High temperature corrosion beneath carbonate melts of aluminide coatings for CSP application
Source abstract
Abstract
Abstract Slurry iron-aluminide coatings deposited by spraying on 9 wt% Cr P91 alloy as well as uncoated P91 were exposed isothermally at 650 °C to a ternary molten salt mixture based on a Na, K and Li carbonate eutectic, under static and dynamic conditions. Uncoated P91 evidenced considerable mass gains and extensive spallation in both conditions. Indeed, P91 developed a very thick fast growing multilayered oxide scale which included LiFeO2, LiFe5O8 and (Fe,Cr)3O4. Under dynamic conditions, the metal loss was higher that when the test was carried out statically but this was not reflected in the gravimetric measurements likely due to spallation of the scales in both cases. The coated systems performed better than the uncoated material up to at least 1000 h according to metallographic inspection. However, the aluminide coating showed non-uniform attack and on the corresponding zones, a thick layer likely consisting of LiFeO2 developed over an internal oxidation zone corresponding to all of the coating initial thickness. K was also detected within the internal oxidation zone suggesting that the coating was internally attacked at least by K containing species (Li cannot be detected by EDS). K and perhaps Li seem to diffuse along the grain boundaries of the coating, leading to internal oxidation responsible for the degradation. On the non-degraded zones, the coating maintained the initial microstructure as very low coating/substrate interdiffusion occurred. A 20 wt% average Al content at the surface does not seem to be high enough to sustain a protective oxide.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Advanced heat transfer fluids for direct molten salt line-focusing CSP plants10.1016/j.pecs.2018.02.002 ↗
2. Corrosion effects between molten salts and thermal storage material for concentrated solar power plants10.1016/j.apenergy.2011.12.057 ↗
3. The effect of humidity, impurities and initial state on the corrosion of carbon and stainless steels in molten HitecXL salt for CSP application10.1016/j.solmat.2017.08.026 ↗
4. Evaluation of corrosion resistance of A516 Steel in a molten nitrate salt mixture using a pilot plant facility for application in CSP plants10.1016/j.solmat.2016.12.002 ↗
5. Advances in central receivers for concentrating solar applications10.1016/j.solener.2017.03.048 ↗
6. Accelerated corrosion Testing of a nickel-base Alloy in a molten salt
7. Mehos · 2017
8. Corrosion resistance of HR3C to a carbonate molten salt for energy storage applications in CSP plants10.1016/j.solmat.2016.08.014 ↗
9. The cost of lithium is unlikely to upend the price of Li-ion storage systems10.1016/j.jpowsour.2016.04.073 ↗
10. Molten salt power towers operating at 600-650 degrees C: salt selection and cost benefits10.1016/j.solener.2018.01.063 ↗
11. Corrosion resistance of Cr/Ni alloy to a molten carbonate salt at various temperatures for the next generation high-temperature CSP plants10.1016/j.solener.2018.06.091 ↗
12. Corrosion of steel alloys in eutectic NaCl + Na2CO3 at 700°C and Li2CO3 + K2CO3 + Na2CO3 at 450°C for thermal energy storage10.1016/j.solmat.2017.05.063 ↗
13. Corrosion of stainless steel 316 in eutectic molten salts for thermal energy storage10.1016/j.solener.2018.03.053 ↗
14. Corrosion behaviour of austenitic stainless steels in carbonate melt at 923 K under controlled CO2-O2 environment10.1016/j.corsci.2018.01.031 ↗
15. Corrosion of Inconel 601 in molten salts for thermal energy storage10.1016/j.solmat.2017.07.036 ↗
16. Hot corrosion study of coated separator plates of molten carbonate fuel cells by slurry aluminides10.1016/S0257-8972(02)00417-6 ↗
17. Slurry coatings for molten carbonate fuel cell separator plates10.4028/www.scientific.net/MSF.369-372.759 ↗
18. Thermal spray coatings for molten carbonate fuel cells separator plates10.1016/S0257-8972(01)01435-9 ↗
19. Corrosion evaluation of alloys and MCrAlX coatings in molten carbonates for thermal solar applications10.1016/j.solmat.2016.07.029 ↗
20. Slurry Aluminizing: a solution for molten nitrate salt corrosion in concentrated solar power plants10.1016/j.solmat.2015.11.024 ↗
21. Aluminide slurry coatings for protection of ferritic steel in molten nitrate corrosion for concentrated solar power technology
22. Evaluation of corrosion resistance of aluminium coating with and without annealing against molten carbonate using electrochemical impedance spectroscopy10.1016/j.jpowsour.2014.03.076 ↗
23. Effect of heat treatment and chemical composition on the corrosion behavior of FeAl intermetallics in molten (Li + K) carbonate10.1016/j.jpowsour.2007.05.010 ↗
24. Deposition process of slurry iron aluminide coatings10.3184/096034008X388812 ↗
25. Protective coatings for high temperature molten salt heat storage systems in solar concentration power plants
26. High temperature molten salt corrosion behavior of aluminide and nickel-aluminide coatings for heat storage in concentrated solar power plants10.1016/j.surfcoat.2018.05.081 ↗
27. Overview of steam oxidation behaviour of Al protective oxide precursor coatings on P9210.1080/02670844.2016.1155691 ↗
28. Laboratory corrosion testing of coatings and substrates simulating coal combustion under a low NOx burner atmosphere10.1002/maco.201307096 ↗
29. Biomass corrosion behavior of steels and coatings in contact with KCl/K2SO4 at 550°C under an oxy-fuel combustion atmosphere: a screening laboratory test10.1016/j.surfcoat.2018.05.082 ↗
30. Universidad Complutense de Madrid · 2016
31. Diffusion stable aluminide coatings; behavior under steam and oxy-fuel fire-side corrosions10.1016/j.surfcoat.2018.07.027 ↗
32. Oxidation and hot corrosion of superalloys
33. Corrosion of iron stainless steels in molten nitrate salt
34. High temperature corrosion of low and high alloy steels under molten carbonate fuel cell conditions10.1002/maco.19970480803 ↗
35. Corrosion of iron base alloys and high alloy steels in the Li2CO3-K2CO3 eutectic mixture10.1016/S0010-938X(97)00020-6 ↗
36. "Acids" and "bases" in molten mass. The determination of oxygen ions concentrations
37. On the oxygen electrode in molten salts10.3891/acta.chem.scand.06-0257 ↗
38. Structural properties and electrochemistry of alpha-LiFeO210.1016/j.jpowsour.2011.09.054 ↗
39. The corrosion behaviour of iron and chromium in molten (Li0.62K0.38)(2)CO310.1016/S0013-4686(97)10191-8 ↗
40. Boiler materials for ultra-supercritical coal power plants-stearnside oxidation10.1361/105994906X108756 ↗
41. Formation and disappearance of an internal oxidation zone in the initial stage of the steam oxidation of Fe-9Cr-0.26Si ferritid-steel10.1179/mht.2003.014 ↗
42. Steam oxidation of 9% to 12% Cr steels: critical evaluation and implications for practical application10.5006/1065 ↗
43. High Temperature corrosion of high alloyed steels under simulated molten carbonate fuel cell conditions10.1515/pm-1996-331105 ↗
44. Reaktionstypen bei der oxydation von legierungen
45. Degradation behaviour of Al-Fe coatings in wet-seal area of molten carbonate fuel cells10.1016/S0378-7753(02)00353-1 ↗