Corrosion of Ni–Fe based alloy in chloride molten salts for concentrating solar power containing aluminum as corrosion inhibitor
Source abstract
Abstract
Chloride molten salt is extremely corrosive at high temperature. Thus, it is significant to study molten salt purification schemes to prevent structural materials from high-temperature corrosion. This paper performed corrosion tests of a Ni–Fe-based materials (HT700 alloy) in ternary chloride molten salt at 800 °C to identify the inhibiting effects of Al powder by using electrochemical methods which included impedance spectroscopy and potentiodynamic polarization, the morphologies and phase composition of HT700 alloy after corrosion tests were determined by scanning electron microscopy equipped with energy dispersive spectroscopy and X-ray diffraction. Addition of Al powder could reduce the corrosion current density of HT700 alloy in chloride molten salt, the Al 2O 3 layer was formed from the reaction of Al and impurities on the surface of the alloy, and the beneficial effects of Al powder increased with increasing Al content added in the chloride molten salt. There was a diffusion layer beneath the oxide scale resulting from the outwards diffusion of Cr in the alloy, addition of Al could hinder the outwards diffusion of Cr, thus prolong the lifetime of HT700 alloy in the chloride molten salt. Otherwise, a protective Ni 3 Al layer formed by the inwards diffusion of Al when the content of addition Al reached up to 10 wt%. Therefore, addition of Al powder in ternary chloride molten salt as corrosion inhibitor was feasible, but the content of added Al should be optimized to balance the corrosive and the thermal-physics properties of the chloride molten salt.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Molten salt chemistry and electrochemical processes · Phase Change Materials Research · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Thermal evaluation of molten salts for solar thermal energy storage
2. Corrosion mechanisms in molten salt thermal energy storage for concentrating solar power10.1016/j.rser.2019.109328 ↗
3. Electrochemical study on the corrosion behaviors of 316 SS in HITEC molten salt at different temperatures10.1016/j.solmat.2018.06.044 ↗
4. Corrosion in the molten fluoride and chloride salts and materials development for nuclear applications10.1016/j.pmatsci.2018.05.003 ↗
5. Basic properties of eutectic chloride salts NaCl-KCl-ZnCl2 and NaCl-KCl-MgCl2 as HTFs and thermal storage media measured using simultaneous DSC-TGA10.1016/j.solener.2018.01.067 ↗
6. Progress in research and development of molten chloride salt technology for next generation concentrated solar power plants10.1016/j.eng.2020.06.027 ↗
7. Experimental test of properties of KCl–MgCl2 eutectic molten salt for heat transfer and thermal storage fluid in concentrated solar power systems10.1115/1.4040065 ↗
8. Electrochemical study on the corrosion behavior of Ti3SiC2 in 3.5% NaCl solution10.1039/C6RA26239B ↗
9. Molten chloride salt for high-temperature thermal energy storage: continuous electrolytic salt purification with two Mg electrodes and AC voltage for corrosion control10.1016/j.solmat.2021.110979 ↗
10. Corrosion evaluation of eutectic chloride molten salt for new generation of CSP plants. Part 2: materials screening performance10.1016/j.est.2020.101381 ↗
11. Corrosion behavior of 316SS and Ni-based alloys in a ternary NaCl-KCl-MgCl2 molten salt10.1016/j.solener.2018.06.094 ↗
12. Effects of alloying elements on the corrosion behavior of Ni-based alloys in molten NaCl-KCl-MgCl2 salt at different temperatures10.1016/j.corsci.2018.08.021 ↗
13. Molten chloride salts for next generation concentrated solar power plants: mitigation strategies against corrosion of structural materials10.1016/j.solmat.2018.12.020 ↗
14. Fe-based amorphous coating for corrosion protection of magnesium alloy10.1016/j.matdes.2016.07.031 ↗
