrosion of Ti3SiC2-based ceramics coated with thin Na2SO4 film at 910 and 950°C in air10.1016/S0010-938X(02)00211-1 ↗
40. Hot corrosion behavior of Ti3SiC2 in the mixture of Na2SO4-NaCl melts10.1016/j.jeurceramsoc.2004.04.013 ↗
41. Failure and corrosion resistance of TiN and TiC coatings deposited on graphite by chemical vapor deposition10.1016/S0257-8972(97)00690-7 ↗
42. Corrosion behavior of TiC – SiC composite ceramics in molten FLiNaK salt10.1016/j.jeurceramsoc.2017.02.020 ↗