15. Enabling chloride salts for thermal energy storage: implications of salt purity10.1039/C9RA03133B ↗
16. Preparation of anhydrous magnesium chloride from magnesia10.1021/ie300765u ↗
17. Cathodic protection using aluminum metal in chloride molten salts as thermal energy storage material in concentrating solar power plants10.3390/app10113724 ↗
18. Corrosion performance of slurry aluminide coatings in molten NaCl–KCl10.1016/j.solmat.2021.110974 ↗
19. Corrosion resistance of alumina forming alloys against molten chlorides for energy production. II: electrochemical impedance spectroscopy under thermal cycling conditions10.1016/j.solmat.2017.03.025 ↗
20. Hot corrosion behavior of commercial alloys in thermal energy storage material of molten MgCl2/KCl/NaCl under inert atmosphere10.1016/j.solmat.2018.04.025 ↗
21. Corrosion evaluation of eutectic chloride molten salt for new generation of CSP plants. Part 1: thermal treatment assessment10.1016/j.est.2019.101125 ↗
22. Corrosion of alloys in a chloride molten salt (NaCl-LiCl) for solar thermal technologies10.1016/j.solmat.2016.05.052 ↗
23. Historical development of concentrating solar power technologies to generate clean electricity efficiently – a review10.1016/j.rser.2014.09.008 ↗
24. Vapor pressure and corrosivity of ternary metal-chloride molten-salt based heat transfer fluids for use in concentrating solar power systems
25. E-pO2− diagram for rare earth elements in molten salt10.1016/S1002-0721(17)60898-6 ↗
26. Effects of cations on corrosion of Inconel 625 in molten chloride salts10.1515/htmp-2014-0225 ↗
27. Survey and evaluation of equations for thermophysical properties of binary/ternary eutectic salts from NaCl, KCl, MgCl2, CaCl2, ZnCl2 for heat transfer and thermal storage fluids in CSP10.1016/j.solener.2017.03.019 ↗
28. Thermo-economic analysis of high-temperature sensible thermal storage with different ternary eutectic alkali and alkaline earth metal chlorides10.1016/j.solener.2018.10.008 ↗
29. The effect of humidity, impurities and initial state on the corrosion of carbon and stainless steels in molten HitecXL salt for CSP application10.1016/j.solmat.2017.08.026 ↗
30. Effects of chloride ions on electrochemical reaction of 316 stainless steel in mixtures of molten nitrate salts10.1002/mawe.201900016 ↗
31. High-temperature oxidation and corrosion of structural materials in molten chlorides10.1023/A:1010333407304 ↗
32. Molten salts in the light of corrosion mitigation strategies and embedded with nanoparticles to enhance the thermophysical properties for CSP plants10.1016/j.solmat.2020.110768 ↗
33. Cyclic voltammetry for monitoring corrosive impurities in molten chlorides for thermal energy storage10.1016/j.egypro.2017.09.489 ↗
34. Experimental demonstration and analysis of a CSP plant with molten salt heat transfer fluid in parabolic troughs10.1016/j.solener.2020.09.091 ↗
35. A study on the electrochemical deposition behavior of uranium ion in a LiCl–KCl molten salt on solid and liquid electrode10.1016/j.jelechem.2012.07.025 ↗
36. Simulated fireside corrosion behavior of a wrought Ni-Fe-Based superalloy for 700 °C-Class ultra-supercritical power plant Applications10.1007/s11665-019-04515-z ↗
37. Electrochemical impedance models for molten salt corrosion10.1016/S0010-938X(00)00108-6 ↗
38. Potential scalability of a cost-effective purification method for MgCl2-Containing salts for next-generation concentrating solar power technologies10.1016/j.solmat.2020.110663 ↗
39. Kinetics and mechanism of the sulfidation of Fe-Mo alloys10.1007/BF00666462 ↗
40. Corrosion of steel alloys in molten NaCl + Na2SO4 at 700 °C for thermal energy storage10.1016/j.solmat.2017.11.017 ↗
41. Electrochemistry of molten salt corrosion10.1016/0921-5093(91)90265-O ↗
42. Corrosion behavior of Ni-based alloys in molten NaCl-CaCl2 -MgCl2 eutectic salt for concentrating solar power10.1016/j.solmat.2017.05.050 ↗
43. Corrosion behavior of Fe–Ni–Cr alloys in the molten salt of LiCl–Li2O at high temperature10.1016/j.jnucmat.2003.10.011 ↗